Influence of various bonding techniques on the fracture strength of thin CAD/CAM-fabricated occlusal glass-ceramic veneers

被引:35
|
作者
Yazigi, Christine [1 ]
Kern, Matthias [1 ]
Chaar, Mohamed Sad [1 ]
机构
[1] Christian Albrechts Univ Kiel, Sch Dent, Dept Prosthodont Propaedeut & Dent Mat, Arnold Heller Str 16, D-24105 Kiel, Germany
关键词
Glass-ceramic veneers; Glass-ceramic tabletops; Occlusal veneers; Immediate dentin sealing; Total etch; Selective etch; Lithium disilicate restorations; Fracture resistance; Adhesive bonding to dentin; PARTIAL-COVERAGE RESTORATIONS; 3-YEAR CLINICAL EFFECTIVENESS; ARTIFICIAL ORAL ENVIRONMENT; SEVERE DENTAL EROSION; SELF-ETCH ADHESIVE; PREPARATION DESIGN; PORCELAIN VENEERS; CERVICAL LESIONS; POSTERIOR TEETH; COMPOSITE RESIN;
D O I
10.1016/j.jmbbm.2017.08.016
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Objectives: To evaluate the efficiency of immediate dentin sealing and the effects of different bonding protocols on the fracture strength of CAD/CAM occlusal veneers bonded to exposed dentin. Methods: Ninety-six extracted maxillary premolars were initially divided into three main groups with 32 specimens each: without immediate dentin sealing, immediate dentin sealing/total etching and immediate dentin sealing/selective etching. Teeth were identically prepared in the dentin to receive occlusal veneers of 0.8 mm thickness, milled from lithium disilicate ceramic blocks (IPS e.max CAD). Each main group was later subdivided, according to the pre-cementation surface etching protocol (total/selective), into two subgroups with 16 specimens each. All restorations were adhesively bonded using a resin cement (Variolink Esthetic). Half of the specimens of each subgroup were subjected to thermo-dynamic loading in a chewing simulator with 1,200,000 cycles at 10 kg load. The other half and the surviving specimens were subjected to quasi-static loading until failure. Statistical analysis was performed using three-way ANOVA and Tukey's post-hoc tests. Results: All specimens except one survived the artificial aging. A significantly higher fracture strength of restorations (p <= 0.001) was obtained when immediate dentin sealing was followed regardless of the etching method with values ranging from a minimum of 1122 +/- 336 N to a maximum of 1853 +/- 333 N. Neither the pre-cementation treatment nor the artificial aging had a statistical significant effect on the fracture strength. Significance: Immediate dentin sealing protocol is recommended whenever dentin is exposed during the preparation for thin glass-ceramic occlusal veneers.
引用
收藏
页码:504 / 511
页数:8
相关论文
共 50 条
  • [1] Influence of thermomechanical fatigue on the fracture strength of CAD-CAM-fabricated occlusal veneers
    Al-Akhali, Majed
    Kern, Matthias
    Elsayed, Adham
    Samran, Abdulaziz
    Chaar, Mohamed Sad
    JOURNAL OF PROSTHETIC DENTISTRY, 2019, 121 (04): : 644 - 650
  • [2] Fracture strength and bonding interface morphology of CAD/CAM-fabricated ceramic laminate veneers on bleached enamel treated with two different antioxidants
    Zhang, Hong
    Chen, Jiawen
    Wang, Ying
    Yu, Yiyan
    Zhao, Yuanhang
    Song, Jiazhuo
    Zhang, Zhimin
    DENTAL MATERIALS JOURNAL, 2023, 42 (04) : 559 - 567
  • [3] Fracture strength of CAD/CAM composite and composite-ceramic occlusal veneers
    Johnson, Andrew C.
    Versluis, Antheunis
    Tantbirojn, Daranee
    Ahuja, Swati
    JOURNAL OF PROSTHODONTIC RESEARCH, 2014, 58 (02) : 107 - 114
  • [4] Biaxial flexural strength of various CAD-CAM glass-ceramic materials
    Alakkad, Layali
    Kostagianni, Aikaterini
    Finkelman, Matthew
    Maawadh, Ahmed
    Ali, Ala
    Papathanasiou, Aikaterini
    AMERICAN JOURNAL OF DENTISTRY, 2021, 34 (02): : 91 - 96
  • [5] Laser debonding of ultrathin occlusal veneers fabricated from different CAD/CAM ceramic materials
    El-Sheikh, Nourhan Ali
    Wahsh, Marwa Mohamad
    Hussein, Ghada Abdelfattah
    BMC ORAL HEALTH, 2024, 24 (01):
  • [6] Influence of material type, thickness and storage on fracture resistance of CAD/CAM occlusal veneers
    Albelasy, Eman
    Hamama, Hamdi H.
    Tsoi, James K. H.
    Mahmoud, Salah H.
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2021, 119
  • [7] Influence of resin-coating techniques on the marginal adaptation and the bond strengths of CAD/CAM-fabricated hybrid ceramic inlays
    Kanamori, Yuna
    Takahashi, Rena
    Nikaido, Toru
    Nitta, Hiroshi
    Shimada, Yasushi
    Tagami, Junji
    Kunzelmann, Karl-Heinz
    DENTAL MATERIALS JOURNAL, 2024, 43 (03) : 407 - 414
  • [8] DIRECT COMPOSITE RESIN LAYERING TECHNIQUES FOR CREATING LIFELIKE CAD/CAM-FABRICATED COMPOSITE RESIN VENEERS AND CROWNS
    LeSage, Brian
    JOURNAL OF PROSTHETIC DENTISTRY, 2014, 112 (01): : 5 - 8
  • [9] Influence of various gypsum materials on precision of fit of CAD/CAM-fabricated zirconia copings
    Kim, Jae-Hong
    Kim, Ki-Baek
    Kim, Woong-Chul
    Rhee, Hyun-Sill
    Lee, Il-Hyun
    Kim, Ji-Hwan
    DENTAL MATERIALS JOURNAL, 2015, 34 (01) : 19 - 24
  • [10] THE FAILURE LOAD OF CAD/CAM GENERATED ZIRCONIA AND GLASS-CERAMIC LAMINATE VENEERS WITH DIFFERENT PREPARATION DESIGNS
    Alghazzawi, Tariq F.
    Lemons, Jack
    Liu, Perng-Ru
    Essig, Milton E.
    Janowski, Gregg M.
    JOURNAL OF PROSTHETIC DENTISTRY, 2012, 108 (06): : 386 - 393