Effects of Sr-modification, iron-based intermetallics and aging treatment on the impact toughness of 356 Al-Si-Mg alloy

被引:55
|
作者
Elsebaie, O. [1 ]
Samuel, A. M. [1 ]
Samuel, F. H. [1 ,2 ,3 ]
机构
[1] Univ Quebec Chicoutimi, Chicoutimi, PQ, Canada
[2] King Saud Univ, Coll Engn, Riyadh, Saudi Arabia
[3] Ctr Excellence Res Engn Mat, Riyadh, Saudi Arabia
基金
加拿大自然科学与工程研究理事会;
关键词
CASTING ALLOYS; BEHAVIOR; SOLIDIFICATION;
D O I
10.1007/s10853-010-5181-1
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Impact toughness as a property has been acquiring increased importance in recent years, since data regarding this property can provide a means for assessing alloy ductility under high rates of deformation. The main objective of this study is to investigate the effects of Sr-modification, Fe-based intermetallic phases and aging conditions on the impact toughness of widely used 356 alloys. The total absorbed energy was measured using a computer-aided instrumented Instron Charpy impact testing machine. Increasing the level of iron additions decreases the impact energy values of 356 alloys to a noticeable degree (similar to 35-57%). The addition of 0.1 wt% Mn to non-modified 356 alloys seems to have no observable effect on the impact energy, while increasing the Mn addition to 0.4 wt% produces a slight improvement in the impact energy values for non-modified and Sr-modified 356 alloys compared to that of those containing only iron under the same conditions. The application of solution heat treatment in combination with Sr-modification was found to significantly improve the impact energy of as-cast 356 alloys, particularly at low iron additions. Artificial aging of non-modified and Sr-modified 356 alloys at 180 A degrees C diminishes the impact energy values with an increase in the aging time up to 8 h compared to those obtained under the solution heat-treated conditions. On the other hand, aging at 220 A degrees C for 12 h increases the impact energy values of Sr-modified 356 alloy containing 0.12 wt% Fe and combined 0.2 wt% Fe-0.1 wt% Mn to about 20 and 18 J, respectively. The fracture behavior of non-modified 356 alloys containing 0.12 wt% Fe is mainly controlled by the acicular eutectic Si particles whereas beta-iron platelets act as crack initiation sites and provide further path for final crack propagation in non-modified 356 alloys containing 0.9 wt% Fe. The beta-iron platelets and pi-iron phase particles contribute largely to crack initiation and propagation in the Sr-modified 356 alloys containing 0.9 wt% Fe.
引用
收藏
页码:3027 / 3045
页数:19
相关论文
共 42 条
  • [31] Effects of Cu and Zr Addition on the Tensile Properties, Corrosion Characteristics and Interfacial Compounds with Cast Iron of Al-Si-Mg Alloy for Compound Casting
    Min, Kyoung-Min
    Jung, Ki-Chae
    Shin, Je-Sik
    Kim, Jeong-Min
    KOREAN JOURNAL OF MATERIALS RESEARCH, 2023, 33 (01): : 8 - 14
  • [32] Effects of melt thermal rate treatment and modification of P and RE on hypereutectic Al-Si-Cu-Mg alloy
    Wang, Q. L.
    Geng, H. R.
    Zuo, M.
    Long, F.
    Peng, X.
    MATERIALS SCIENCE AND TECHNOLOGY, 2013, 29 (10) : 1233 - 1240
  • [33] Effects of Heat Treatment on the Microstructure, Impact Toughness and Fracture Strength of Al-6Si-2Cu Cast Alloy
    Hossain, Abul
    Gulshan, Fahmida
    Kurny, A. S. W.
    PROCEEDINGS OF THE 12TH INTERNATIONAL CONFERENCE ON MECHANICAL ENGINEERING (ICME 2017), 2018, 1980
  • [34] Effects of Solution Treatment on the Microstructure, Tensile Properties, and Impact Toughness of an Al-5.0Mg-3.0Zn-1.0Cu Cast Alloy
    Tang, Hua-Ping
    Wang, Qu-Dong
    Luo, Colin
    Lei, Chuan
    Liu, Tian-Wen
    Li, Zhong-Yang
    Wang, Kui
    Jiang, Hai-Yan
    Ding, Wen-Jiang
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2021, 34 (01) : 98 - 110
  • [35] Effects of solution treatment temperature and time on the porosities and mechanical properties of vacuum die-casted and T6 heat-treated Al-Si-Mg alloy
    Kang, Ho-jung
    Jang, Ho-sung
    Oh, Seong-hyo
    Yoon, Pil-hwan
    Lee, Gyu-heun
    Park, Jin-young
    Kim, Eok-soo
    Choi, Yoon-suk
    VACUUM, 2021, 193
  • [36] Effects of Solution Treatment on the Microstructure,Tensile Properties,and Impact Toughness of an Al–5.0Mg–3.0Zn–1.0Cu Cast Alloy
    Hua-Ping Tang
    Qu-Dong Wang
    Colin Luo
    Chuan Lei
    Tian-Wen Liu
    Zhong-Yang Li
    Kui Wang
    Hai-Yan Jiang
    Wen-Jiang Ding
    ActaMetallurgicaSinica(EnglishLetters), 2021, 34 (01) : 98 - 110
  • [37] Effects of Solution Treatment on the Microstructure, Tensile Properties, and Impact Toughness of an Al–5.0Mg–3.0Zn–1.0Cu Cast Alloy
    Hua-Ping Tang
    Qu-Dong Wang
    Colin Luo
    Chuan Lei
    Tian-Wen Liu
    Zhong-Yang Li
    Kui Wang
    Hai-Yan Jiang
    Wen-Jiang Ding
    Acta Metallurgica Sinica (English Letters), 2021, 34 : 98 - 110
  • [38] Effect of Aging Treatment Temperature on Microstructure and Properties of Al-9.3Si-0.41Mg-0.2Zr-0.01Sr-0.08Ti-0.2Ce Cast Aluminum Alloy
    Wang, Qin
    Zhou, Qingshan
    Liu, Lele
    Xu, Xiaojing
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024,
  • [39] Effects of dynamic cooling pre-aging treatment on mechanical properties and paint-bake hardening behavior of Al-Mg-Si alloy automotive sheets
    Gao Guan-jun
    Li Xi-wu
    Yan Li-zhen
    Xiong Bai-qing
    Li Zhi-hui
    Zhang Yong-an
    Wen Kai
    Li Ya-nan
    JOURNAL OF CENTRAL SOUTH UNIVERSITY, 2022, 29 (03) : 950 - 959
  • [40] Effects of an electric field applied during the solution heat treatment of the Al-Mg-Si-Cu alloy AA6111 on the subsequent natural aging kinetics and tensile properties
    Jung, K
    Conrad, H
    ZEITSCHRIFT FUR METALLKUNDE, 2006, 97 (02): : 145 - 149