High Temperature Erosion Behaviors of High V-Cr-Ni Spheroidal Carbides Cast Iron

被引:2
|
作者
Shimizu, Kazumichi [1 ]
Naruse, Takeshi [1 ]
Xinba, Yaer [1 ]
Teramachi, Hideki [2 ]
Araya, Shinji [1 ]
Ishida, Masahide [1 ]
机构
[1] Muroran Inst Technol, Mitumoto Cho 27-1, Muroran, Hokkaido 0508585, Japan
[2] TERAMACHI Co Ltd, Saijo, Japan
来源
关键词
Wear; Erosion; High temperature; Erosion rate; Hardness; ELEVATED-TEMPERATURE; COATINGS; WEAR;
D O I
10.4028/www.scientific.net/KEM.457.255
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
High temperature erosion occurs in production of the inorganic fibrous insulator in plant. Austenitic and martensitic stainless steels are often used for these severe high temperature erosion conditions. The paper presents erosion properties of some stainless steels, several cast iron and cast steel using a blast type high temperature erosion furnace. The solid particle erosion behavior at high temperatures (900 degrees C) of carbon steel of S50C, carbon tool steel of SK3, SUS403, SUS630, and High V-Cr-Ni spheroidal carbides cast iron (SCI-VCrNi) are investigated. Alumina balls entrained in a stream of hot air impact on the target materials at an air velocity of 100 m/s. the impingement angle is 90 degrees. The influence of the test temperature and the material removal are discussed. The high temperature erosion behaviors of specimens are discussed by the eroded surface morphology and vertical section observation using SEM and optical microscopy observations.
引用
收藏
页码:255 / +
页数:2
相关论文
共 50 条
  • [31] PRODUCTION OF HIGH-QUALITY SPHEROIDAL CAST IRON - EXPERIMENTS AND RESULTS
    MAYER, H
    HAMMERLI.F
    FONDERIE-FRANCE, 1971, 26 (298): : 71 - &
  • [32] HIGH-STRENGTH BAINITIC CAST-IRON WITH SPHEROIDAL GRAPHITE
    DORAZIL, E
    BARTA, B
    CRHAK, J
    MUNSTEROVA, E
    METAL SCIENCE AND HEAT TREATMENT, 1978, 20 (7-8) : 532 - 535
  • [33] High-cycle fatigue behaviour of spheroidal graphite cast iron
    Agha, HY
    Beranger, AS
    Billardon, R
    Hild, F
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 1998, 21 (03) : 287 - 296
  • [34] Fatigue of a spheroidal graphite cast iron in the very high cycle range
    Wang, QY
    Bathias, C
    Rathery, S
    Bérard, JY
    REVUE DE METALLURGIE-CAHIERS D INFORMATIONS TECHNIQUES, 1999, 96 (02): : 221 - 226
  • [35] STRUCTURE, NUCLEATION, GROWTH AND MORPHOLOGY OF SECONDARY CARBIDES IN HIGH CHROMIUM AND CR-NI WHITE CAST IRONS
    POWELL, GLF
    LAIRD, G
    JOURNAL OF MATERIALS SCIENCE, 1992, 27 (01) : 29 - 35
  • [36] Influence of high temperature aging on the carbides of 25Cr35Ni-Nb alloys
    Lian, Xiaoming
    Chen, Xuedong
    Lv, Yunrong
    Chen, Tao
    STRUCTURAL INTEGRITY IN NUCLEAR ENGINEERING, 2011, : 181 - 185
  • [37] Development of a Ni–Cr–Mo–V Alloyed Ductile Iron with High Hardness
    Chao Yang
    Zhijie Gao
    Yuzhou Du
    Ke Wang
    Bailing Jiang
    International Journal of Metalcasting, 2024, 18 : 1677 - 1685
  • [38] Development of refinement of the primary carbides in high chromium white cast iron
    Wu, Xiao-Jun
    Xing, Jian-Dong
    Fu, Han-Guang
    Zhi, Xiao-Hui
    Zhuzao/Foundry, 2006, 55 (10): : 999 - 1003
  • [39] Effect of niobium on primary carbides of hypereutectic high chromium cast iron
    Zhi, X. H.
    Wang, J. X.
    IRONMAKING & STEELMAKING, 2014, 41 (05) : 394 - 399
  • [40] Morphology and Material Properties of Carbides in High (24%) Chromium Cast Iron
    Orlowicz, A. W.
    Mroz, M.
    Tupaj, M.
    Trytek, A.
    Jacek, M.
    Radon, M.
    ARCHIVES OF FOUNDRY ENGINEERING, 2018, 18 (01) : 77 - 80