Characterisation of LPCVD silicon oxynitride films by optical spectroscopy

被引:0
|
作者
Bercu, M
Cobianu, C
Modreanu, M
Bercu, BN
机构
[1] Univ Bucharest, Fac Phys, Bucharest, Romania
[2] Natl Inst Res & Dev Microtechnol, Bucharest 72225, Romania
[3] Valahia Univ Targoviste, Fac Elect Engn, Bucharest, Romania
来源
JOURNAL DE PHYSIQUE IV | 2001年 / 11卷 / PR3期
关键词
D O I
暂无
中图分类号
O4 [物理学];
学科分类号
0702 ;
摘要
The Si-H and Si-N vibration modes contributions to IR absorption bands in the wave number range of 600-960 cm(-1) has been investigated for the as-deposited LPCVD SiON layers prepared at different N2O/NH3 ratios. The increasing of N/O atomic ratio was related to the specific changes of the Wide IR absorption band profile. The variation of the Si-O bonds population in the oxynitride films deposited on c-Si has been found by IR spectroscopy after post thermal annealing at 1050 degreesC in Wet O-2. The Si-O bonding in SiON film has been related to a sequence of two steps, indicated by the time dependency of the integral absorption band of the asymmetric stretching vibration mode at 1075cm(-1). We have found a fast increase of Si-O population after about 40 min of heating. The time dependency shows an almost a linear dependence versus t(1/2). The break of the slope is produced only after a preliminary low rate increase process in Si-O bonding, roughly speaking being 20 times smaller than in the second process. The high rate of Si-O bond formation at long annealing times has been found to be related to the removal of the low frequency wing of the Si-H stretching absorption band at about 2100 cm(-1). This feature is also connected to the already reported Si-H frequency shift in local tetraedra as a result to Si-O bonding. The annealing behaviour of both, the real and the imaginary part of the refractive index n*(lambda)=n(lambda)+ik(lambda) has been extracted using UV-VIS spectra simulation. The result indicates a systematic decrease of n and k with the heating time at 1050 degreesC in wet O-2, suggesting the increasing of oxygen content in SiON film, We have proposed a preliminary physical model for the Si-O bond formation in SiON at 1050C in wet O-2, based on two-step process. The first step assumes that at an early stage a local oxygen re-bonding to the tetraedra (like: Si[Si-2,A,H], where A can be N, OH, (NH)(2), or H) changes the local chemical structure by breaking Si-Si bonds, especially close to the gas/solid interface. The partial reconstruction of SiON layer in a hot and Wet O-2 atmosphere facilitates the incorporation of the oxidative species based on a diffusion limited process through a Si-O-Si network, embedded in the SiON film.
引用
下载
收藏
页码:963 / 969
页数:7
相关论文
共 50 条
  • [21] Vibrational spectroscopy characterization of magnetron sputtered silicon oxide and silicon oxynitride films
    Godinho, V.
    Denisov, V. N.
    Mavrin, B. N.
    Novikova, N. N.
    Vinogradov, E. A.
    Yakovlev, V. A.
    Fernandez-Ramos, C.
    Jimenez de Haro, M. C.
    Fernandez, A.
    APPLIED SURFACE SCIENCE, 2009, 256 (01) : 156 - 164
  • [22] ULTRA-THIN LPCVD SILICON OXYNITRIDE DIELECTRICS FOR VLSI
    PAN, P
    ABERNATHEY, J
    GEISS, P
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1987, 134 (11) : C626 - C626
  • [23] CHEMICAL-COMPOSITION OF LPCVD SILICON-NITRIDE AND SILICON OXYNITRIDE LAYERS
    KUIPER, AET
    HABRAKEN, FHPM
    VANOOSTROM, A
    TAMMINGA, Y
    PHILIPS JOURNAL OF RESEARCH, 1983, 38 (1-2) : 1 - 18
  • [24] Optical properties of silicon thin films related to LPCVD growth condition
    Modreanu, M
    Gartner, M
    Cobianu, C
    O'Looney, B
    Murphy, F
    THIN SOLID FILMS, 2004, 450 (01) : 105 - 110
  • [25] Spectroscopic ellipsometry characterisation of solid phase crystallisation of silicon thin films obtained by LPCVD
    Modreanu, M
    Gartner, M
    Cobianu, C
    Manea, E
    CAS: 2002 INTERNATIONAL SEMICONDUCTOR CONFERENCE, VOLS 1 AND 2, PROCEEDINGS, 2001, : 287 - 290
  • [26] Characterization of silicon oxynitride thin films by infrared reflection absorption spectroscopy
    Firon, M
    Bonnelle, C
    Mayeux, A
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A, 1996, 14 (04): : 2488 - 2492
  • [27] Characterization of silicon oxynitride thin films by infrared reflection absorption spectroscopy
    Firon, M.
    Bonnelle, C.
    Mayeux, A.
    Journal of Vacuum Science and Technology A: Vacuum, Surfaces and Films, 1996, 14 (04): : 2488 - 2492
  • [28] Electroluminescence in silicon oxynitride films
    Price, KJ
    Sharpe, LR
    McNeil, LE
    Irene, EA
    JOURNAL OF APPLIED PHYSICS, 1999, 86 (05) : 2638 - 2641
  • [29] Defects in silicon oxynitride films
    Futatsudera, M
    Kimura, T
    Matsumoto, A
    Inokuma, T
    Kurata, Y
    Hasegawa, S
    THIN SOLID FILMS, 2003, 424 (01) : 148 - 151
  • [30] ISSUES ON SILICON OXYNITRIDE FILMS
    STEIN, HJ
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1988, 135 (08) : C361 - C361