A Reliability Study of Nanoparticles Reinforced Composite Lead-Free Solder

被引:21
|
作者
Chen, Si [1 ,2 ]
Zhang, Lili [1 ,2 ]
Liu, Johan [1 ,2 ,3 ,4 ]
Gao, Yulai [5 ]
Zhai, Qijie [5 ]
机构
[1] Shanghai Univ, Key Lab Adv Display & Syst Applicat, Shanghai 200072, Peoples R China
[2] Shanghai Univ, SMIT Ctr, Sch Automat & Mech Engn, Shanghai 200072, Peoples R China
[3] Chalmers Univ Technol, SMIT Ctr, SE-41296 Gothenburg, Sweden
[4] Chalmers Univ Technol, Bionano Syst Lab, Dept Microtechnol & Nanosci, SE-41296 Gothenburg, Sweden
[5] Shanghai Univ, Sch Mat Sci & Engn, Shanghai 200072, Peoples R China
基金
美国国家科学基金会;
关键词
composite solder; nanoparticles; shear strength; thermal cycling; fracture mode;
D O I
10.2320/matertrans.MJ201002
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This work looks at the development and investigation of a reinforced composite solder with low melting point The composite solder was prepared by adding Sn 3 0Ag 0 5Cu nanoparticles Into Sn 58BI solder paste 1 he Sn 3 0Ag 0 5Cu nanoparticles were manufactured using a self developed Consumable electrode Direct Current Arc (CDCA) technique The test FR 4 Printed Circuit Board (PCB) with Cu pad and Electroless Nickel Immersion Gold (ENIG) surface finish were fabricated and fifty SR1206 chip resistors were mounted on pads of test PCB with the reinforced composite solder paste by using conventional surface mount technology The differential scanning calorimetry (DSC) was used to analyze the constituent of the composite solder Joint after reflow A scanning electron microscope (SEM) transmission electron microscope (TEM) and optical microscope (OM) were employed in order to observe the morphology of nanoparticles the microstructure of reinforced composite solder Joint the crack initiation and propagation in solder Joint and the fracture mode after shear test The thermal cycling (TC) was carried out with a temperature range of 40 degrees C and 125 C The contract resistance of the solder Joint was measured during thermal cycling and the shear test of solder Joints was performed before and after 500 thermal cycles After the shear test all fracture surfaces were inspected to identify the fracture mode of the composite solder joint The results of the experiments detailed in this work indicate that the shear strength of the composite solder increased 2 times in comparison to Sn 58B(1) Meanwhile the thermomechanical fatigue (TMF) resistance of the composite solder with 1 mass% nanoparticles was 16 times stronger than Sn 58BI and 4 times stronger than Sn 3 0Ag 0 5Cu However the tendency of forming micro cracks between nanoparticles and solder matrix and the fracture within solder was increased for solder joints with more than 3 mass% nanoparticles after thermal cycling [doi 10.2320/matertrans.MJ201002].
引用
收藏
页码:1720 / 1726
页数:7
相关论文
共 50 条
  • [1] Present Research Status of Lead-free Solder Reinforced by Nanoparticles
    Wang J.
    Xue S.
    Lyu Z.
    Wang L.
    Liu H.
    Cailiao Daobao/Materials Reports, 2019, 33 (07): : 2133 - 2145
  • [2] Synthesis and characterization of ceramic nanoparticles reinforced lead-free solder
    Fathian, Zahra
    Maleki, Ali
    Niroumand, Behzad
    CERAMICS INTERNATIONAL, 2017, 43 (06) : 5302 - 5310
  • [3] Reliability of lead-free solder alloys
    Igoshev, V
    Kleiman, J
    ENVIRONMENT CONSCIOUS MATERIALS - ECOMATERIALS, 2000, : 703 - 715
  • [4] Reliability of solder joints assembled with lead-free solder
    Ochiai, Masayuki
    Akamatsu, Toshiya
    Ueda, Hidefumi
    2002, Fujitsu Ltd (38):
  • [5] Reliability of solder joints assembled with lead-free solder
    Ochiai, M
    Akamatsu, T
    Ueda, H
    FUJITSU SCIENTIFIC & TECHNICAL JOURNAL, 2002, 38 (01): : 96 - 101
  • [6] The Effect of Thermal Cycling on Nanoparticle Reinforced Composite Lead-free Solder
    Chen, Si
    Cheng, Zhaonian
    Liu, Johan
    Gao, Yulai
    Zhai, Qijie
    2009 INTERNATIONAL CONFERENCE ON ELECTRONIC PACKAGING TECHNOLOGY & HIGH DENSITY PACKAGING (ICEPT-HDP 2009), 2009, : 1159 - +
  • [7] A study on μBGA solder joints reliability using lead-free solder materials
    Shin, YE
    Lee, JH
    Koh, YW
    Lee, CW
    Yun, JH
    Jung, SB
    KSME INTERNATIONAL JOURNAL, 2002, 16 (07): : 919 - 926
  • [8] A study on μBGA solder joints reliability using lead-free solder materials
    Young-Eui Shin
    Jun Hwan Lee
    Young-Wook Koh
    Chong-Won Lee
    Jun Ho Yun
    Seung-Boo Jung
    KSME International Journal, 2002, 16 : 919 - 926
  • [9] Reliability of lead-free solder interconnects - A review
    Tonapi, S
    Gopakumar, S
    Borgesen, P
    Srihari, K
    ANNUAL RELIABILITY AND MAINTAINABILITY SYMPOSIUM, 2002 PROCEEDINGS, 2002, : 423 - 428
  • [10] Reliability Testing of Lead-Free Solder Joints
    Bazu, Marius
    Ilian, Virgil Emil
    Galateanu, Lucian
    Varsescu, Dragos
    Pietrikova, Alena
    2012 35TH INTERNATIONAL SPRING SEMINAR ON ELECTRONICS TECHNOLOGY (ISSE 2012): POWER ELECTRONICS, 2012, : 173 - 177