- [31] Cavitation and failure during hot forging of Ti-6Al-4V METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1999, 30 (05): : 1411 - 1424
- [32] The martensitic transformation texture in Ti-6Al-4V ICOTOM 14: TEXTURES OF MATERIALS, PTS 1AND 2, 2005, 495-497 : 669 - 674
- [33] Cavitation and failure during hot forging of Ti-6Al-4V Metall Mat Trans A Phys Metall Mat Sci, 5 (1411-1424):
- [34] Cavitation and failure during hot forging of Ti-6Al-4V Metallurgical and Materials Transactions A, 1999, 30 : 1411 - 1424
- [38] Effect of hydrogenation on the hot deformation of Ti-6Al-4V alloy Xiyou Jinshu Cailiao Yu Gongcheng, 2008, 12 (2089-2093):