Studies on the structure and composition of Si-N-C fibers containing boron at high temperature

被引:0
|
作者
First Military Medical Univ, Guangzhou, China [1 ]
机构
来源
关键词
Amorphous materials - Boron - Crystal structure - High temperature testing - Infrared spectroscopy - Pyrolysis - Scanning electron microscopy - Silicon carbide - X ray diffraction - X ray photoelectron spectroscopy;
D O I
暂无
中图分类号
学科分类号
摘要
The composition and structure of Si-N-C fibers containing boron as well as their changes at high temperature are studied in this paper. The IR, XPS, EA, XRD and SEM analytical results show that Si-N-C fibers containing boron treated at 1250°C comprise Si, N, C, O and B and are amorphous, while the structures of fibers pyrolysed up to 1800°C are converted into α-SiC crystal, and B exists in the fibers in the form of B-N bonds at high temperature. The Si-N-C fibers containing boron have smooth surface and small crystalline - size in comparison with the fibers without boron, which indicates that the incorporation of boron leads to the improvement of the microstructure of fibers at high temperature.
引用
收藏
页码:15 / 19
相关论文
共 50 条
  • [1] Composition and structure of boron-containing Si-N-C fibres at high temperature
    Lu, L
    Song, YC
    Feng, CX
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1998, 17 (07) : 599 - 602
  • [2] UTILIZATION OF POLYMER PRECURSORS IN THE FORMATION OF SI-N-C ADVANCED CERAMIC FIBERS
    SALINGER, RM
    BARNARD, TD
    LI, CT
    MAHONE, LG
    SAMPE QUARTERLY-SOCIETY FOR THE ADVANCEMENT OF MATERIAL AND PROCESS ENGINEERING, 1988, 19 (03): : 27 - 30
  • [3] UTILIZATION OF POLYMER PRECURSORS IN THE FORMATION OF Si-N-C ADVANCED CERAMIC FIBERS.
    Salinger, R.M.
    Barnard, T.D.
    Li, C.-T.
    Mahone, L.G.
    S.A.M.P.E. quarterly, 1988, 19 (03): : 27 - 30
  • [4] Mechanical behavior and high-temperature performance of a woven Nicalon™/Si-N-C ceramic-matrix composite
    Lee, SS
    Zawada, LP
    Staehler, JM
    Folsom, CA
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1998, 81 (07) : 1797 - 1811
  • [5] MICROSTRUCTURAL CHANGES OF AMORPHOUS SI-N-C FINE POWDERS AT HIGH-TEMPERATURES
    AMANO, T
    IZAKI, K
    NIPPON SERAMIKKUSU KYOKAI GAKUJUTSU RONBUNSHI-JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1989, 97 (03): : 339 - 345
  • [6] Synthesis of Si-N-C Ceramic Composites by Pyrolysis of Polysilazane and Polycarbosilane
    Bao Xingyi
    Li Song
    Tang Xiaoxia
    Zhang Yue
    HIGH-PERFORMANCE CERAMICS VII, PTS 1 AND 2, 2012, 512-515 : 306 - 309
  • [7] Crystallization and phase development of nanometric amorphous Si-N-C powders
    Li, Y.-L.
    Liang, Y.
    Hu, Z.-Q.
    Nanostructured Materials, 1994, 4 (07): : 857 - 864
  • [8] Correlation of boron content and high temperature stability in Si-B-C-N ceramics
    Müller, A
    Gerstel, P
    Weinmann, M
    Bill, J
    Aldinger, F
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2000, 20 (14-15) : 2655 - 2659
  • [9] 含硼Si-N-C纤维的高温结构组成研究
    卢玲
    宋永才
    冯春祥
    高技术通讯, 1997, (09) : 15 - 19
  • [10] THERMODYNAMIC STUDIES OF HIGH-TEMPERATURE EQUILIBRIA OF THE SI - N, SI - C - H AND SI - O - C - H SYSTEMS
    KOSTIC, ZG
    PAVLOVIC, P
    STEFANOVIC, P
    JOURNAL DE PHYSIQUE, 1990, 51 (18): : C511 - C517