Low-temperature full wafer adhesive bonding

被引:178
|
作者
Niklaus, F [1 ]
Enoksson, P [1 ]
Kälvesten, E [1 ]
Stemme, G [1 ]
机构
[1] Royal Inst Technol, Dept Signals Sensors & Syst, S-10044 Stockholm, Sweden
关键词
D O I
10.1088/0960-1317/11/2/303
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
We have systematically investigated the influence of different bonding parameters on void formation in a low-temperature adhesive bonding process. As a result of these studies we present guidelines for void free adhesive bonding of 10 cm diameter wafers. We have focused on polymer coatings with layer thicknesses between 1 mum and 18 mum. The tested polymer materials were benzocyclobutene (BCE) from Dow Chemical, a negative photoresist (ULTRA-i 300) and a positive photoresist (S1818) from Shipley, a polyimide (HTR3) from Arch Chemical and two different polyimides (PI2555 and PI2610) from DuPont. The polymer material, the banding pressure and the pre-curing time and temperature for the polymer significantly influence void formation at the bond interface. High bonding pressure and optimum pre-curing times/temperatures counteract void formation. We present the process parameters to achieve void-free bonding with the BCB coating and with the ULTRA-i 300 photoresist coating as adhesive materials. Excellent void-free and strong bonds have been achieved by using BCB as the bonding material which requires a minimum bonding temperature of 180 degreesC.
引用
收藏
页码:100 / 107
页数:8
相关论文
共 50 条
  • [1] Low temperature full wafer adhesive bonding of structured wafers
    Niklaus, F
    Andersson, H
    Enoksson, P
    Stemme, G
    [J]. SENSORS AND ACTUATORS A-PHYSICAL, 2001, 92 (1-3) : 235 - 241
  • [2] Wafer bonding by low-temperature soldering
    Lee, C
    Huang, WF
    Shie, JS
    [J]. SENSORS AND ACTUATORS A-PHYSICAL, 2000, 85 (1-3) : 330 - 334
  • [3] LOW-TEMPERATURE WAFER DIRECT BONDING
    TONG, QY
    CHA, GH
    GAFITEANU, R
    GOSELE, U
    [J]. JOURNAL OF MICROELECTROMECHANICAL SYSTEMS, 1994, 3 (01) : 29 - 35
  • [4] Influence of Bonding Atmosphere on Low-Temperature Wafer Bonding
    Wang, Ying-Hui
    Suga, Tadatomo
    [J]. 2010 PROCEEDINGS 60TH ELECTRONIC COMPONENTS AND TECHNOLOGY CONFERENCE (ECTC), 2010, : 435 - 439
  • [5] Low-temperature Au/Si wafer bonding
    Jing, E.
    Xiong, B.
    Wang, Y.
    [J]. ELECTRONICS LETTERS, 2010, 46 (16) : 1143 - U72
  • [6] Hydrophilic low-temperature direct wafer bonding
    Ventosa, C.
    Rieutord, F.
    Libralesso, L.
    Morales, C.
    Fournel, F.
    Moriceau, H.
    [J]. JOURNAL OF APPLIED PHYSICS, 2008, 104 (12)
  • [7] Low-temperature hydrophobic silicon wafer bonding
    Tong, QY
    Gan, Q
    Hudson, G
    Fountain, G
    Enquist, P
    Scholz, R
    Gösele, U
    [J]. APPLIED PHYSICS LETTERS, 2003, 83 (23) : 4767 - 4769
  • [8] LOW-TEMPERATURE SILICON-WAFER BONDING
    QUENZER, HJ
    BENECKE, W
    [J]. SENSORS AND ACTUATORS A-PHYSICAL, 1992, 32 (1-3) : 340 - 344
  • [9] LOW-TEMPERATURE, HIGH-STRENGTH, WAFER-TO-WAFER BONDING
    FLEMING, JG
    ROHERTYOSMUN, E
    GODSHALL, NA
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1992, 139 (11) : 3300 - 3302
  • [10] Low-Temperature Wafer-to-Wafer Hybrid Bonding by Nanocrystalline Copper
    Chiu, Wei-Lan
    Lee, Ou-Hsiang
    Chiang, Chia-Wen
    Chang, Hsiang-Hung
    [J]. IEEE 72ND ELECTRONIC COMPONENTS AND TECHNOLOGY CONFERENCE (ECTC 2022), 2022, : 679 - 684