Ternary TiAlGe ohmic contacts for p-type 4H-SiC

被引:13
|
作者
Sakai, T [1 ]
Nitta, K [1 ]
Tsukimoto, S [1 ]
Moriyama, M [1 ]
Murakami, M [1 ]
机构
[1] Kyoto Univ, Dept Mat Sci & Engn, Kyoto 6068501, Japan
关键词
D O I
10.1063/1.1643772
中图分类号
O59 [应用物理学];
学科分类号
摘要
Reduction of annealing temperature to prepare low resistance ohmic contact materials for p-type 4H-SiC was achieved by adding Ge to the conventional TiAl contacts. Although the binary TiAl contact is required to anneal at temperature as high as 1000degreesC to convert Schottky to ohmic behavior after deposition of the Ti and Al layers on the SiC substrate, the GeTiAl contacts provided the specific contact resistance of about 1x10(-4) Omega cm(2) by annealing at temperature as low as 600degreesC. This low annealing temperature is desirable to reduce the gate leakage current of the SiC devices. The GeTiAl ohmic contacts were thermally stable during isothermal annealing at 400degreesC subsequently after preparing the ohmic contacts by annealing at 600degreesC, which is also required by the device packaging process. (C) 2004 American Institute of Physics.
引用
收藏
页码:2187 / 2189
页数:3
相关论文
共 50 条
  • [41] Reliable ohmic contacts to LPE p-type 4H-SiC for high-power p-n diode
    (Trans Tech Publications Ltd): : 389 - 393
  • [42] Role of interface layers and localized states in TiAl-based ohmic contacts to p-type 4H-SiC
    Gao, M.
    Tsukimoto, S.
    Goss, S. H.
    Tumakha, S. P.
    Onishi, T.
    Murakami, M.
    Brillson, L. J.
    JOURNAL OF ELECTRONIC MATERIALS, 2007, 36 (04) : 277 - 284
  • [43] Role of Interface Layers and Localized States in TiAl-Based Ohmic Contacts to p-Type 4H-SiC
    M. Gao
    S. Tsukimoto
    S.H. Goss
    S.P. Tumakha
    T. Onishi
    M. Murakami
    L.J. Brillson
    Journal of Electronic Materials, 2007, 36 : 277 - 284
  • [44] Study of Ni/Al/Au ohmic contacts to p-Type 4H-SiC applied in 600 °C environment
    Lei, Cheng
    Li, Qiang
    Liang, Ting
    Liu, RuiFang
    Li, YongWei
    Zhou, XingJian
    Jia, Pinggang
    Ghaffar, Abdul
    Xiong, JiJun
    JOURNAL OF CRYSTAL GROWTH, 2022, 592
  • [45] Characterization of Ti/Al ohmic contacts to p-type 4H-SiC using cathodoluminescence and Auger electron spectroscopies
    Gao, M.
    Tumakha, S. P.
    Onishi, T.
    Tsukimoto, S.
    Murakami, M.
    Brillson, L. J.
    Silicon Carbide and Related Materials 2005, Pts 1 and 2, 2006, 527-529 : 891 - 894
  • [46] Aluminum Doping by Low-temperature Homoepitaxial Growth for Ni Ohmic Contacts to p-type 4H-SiC
    Krishnan, Bharat
    Kotamraju, Siva Prasad
    Melnychuk, Galyna
    Merrett, Neil
    Koshka, Yaroslav
    SILICON CARBIDE AND RELATED MATERIALS 2008, 2009, 615-617 : 581 - 584
  • [47] Improved ohmic contacts to p-type 6H-SiC
    Spiess, L
    Nennewitz, O
    Pezoldt, J
    SILICON CARBIDE AND RELATED MATERIALS 1995, 1996, 142 : 585 - 588
  • [48] Comparison of Electrical Properties of Ohmic Contact Realized on p-type 4H-SiC
    Nguyen, D. M.
    Raynaud, C.
    Lazar, M.
    Vang, H.
    Planson, D.
    SILICON CARBIDE AND RELATED MATERIALS 2007, PTS 1 AND 2, 2009, 600-603 : 639 - 642
  • [49] Study of the electrical, thermal and chemical properties of Pd ohmic contacts to p-type 4H-SiC: Dependence on annealing conditions
    Institute of Applied Physics, BAS, 59, St. Petersburg blvd., 4000 Plovdiv, Bulgaria
    不详
    不详
    Mater Sci Eng B Solid State Adv Technol, (291-295):
  • [50] Correlation between the electrical properties and the interfacial microstructures of TiAl-based ohmic contacts to p-type 4H-SiC
    Tsukimoto, S
    Nitta, K
    Sakai, T
    Moriyama, M
    Murakami, M
    JOURNAL OF ELECTRONIC MATERIALS, 2004, 33 (05) : 460 - 466