High Temperature Erosion Behaviors of High V-Cr-Ni Spheroidal Carbides Cast Iron

被引:2
|
作者
Shimizu, Kazumichi [1 ]
Naruse, Takeshi [1 ]
Xinba, Yaer [1 ]
Teramachi, Hideki [2 ]
Araya, Shinji [1 ]
Ishida, Masahide [1 ]
机构
[1] Muroran Inst Technol, Mitumoto Cho 27-1, Muroran, Hokkaido 0508585, Japan
[2] TERAMACHI Co Ltd, Saijo, Japan
来源
关键词
Wear; Erosion; High temperature; Erosion rate; Hardness; ELEVATED-TEMPERATURE; COATINGS; WEAR;
D O I
10.4028/www.scientific.net/KEM.457.255
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
High temperature erosion occurs in production of the inorganic fibrous insulator in plant. Austenitic and martensitic stainless steels are often used for these severe high temperature erosion conditions. The paper presents erosion properties of some stainless steels, several cast iron and cast steel using a blast type high temperature erosion furnace. The solid particle erosion behavior at high temperatures (900 degrees C) of carbon steel of S50C, carbon tool steel of SK3, SUS403, SUS630, and High V-Cr-Ni spheroidal carbides cast iron (SCI-VCrNi) are investigated. Alumina balls entrained in a stream of hot air impact on the target materials at an air velocity of 100 m/s. the impingement angle is 90 degrees. The influence of the test temperature and the material removal are discussed. The high temperature erosion behaviors of specimens are discussed by the eroded surface morphology and vertical section observation using SEM and optical microscopy observations.
引用
收藏
页码:255 / +
页数:2
相关论文
共 50 条
  • [41] Effect of aluminum on the primary carbides of a hypereutectic high chromium cast iron
    Zhi, X.
    Han, Y.
    Lui, J.
    MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 2015, 46 (01) : 33 - 39
  • [42] Effect of vanadium and chromium on the microstructural features of V–Cr–Mn–Ni spheroidal carbide cast irons
    V.G.Efremenko
    K.Shimizu
    A.P.Cheiliakh
    T.V.Kozarevskaya
    K.Kusumoto
    K.Yamamoto
    International Journal of Minerals Metallurgy and Materials, 2014, 21 (11) : 1096 - 1108
  • [43] Obtaining of High Cr Content Cast Iron Materials
    Florea, C.
    Bejinariu, C.
    Carcea, I.
    Cimpoesu, N.
    Chicet, D. L.
    Savin, C.
    INTERNATIONAL CONFERENCE ON INNOVATIVE RESEARCH - ICIR EUROINVENT 2017, 2017, 209
  • [44] High Temperature Oxidation Behavior of Flake and Spheroidal Graphite Cast Irons
    Lin, Meng-Bin
    Wang, Chaur-Jeng
    Volinsky, Alex A.
    OXIDATION OF METALS, 2011, 76 (3-4): : 161 - 168
  • [45] High Temperature Oxidation Behavior of Flake and Spheroidal Graphite Cast Irons
    Meng-Bin Lin
    Chaur-Jeng Wang
    Alex A. Volinsky
    Oxidation of Metals, 2011, 76 : 161 - 168
  • [46] Zirconium carbide dispersed high Cr-Ni cast iron produced by plasma spraying
    Hoshiyama, Yasuhiro
    Miyazaki, Tsutomu
    Miyake, Hidekazu
    SURFACE & COATINGS TECHNOLOGY, 2013, 228 : S7 - S10
  • [47] Friction welding of high Cr white cast iron to AISI 1030 steel with Ni interlayer
    Teker, Tanju
    Karakurt, Eyyup Murat
    MATERIALS TESTING, 2021, 63 (11) : 1012 - 1017
  • [48] Lifespan of relaxed high toughness spheroidal-graphite cast iron after retightening under conditions of variable high temperature and plasticity
    Dai, Su-Jiang
    Zhang, Wei-Zheng
    Yuan, Yan-Peng
    Zhao, Wei-Mao
    Jilin Daxue Xuebao (Gongxueban)/Journal of Jilin University (Engineering and Technology Edition), 2010, 40 (04): : 1005 - 1008
  • [49] The high temperature property of Ni/WC infiltrated composite layer on cast iron substrate
    Yang, Gui-rong
    Song, Wen-ming
    Sun, Xian-ming
    Ma, Ying
    Lu, Jin-jun
    Hao, Yuan
    Li, Yuan-dong
    Wang, Hai-tang
    MANUFACTURING SCIENCE AND ENGINEERING, PTS 1-5, 2010, 97-101 : 1295 - +
  • [50] BAINITIC HIGH-STRENGTH CAST-IRON WITH SPHEROIDAL GRAPHITE (REVIEW)
    VORONENKO, BI
    ROMATOVSKII, YI
    METAL SCIENCE AND HEAT TREATMENT, 1991, 33 (9-10) : 762 - 771