A Reliability Study of Nanoparticles Reinforced Composite Lead-Free Solder

被引:21
|
作者
Chen, Si [1 ,2 ]
Zhang, Lili [1 ,2 ]
Liu, Johan [1 ,2 ,3 ,4 ]
Gao, Yulai [5 ]
Zhai, Qijie [5 ]
机构
[1] Shanghai Univ, Key Lab Adv Display & Syst Applicat, Shanghai 200072, Peoples R China
[2] Shanghai Univ, SMIT Ctr, Sch Automat & Mech Engn, Shanghai 200072, Peoples R China
[3] Chalmers Univ Technol, SMIT Ctr, SE-41296 Gothenburg, Sweden
[4] Chalmers Univ Technol, Bionano Syst Lab, Dept Microtechnol & Nanosci, SE-41296 Gothenburg, Sweden
[5] Shanghai Univ, Sch Mat Sci & Engn, Shanghai 200072, Peoples R China
基金
美国国家科学基金会;
关键词
composite solder; nanoparticles; shear strength; thermal cycling; fracture mode;
D O I
10.2320/matertrans.MJ201002
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This work looks at the development and investigation of a reinforced composite solder with low melting point The composite solder was prepared by adding Sn 3 0Ag 0 5Cu nanoparticles Into Sn 58BI solder paste 1 he Sn 3 0Ag 0 5Cu nanoparticles were manufactured using a self developed Consumable electrode Direct Current Arc (CDCA) technique The test FR 4 Printed Circuit Board (PCB) with Cu pad and Electroless Nickel Immersion Gold (ENIG) surface finish were fabricated and fifty SR1206 chip resistors were mounted on pads of test PCB with the reinforced composite solder paste by using conventional surface mount technology The differential scanning calorimetry (DSC) was used to analyze the constituent of the composite solder Joint after reflow A scanning electron microscope (SEM) transmission electron microscope (TEM) and optical microscope (OM) were employed in order to observe the morphology of nanoparticles the microstructure of reinforced composite solder Joint the crack initiation and propagation in solder Joint and the fracture mode after shear test The thermal cycling (TC) was carried out with a temperature range of 40 degrees C and 125 C The contract resistance of the solder Joint was measured during thermal cycling and the shear test of solder Joints was performed before and after 500 thermal cycles After the shear test all fracture surfaces were inspected to identify the fracture mode of the composite solder joint The results of the experiments detailed in this work indicate that the shear strength of the composite solder increased 2 times in comparison to Sn 58B(1) Meanwhile the thermomechanical fatigue (TMF) resistance of the composite solder with 1 mass% nanoparticles was 16 times stronger than Sn 58BI and 4 times stronger than Sn 3 0Ag 0 5Cu However the tendency of forming micro cracks between nanoparticles and solder matrix and the fracture within solder was increased for solder joints with more than 3 mass% nanoparticles after thermal cycling [doi 10.2320/matertrans.MJ201002].
引用
收藏
页码:1720 / 1726
页数:7
相关论文
共 50 条
  • [21] Lead-free solder reinforced with multiwalled carbon nanotubes
    S. M. L. Nai
    J. Wei
    M. Gupta
    Journal of Electronic Materials, 2006, 35 : 1518 - 1522
  • [22] SnZnAl lead-free solder with high packaging reliability
    Kitajima, M
    Shono, T
    Masuda, S
    2003 INTERNATIONAL SYMPOSIUM ON MICROELECTRONICS, 2003, 5288 : 762 - 767
  • [23] Reliability testing of WLCSP lead-free solder joints
    Chiang, Huann-Wu
    Chen, Jun-Yuan
    Chen, Ming-Chuan
    Lee, Jeffrey C. B.
    Shiau, Gary
    JOURNAL OF ELECTRONIC MATERIALS, 2006, 35 (05) : 1032 - 1040
  • [24] Reliability testing of WLCSP lead-free solder joints
    Huann-Wu Chiang
    Jun-Yuan Chen
    Ming-Chuan Chen
    Jeffrey C. B. Lee
    Gary Shiau
    Journal of Electronic Materials, 2006, 35 : 1032 - 1040
  • [25] State of the Art of Lead-Free Solder Joint Reliability
    Lau, John H.
    JOURNAL OF ELECTRONIC PACKAGING, 2021, 143 (02)
  • [26] Reliability of high temperature lead-free solder alternative
    McCluskey, F. P.
    Wang, Z.
    Dash, M.
    Huff, D.
    ESTC 2006: 1ST ELECTRONICS SYSTEMINTEGRATION TECHNOLOGY CONFERENCE, VOLS 1 AND 2, PROCEEDINGS, 2006, : 444 - +
  • [27] Nano ZrO2 particulate-reinforced lead-free solder composite
    Shen, Jun
    Liu, Yongchang
    Wang, Dongjiang
    Gao, Houxiu
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2006, 22 (04) : 529 - 532
  • [29] Study on the Reliability of Carbon Nanotube-Reinforced Sn-58Bi Lead-Free Solder Joints
    Li Yang
    Haixiang Liu
    Yaocheng Zhang
    Huakuan Yu
    Journal of Materials Engineering and Performance, 2017, 26 : 6028 - 6036
  • [30] Study on the Reliability of Carbon Nanotube-Reinforced Sn-58Bi Lead-Free Solder Joints
    Yang, Li
    Liu, Haixiang
    Zhang, Yaocheng
    Yu, Huakuan
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (12) : 6028 - 6036