摘要
A modern ceramic-matrix composite (CMC) has been extensively characterized for a high-temperature aerospace turbine-engine application. The CMC system has a silicon-nitrogen-carbon (SI-N-C) matrix reinforced with Nicalon fibers woven in a balanced eight-harness satin weave fabric Tensile tests have demonstrated that this CMC exhibits excellent strength retention up to 1100 degrees C. The room-temperature fatigue limit was 160 MPa, similar to 80% of the room-temperature tensile strength. The composite reached run-out conditions under cyclic (10(5) cycles at 1 Hz) and sustained tension (100 h) conditions at a stress of 110 MPa, which was similar to 35 MPa above the proportional limits at temperatures up to 1100 degrees C in air. At stress levels >110 MPa, cyclic loading at 1000 degrees C caused a more severe reduction in life, based on time, compared with sustained tension. Further life degradation was observed in the 1000 degrees C fatigue specimens that were exposed to a salt-fog environment, This degradation decreased the fatigue life similar to 85% at the stress levels that were tested.
引用
收藏
页码:1797 / 1811
页数:15
相关论文
共 50 条
  • [31] INTERFACIAL STABILITY, OXIDATION RESPONSE AND MECHANICAL-PROPERTIES OF A NICALON(TM) FIBER-REINFORCED CHEMICAL BONDED CERAMIC-MATRIX COMPOSITE
    BANDYOPADHYAY, A
    ASWATH, PB
    JOURNAL OF MATERIALS SCIENCE, 1994, 29 (16) : 4205 - 4215
  • [32] High-temperature transverse fracture toughness of nicalon-fiber-reinforced CAS-II glass-ceramic matrix composite
    Kahraman, R
    Mandell, JF
    Deibert, MC
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1997, 80 (07) : 1812 - 1820
  • [33] Studies on the structure and composition of Si-N-C fibers containing boron at high temperature
    First Military Medical Univ, Guangzhou, China
    Gaojishu Tongxin/High Technology Letters, 1997, 7 (09): : 15 - 19
  • [34] ROOM-TEMPERATURE MECHANICAL-BEHAVIOR OF FIBER-REINFORCED CERAMIC-MATRIX COMPOSITES
    MAH, T
    MENDIRATTA, MG
    KATZ, AP
    RUH, R
    MAZDIYASNI, KS
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1985, 68 (01) : C27 - C30
  • [35] Tension-Tension Fatigue Behavior of Unidirectional C/Sic Ceramic-Matrix Composite at Room Temperature and 800 °C in Air Atmosphere
    Li, Longbiao
    MATERIALS, 2015, 8 (06) : 3316 - 3333
  • [36] ENHANCED HIGH-TEMPERATURE MECHANICAL BEHAVIOR OF AN IN SITU TIAL MATRIX COMPOSITE REINFORCED WITH ALUMINA
    Pilone, D.
    Mondal, A.
    Brotzu, A.
    Felli, F.
    Pulci, G.
    Paglia, L.
    Marra, F.
    INTERNATIONAL JOURNAL OF METALCASTING, 2023, 17 (02) : 1139 - 1148
  • [37] Composition and structure of boron-containing Si-N-C fibres at high temperature
    Lu, L
    Song, YC
    Feng, CX
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1998, 17 (07) : 599 - 602
  • [38] Enhanced High-Temperature Mechanical Behavior of an in Situ TiAl Matrix Composite Reinforced With Alumina
    D. Pilone
    A. Mondal
    G. Pulci
    L. Paglia
    A. Brotzu
    F. Marra
    F. Felli
    International Journal of Metalcasting, 2023, 17 : 1139 - 1148
  • [39] High-temperature fracture behavior of ceramic matrix composites: an overview
    Rosa, L. Guerra
    EVALUATION, INSPECTION AND MONITORING OF STRUCTURAL INTEGRITY, 2008, : 17 - 28
  • [40] Fatigue hysteresis behavior of unidirectional C/SiC ceramic-matrix composite at room and elevated temperatures
    Li Longbiao
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 625 : 1 - 18