High temperature corrosion of B2 iron aluminides

被引:37
|
作者
Mignone, A [1 ]
Frangini, S
La Barbera, A
Tassa, O
机构
[1] ENEA CR Casaccia, Mat Div, Rome, Italy
[2] CSM Mat & Components Dept, Rome, Italy
关键词
FeAl; mechanical alloying; oxidation; microstructure;
D O I
10.1016/S0010-938X(98)00014-6
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The high temperature oxidation of two B2-Fe40A1 Iron Aluminides has been studied in isothermal and cyclic conditions in the range 700 degrees C to 1100 degrees C and compared with a FeCrAlY alloy. One of the aluminides was prepared by mechanical alloying with the addition of an Y2O3-dispersion that conferred to it improved mechanical properties. No significative differences in the isothermal oxidation of the aluminides have been observed due to the presence of the Y2O3. Both aluminides presented higher oxidation rates than the FeCrAlY alloy at 758 degrees and 858 degrees C but lower rates at 1118 degrees C. The tests carried out under thermal cycling (100 1-hour cycles: 40 minutes at 900 degrees C plus 20 minutes at room temperature) showed that the FeCrAlY alloy presented a lower weight increase than both Iron aluminides. Scanning electron microscopy observations revealed a similar acicular morphology of the thin oxide layer formed on the aluminides. The oxide grown on the FeCrAlY alloy presented nodule formation. (C) 1998 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:1331 / 1347
页数:17
相关论文
共 50 条
  • [41] Microstructural development and creep deformation in equiaxed γ, γ + α2, and γ + α2 + B2 titanium aluminides
    Ott E.A.
    Pollock T.M.
    Metallurgical and Materials Transactions A, 1998, 29 (13) : 965 - 978
  • [42] High temperature corrosion behaviour of nickel aluminides:: effects of chromium and zirconium
    Klöwer, J
    Brill, U
    Heubner, U
    INTERMETALLICS, 1999, 7 (10) : 1183 - 1194
  • [43] A review of the electrochemical corrosion behaviour of iron aluminides
    Rao, VS
    ELECTROCHIMICA ACTA, 2004, 49 (26) : 4533 - 4542
  • [44] The development of research progress on oxidation of iron aluminides intermetallics at high temperature
    Tan, Ping
    Chen, Jin-Mei
    Tang, Hui-Ping
    Wang, Jian-Yong
    Wang, Jian
    Yang, Bao-Jun
    Li, Ya-Ning
    Gongneng Cailiao/Journal of Functional Materials, 2012, 43 (SUPPL. 1): : 29 - 32
  • [45] HIGH-TEMPERATURE OXIDATION PROPERTIES OF IRON ALUMINIDES WITH Zr ADDITION
    Kejzlar, Pavel
    Hotar, Adam
    METAL 2014: 23RD INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS, 2014, : 1271 - 1276
  • [46] On the impact toughness of Fe-40Al-based B2 aluminides
    Pang, LX
    Kumar, KS
    INTERMETALLICS, 2000, 8 (02) : 157 - 163
  • [47] Portevin Le Chatelier instabilities and stoichiometric effects in B2 titanium aluminides
    Popille, F
    Kubin, LP
    Douin, J
    Naka, S
    SCRIPTA MATERIALIA, 1996, 34 (06) : 977 - 984
  • [48] Texture of high temperature deformed γ-α2 titanium aluminides
    Bermig, G.
    Tobisch, J.
    Scheffzuek, C.
    Oertel, C.
    Materials Science Forum, 1994, 157-6 (pt 1) : 309 - 314
  • [49] High temperature corrosion behavior of iron aluminides containing ternary additions in H2/H2S/H2O mixed gases
    Kai, W
    Chu, JP
    Huang, RT
    Lee, PY
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1997, 240 : 859 - 870
  • [50] Portevin-Le Chatelier instabilities and stoichiometric effects in B2 titanium aluminides
    CNRS-ONERA, Chatillon, France
    Scripta Mater, 6 (977-984):