Pressureless joining of silicon carbide using Ti3SiC2 MAX phase at 1500°C

被引:21
|
作者
Ma, Hai-Bin [1 ]
Xue, Jia-Xiang [1 ]
Zhai, Jian-Han [1 ]
Liu, Tong [1 ]
Ren, Qi-Sen [1 ]
Liao, Ye-Hong [1 ]
Wu, Li-Xiang [2 ]
Guo, Wei-Ming [2 ]
Sun, Shi-Kuan [2 ]
Lin, Hua-Tay [2 ]
机构
[1] China Nucl Power Technol Res Inst, ATF Res & Dev Ctr, Shenzhen 518026, Peoples R China
[2] Guangdong Univ Technol, Sch Electromech Engn, Guangzhou 510090, Guangdong, Peoples R China
基金
国家重点研发计划;
关键词
Silicon carbide; Pressureless joining; Microstructure; Shear strength; C/SIC COMPOSITE JOINTS; SHEAR-STRENGTH; CERAMICS; TI; MICROSTRUCTURE; INTERLAYER; IRRADIATION; COMPONENTS; TI3ALC2; METAL;
D O I
10.1016/j.ceramint.2020.02.155
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Silicon carbide ceramics were pressureless joined by using Ti foil and Si powder, which generated Ti3SiC2 phase as the interlayer. The phase composition, microstructure and the shear strength were investigated. It was revealed that the SiC assembly after joining at 1500 degrees C showed the high shear strength of 76.2 +/- 19.5 MPa. The secondary phase of TiC within the interlayer was expected to contribute to densification improvement of Ti3SiC2 phase and thermal stress reduction.
引用
收藏
页码:14269 / 14272
页数:4
相关论文
共 50 条
  • [31] Basal Plane Delamination Energy Measurement in a Ti3SiC2 MAX Phase
    Gavalda-Diaz, Oriol
    Lyons, Jack
    Wang, Siyang
    Emmanuel, Max
    Marquardt, Katharina
    Saiz, Eduardo
    Giuliani, Finn
    JOM, 2021, 73 (06) : 1582 - 1588
  • [32] Research Progress in MAX Phase Ti3SiC2 Highly Conductive Coating
    Zhu, Jie
    Zhang, Fangzhou
    Xie, Youju
    Jia, Lintao
    Wang, Mengqian
    Li, Aijun
    Cailiao Daobao/Materials Reports, 2021, 35 (23): : 23025 - 23032
  • [33] Fabrication of Ti3SiC2 and Ti4SiC3 MAX phase ceramics through reduction of TiO2 with SiC
    Istomin, Pavel
    Istomina, Elena
    Nadutkin, Aleksandr
    Grass, Vladislav
    Leonov, Aleksandr
    Kaplan, Mikhail
    Presniakov, Mikhail
    CERAMICS INTERNATIONAL, 2017, 43 (18) : 16128 - 16135
  • [34] Shock compaction of the titanium-silicon ternary carbide (Ti3SiC2) powders
    Georgia Inst of Technology, Atlanta, United States
    Ceram Eng Sci Proc, 4 (427-434):
  • [35] Shock compaction and synthesis of the titanium-silicon ternary carbide (Ti3SiC2)
    Jordan, JL
    Thadhani, NN
    SHOCK COMPRESSION OF CONDENSED MATTER-1999, PTS 1 AND 2, 2000, 505 : 755 - 758
  • [36] Synthesis of Ti3SiC2 by pressureless sintering of the elemental powders in vacuum
    Li, H
    Chen, D
    Zhou, J
    Zhao, JH
    He, LH
    MATERIALS LETTERS, 2004, 58 (11) : 1741 - 1744
  • [37] Effect of Al addition on pressureless reactive sintering of Ti3SiC2
    Sun, ZhengMing
    Zou, Yong
    Tada, Shuji
    Hashimoto, Hitoshi
    SCRIPTA MATERIALIA, 2006, 55 (11) : 1011 - 1014
  • [38] Injection moulding of porous MAX phase Ti3SiC2 without using space-holder
    Tabares, Eduardo
    Cifuentes, Sandra C.
    Jimenez-Morales, Antonia
    Tsipas, Sophia A.
    POWDER TECHNOLOGY, 2021, 380 : 96 - 105
  • [39] Synthesize Ti3SiC2 from TiH2 by Pressureless Sintering
    Li, Liang
    Zhou, Aiguo
    Wang, Libo
    Hu, Feixiang
    HIGH-PERFORMANCE CERAMICS VII, PTS 1 AND 2, 2012, 512-515 : 676 - 680
  • [40] The phase and morphological evolution of Ti3SiC2 MAX phase powder after HF treatment
    Aghamohammadi, Hamed
    Heidarpour, Akbar
    Jamshidi, Rasoul
    CERAMICS INTERNATIONAL, 2018, 44 (15) : 17992 - 18000