Effects of Sr-modification, iron-based intermetallics and aging treatment on the impact toughness of 356 Al-Si-Mg alloy

被引:55
|
作者
Elsebaie, O. [1 ]
Samuel, A. M. [1 ]
Samuel, F. H. [1 ,2 ,3 ]
机构
[1] Univ Quebec Chicoutimi, Chicoutimi, PQ, Canada
[2] King Saud Univ, Coll Engn, Riyadh, Saudi Arabia
[3] Ctr Excellence Res Engn Mat, Riyadh, Saudi Arabia
基金
加拿大自然科学与工程研究理事会;
关键词
CASTING ALLOYS; BEHAVIOR; SOLIDIFICATION;
D O I
10.1007/s10853-010-5181-1
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Impact toughness as a property has been acquiring increased importance in recent years, since data regarding this property can provide a means for assessing alloy ductility under high rates of deformation. The main objective of this study is to investigate the effects of Sr-modification, Fe-based intermetallic phases and aging conditions on the impact toughness of widely used 356 alloys. The total absorbed energy was measured using a computer-aided instrumented Instron Charpy impact testing machine. Increasing the level of iron additions decreases the impact energy values of 356 alloys to a noticeable degree (similar to 35-57%). The addition of 0.1 wt% Mn to non-modified 356 alloys seems to have no observable effect on the impact energy, while increasing the Mn addition to 0.4 wt% produces a slight improvement in the impact energy values for non-modified and Sr-modified 356 alloys compared to that of those containing only iron under the same conditions. The application of solution heat treatment in combination with Sr-modification was found to significantly improve the impact energy of as-cast 356 alloys, particularly at low iron additions. Artificial aging of non-modified and Sr-modified 356 alloys at 180 A degrees C diminishes the impact energy values with an increase in the aging time up to 8 h compared to those obtained under the solution heat-treated conditions. On the other hand, aging at 220 A degrees C for 12 h increases the impact energy values of Sr-modified 356 alloy containing 0.12 wt% Fe and combined 0.2 wt% Fe-0.1 wt% Mn to about 20 and 18 J, respectively. The fracture behavior of non-modified 356 alloys containing 0.12 wt% Fe is mainly controlled by the acicular eutectic Si particles whereas beta-iron platelets act as crack initiation sites and provide further path for final crack propagation in non-modified 356 alloys containing 0.9 wt% Fe. The beta-iron platelets and pi-iron phase particles contribute largely to crack initiation and propagation in the Sr-modified 356 alloys containing 0.9 wt% Fe.
引用
收藏
页码:3027 / 3045
页数:19
相关论文
共 42 条
  • [21] Effect of iron content and heat treatment on microstructure and mechanical properties of a recycled Al-Si-Mg aluminum alloy
    Sha Lan
    Gang Feng
    Yajun Wang
    Jinsheng Zhang
    Fujian Gong
    Chun Wang
    Jianhua Zhao
    Qing Yang
    Zhibai Wang
    China Foundry, 2025, 22 (02) : 205 - 214
  • [22] Refining and modification effects of (Al, Zr, Si)-Al4Sr on Al-7Si-0.5 Mg alloy
    Ding, Jinhua
    Lu, Cheng
    Sun, Yijiao
    Cui, Chunxiang
    Zhao, Ertuan
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2021, 15 : 1604 - 1612
  • [23] Modification and refinement effects of Sb and Sr on Mg17Al12 and Mg2Si phases in Mg-12Al-0.7Si alloy
    Zhi-wen Wang
    Hong-xia Wang
    Jia-lin Gong
    Ming Li
    Wei-li Cheng
    Wei Liang
    China Foundry, 2016, 13 (05) : 310 - 315
  • [24] Modification and refinement effects of Sb and Sr on Mg17Al12 and Mg2Si phases in Mg-12Al-0.7Si alloy
    Wang, Zhi-wen
    Wang, Hong-xia
    Gong, Jia-lin
    Li, Ming
    Cheng, Wei-li
    Liang, Wei
    CHINA FOUNDRY, 2016, 13 (05) : 310 - 315
  • [25] Modification and refinement effects of Sb and Sr on Mg17Al12 and Mg2Si phases in Mg-12Al-0.7Si alloy
    Zhi-wen Wang
    Hong-xia Wang
    Jia-lin Gong
    Ming Li
    Wei-li Cheng
    Wei Liang
    China Foundry, 2016, 13 : 310 - 315
  • [26] Effects of cold rolling on the aging kinetics in an Al-Mg-Si based commercial alloy
    Long, DC
    Ohmori, Y
    Nakai, K
    MATERIALS TRANSACTIONS JIM, 2000, 41 (06): : 690 - 695
  • [27] Structure of Iron-Based Cladding Layer on Al-Mg-Si Alloy Coated by a Resistance Seam Welding Method
    Wang, Wenqin
    Yamaguchi, Tomiko
    Nishio, Kazumasa
    MATERIALS TRANSACTIONS, 2014, 55 (11) : 1698 - 1706
  • [28] Impact toughness of Al-Si-Cu-Mg-Fe cast alloys: Effects of minor additives and aging conditions
    Elsebaie, Ossama
    Samuel, Agnes M.
    Samuel, F. H.
    Doty, H. W.
    MATERIALS & DESIGN, 2014, 60 : 496 - 509
  • [29] Effects of multiple-step thermal ageing treatment on the hardness characteristics of A356.0-type Al-Si-Mg alloy
    Abdulwahab, M.
    Madugu, I. A.
    Yaro, S. A.
    Hassan, S. B.
    Popoola, A. P. I.
    MATERIALS & DESIGN, 2011, 32 (03) : 1159 - 1166
  • [30] Modelling and Optimization for Heat Treatment of Al-Si-Mg Alloy Prepared by Indirect Squeeze Casting Based on Response Surface Methodology
    Chen, Liwen
    Zhao, Yuhong
    Wen, Zhiqin
    Tian, Jinzhong
    Hou, Hua
    MATERIALS RESEARCH-IBERO-AMERICAN JOURNAL OF MATERIALS, 2017, 20 (05): : 1274 - 1281