Effect of Water Aging of Adherend Composite on Repair Bond Strength of Nanofilled Composites

被引:14
|
作者
Nagano, Daiki [1 ]
Nakajima, Masatoshi [1 ]
Takahashi, Masahiro [1 ]
Ikeda, Masaomi [2 ]
Hosaka, Keiichi [1 ]
Sato, Kento [1 ]
Prasansuttiporn, Taweesak [3 ]
Foxton, Richard M. [4 ]
Tagami, Junji [1 ]
机构
[1] Tokyo Med & Dent Univ, Grad Sch Med & Dent Sci, Dept Oral Hlth Sci, Cariol & Operat Dent, Tokyo, Japan
[2] Tokyo Med & Dent Univ, Grad Sch Med & Dent Sci, Dept Oral Prosthet Engn, Tokyo, Japan
[3] Chiang Mai Univ, Fac Dent, Dept Restorat Dent & Periodontol, Chiang Mai, Thailand
[4] Kings Coll London, Kings Coll London Dent Inst, Dept Restorat Dent, London, England
来源
JOURNAL OF ADHESIVE DENTISTRY | 2018年 / 20卷 / 05期
关键词
bond strength; dental materials; resin composite repair; surface treatments; water solubility; water sorption; SURFACE TREATMENTS; RESIN COMPOSITE; ELUTION; LIGHT; ADHESIVE; TEGDMA; MONOMERS; HALOGEN; AGENTS;
D O I
10.3290/j.jad.a41331
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose: To evaluate the effect of water aging of adherend composite on repair bond strength to nanofilled composites with specific fillers using different bonding agents. Materials and Methods: Three nanofilled composites - Beautifil II with S-PRG filler (BE) / Filtek Supreme ultra with nanocluster filler (SP) / Estelite Sigma Quick (ES) - and one microhybrid composite, Clearfil APX (AP), were used in this study. The composite disks were immersed in water for different durations (immediate, 1 week, 2 weeks or 1 month), and then the polished surfaces were treated with one of three bonding agents - no treatment (control), application of Clearfil SE One (SE), application of Clearfil SE One plus Clearfil Porcelain Bond Activator (PB) - then filled with a repair composite. The bonded composite disks were subjected to the microshear bond strength (mu SBS) test. Additionally, water sorption (W-sp) and solubility (W-sl) of the resin composite were measured. The pSBS data were was statistically analyzed using a three-way ANOVA and t-test with Bonferroni correction for multiple comparisons. Results: Water aging of adherend composite affected the repair bond strength (p < 0.05). For BE, SP, and ES, application of an adhesive agent improved repair bond strengths to water-aged composites (p < 0.05), but adding a silane coupling agent could not (p > 0.05). For AP, the mu SBS significantly increased, with control group < SE group < PB group (p < 0.05). Conclusion: Microhybrid composite was a more suitable material for composite repair than nanofilled composite, due to adhesion to exposed, larger silica fillers. S-PRG filler and nanocluster filler in the nanofilled composites played a slight role in improving their repair bonding performances with the bonding agents tested.
引用
收藏
页码:425 / 433
页数:9
相关论文
共 50 条
  • [31] Water uptake and strength characteristics of a nanofilled resin-based composite
    Curtis, A. R.
    Shortall, A. C.
    Marquis, P. M.
    Palin, W. M.
    [J]. JOURNAL OF DENTISTRY, 2008, 36 (03) : 186 - 193
  • [32] Effect of Silane Reaction Time on the Repair of a Nanofilled Composite by a Tribochemical Treatment
    Pilo, Raphael
    Brosh, Tamar
    Geron, Valery
    Levartovsky, Shifra
    Eliades, George
    [J]. JOURNAL OF ADHESIVE DENTISTRY, 2016, 18 (02): : 125 - 134
  • [33] Repair Bond Strength of a CAD/CAM Nanoceramic Resin and Direct Composite Resin: Effect of Aging and Surface Conditioning Methods
    Duarte Moura, Dayanne Monielle
    de Oliveira Dal Piva, Amanda Maria
    do Nascimento Januario, Ana Beatriz
    Verissimo, Aretha Heitor
    Bottino, Marco Antonio
    Ozcan, Mutlu
    Assuncao Souza, Rodrigo Othavio
    [J]. JOURNAL OF ADHESIVE DENTISTRY, 2020, 22 (03): : 275 - 283
  • [34] Effect of Various Aging Protocols and Intermediate Agents on the Bond Strength of Repaired Composites
    Silva Sousa, Ana Beatriz
    Jardilino Silami, Francisca Daniele
    Roberti Garcia, Lucas da Fonseca
    Naves, Lucas Zago
    Panzeri Pires-de-Souza, Fernanda de Carvalho
    [J]. JOURNAL OF ADHESIVE DENTISTRY, 2013, 15 (02): : 137 - 144
  • [35] Effect of different surface treatments on the repair bond strength of resin composites with titanium
    Korkmaz, Fatih Mehmet
    Ates, Sabit Melih
    Caglar, Ipek Satiroglu
    Baygin, Ozgul
    Duymus, Zeynep Yesil
    [J]. JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2019, 33 (21) : 2385 - 2403
  • [36] Immediate repair bond strengths of microhybrid, nanohybrid and nanofilled composites after different surface treatments
    Rinastiti, Margareta
    Oezcan, Mutlu
    Siswomihardjo, Widowati
    Busscher, Henk J.
    [J]. JOURNAL OF DENTISTRY, 2010, 38 (01) : 29 - 38
  • [37] Effect of different artificial aging conditions on ceramic-composite bond strength
    Wegner, SM
    Gerdes, W
    Kern, M
    [J]. INTERNATIONAL JOURNAL OF PROSTHODONTICS, 2002, 15 (03) : 267 - 272
  • [38] Microtensile bond strength of a nanofilled composite resin to human dentin after nonvital tooth bleaching
    Mueller Arcari, Gilberto
    Araujo, Elito
    Narciso Baratieri, Luiz
    Carpena Lopes, Guilherme
    [J]. JOURNAL OF ADHESIVE DENTISTRY, 2007, 9 (03): : 333 - 340
  • [39] EFFECT OF HYDROTHERMAL AGING ON BOND STRENGTH
    GAUR, U
    CHOU, CT
    MILLER, B
    [J]. COMPOSITES, 1994, 25 (07): : 609 - 612
  • [40] Effect of Argon Plasma Surface Treatment on Bond Strength of Resin Composite Repair
    Ayres, A. P. A.
    Hirata, R.
    Fronza, B. M.
    Lopes, B. B.
    Ambrosano, G. M. B.
    Giannini, M.
    [J]. OPERATIVE DENTISTRY, 2019, 44 (02) : E75 - E82