Ternary TiAlGe ohmic contacts for p-type 4H-SiC

被引:13
|
作者
Sakai, T [1 ]
Nitta, K [1 ]
Tsukimoto, S [1 ]
Moriyama, M [1 ]
Murakami, M [1 ]
机构
[1] Kyoto Univ, Dept Mat Sci & Engn, Kyoto 6068501, Japan
关键词
D O I
10.1063/1.1643772
中图分类号
O59 [应用物理学];
学科分类号
摘要
Reduction of annealing temperature to prepare low resistance ohmic contact materials for p-type 4H-SiC was achieved by adding Ge to the conventional TiAl contacts. Although the binary TiAl contact is required to anneal at temperature as high as 1000degreesC to convert Schottky to ohmic behavior after deposition of the Ti and Al layers on the SiC substrate, the GeTiAl contacts provided the specific contact resistance of about 1x10(-4) Omega cm(2) by annealing at temperature as low as 600degreesC. This low annealing temperature is desirable to reduce the gate leakage current of the SiC devices. The GeTiAl ohmic contacts were thermally stable during isothermal annealing at 400degreesC subsequently after preparing the ohmic contacts by annealing at 600degreesC, which is also required by the device packaging process. (C) 2004 American Institute of Physics.
引用
收藏
页码:2187 / 2189
页数:3
相关论文
共 50 条
  • [21] Electrical characteristics and structural properties of ohmic contacts to p-type 4H-SiC epitaxial layers
    Vasilevskii, KV
    Rendakova, SV
    Nikitina, IP
    Babanin, AI
    Andreev, AN
    Zekentes, K
    SEMICONDUCTORS, 1999, 33 (11) : 1206 - 1211
  • [22] Interface annealing characterization of Ti/Al/Au ohmic contacts to p-type 4H-SiC
    Han Chao
    Zhang Yuming
    Song Qingwen
    Tang Xiaoyan
    Guo Hui
    Zhang Yimen
    Yang Fei
    Niu Yingxi
    JOURNAL OF SEMICONDUCTORS, 2015, 36 (12)
  • [23] Temperature stable Pd ohmic contacts to p-type 4H-SiC formed at low temperatures
    Kassamakova, L
    Kakanakov, RD
    Kassamakov, IV
    Nordell, N
    Savage, S
    Hjörvarssön, B
    Svedberg, EB
    Åbom, L
    Madsen, LD
    IEEE TRANSACTIONS ON ELECTRON DEVICES, 1999, 46 (03) : 605 - 611
  • [24] Ni/W/Ni ohmic contacts for both n- and p-type 4H-SiC
    Dongwoo Bae
    Gilcho Ahn
    Chungbu Jeong
    Kwangsoo Kim
    Electrical Engineering, 2018, 100 : 2431 - 2437
  • [25] Investigations on Ni-Ti-Al ohmic contacts obtained on p-type 4H-SiC
    Laariedh, F.
    Lazar, M.
    Cremillieu, P.
    Leclercq, J. -L.
    Planson, D.
    HETEROSIC & WASMPE 2011, 2012, 711 : 169 - +
  • [26] Electrical characteristics and structural properties of ohmic contacts to p-type 4H-SiC epitaxial layers
    K. V. Vasilevskii
    S. V. Rendakova
    I. P. Nikitina
    A. I. Babanin
    A. N. Andreev
    K. Zekentes
    Semiconductors, 1999, 33 : 1206 - 1211
  • [27] Ni/W/Ni ohmic contacts for both n- and p-type 4H-SiC
    Bae, Dongwoo
    Ahn, Gilcho
    Jeong, Chungbu
    Kim, Kwangsoo
    ELECTRICAL ENGINEERING, 2018, 100 (04) : 2431 - 2437
  • [28] Interface annealing characterization of Ti/Al/Au ohmic contacts to p-type 4H-SiC
    韩超
    张玉明
    宋庆文
    汤晓燕
    郭辉
    张义门
    杨霏
    钮应喜
    Journal of Semiconductors, 2015, 36 (12) : 57 - 65
  • [29] On the Ti3SiC2 Metallic Phase Formation for p-type 4H-SiC Ohmic Contacts
    Jennings, M. R.
    Fisher, C. A.
    Walker, D.
    Sanchez, A.
    Perez-Tomas, A.
    Hamilton, D. P.
    Gammon, P. M.
    Burrows, S. E.
    Thomas, S. M.
    Sharma, Y.
    Li, F.
    Mawby, P. A.
    SILICON CARBIDE AND RELATED MATERIALS 2013, PTS 1 AND 2, 2014, 778-780 : 693 - +
  • [30] Thermal stability study of n-type and p-type ohmic contacts simultaneously formed on 4H-SiC
    Zhang, Yimeng
    Guo, Tao
    Tang, Xiaoyan
    Yang, Jie
    He, Yanjing
    Zhang, Yuming
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 731 : 1267 - 1274