High temperature corrosion of B2 iron aluminides

被引:37
|
作者
Mignone, A [1 ]
Frangini, S
La Barbera, A
Tassa, O
机构
[1] ENEA CR Casaccia, Mat Div, Rome, Italy
[2] CSM Mat & Components Dept, Rome, Italy
关键词
FeAl; mechanical alloying; oxidation; microstructure;
D O I
10.1016/S0010-938X(98)00014-6
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The high temperature oxidation of two B2-Fe40A1 Iron Aluminides has been studied in isothermal and cyclic conditions in the range 700 degrees C to 1100 degrees C and compared with a FeCrAlY alloy. One of the aluminides was prepared by mechanical alloying with the addition of an Y2O3-dispersion that conferred to it improved mechanical properties. No significative differences in the isothermal oxidation of the aluminides have been observed due to the presence of the Y2O3. Both aluminides presented higher oxidation rates than the FeCrAlY alloy at 758 degrees and 858 degrees C but lower rates at 1118 degrees C. The tests carried out under thermal cycling (100 1-hour cycles: 40 minutes at 900 degrees C plus 20 minutes at room temperature) showed that the FeCrAlY alloy presented a lower weight increase than both Iron aluminides. Scanning electron microscopy observations revealed a similar acicular morphology of the thin oxide layer formed on the aluminides. The oxide grown on the FeCrAlY alloy presented nodule formation. (C) 1998 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:1331 / 1347
页数:17
相关论文
共 50 条
  • [31] HIGH-TEMPERATURE STRENGTHENING OF B2 NIAL
    PATHARE, VM
    VEDULA, K
    MICHAL, GM
    JOURNAL OF METALS, 1985, 37 (11): : A87 - A87
  • [32] Solid solution strengthening in ternary B2 iron aluminides containing 3d transition elements
    Schneibel, JH
    Specht, ED
    Simpson, WA
    INTERMETALLICS, 1996, 4 (07) : 581 - 583
  • [33] High temperature load relaxation behavior of superplastic iron aluminides
    Song, JH
    Lim, HT
    Ha, TK
    Chang, YW
    SUPERPLASTICITY IN ADVANCED MATERIALS, ICSAM-2000, 2001, 357-3 : 231 - 236
  • [34] DEFORMATION-BEHAVIOR OF B2 TYPE ALUMINIDES - FEAL AND NIAL
    FU, CL
    YOO, MH
    ACTA METALLURGICA ET MATERIALIA, 1992, 40 (04): : 703 - 711
  • [35] Formation of amorphous alumina during sintering of nanocrystalline B2 aluminides
    Chawake, Niraj
    Koundinya, N. T. S. N.
    Kashyap, Sanjay
    Srivastav, Ajeet K.
    Yadav, Devinder
    Mondal, R. A.
    Kottada, Ravi Sankar
    MATERIALS CHARACTERIZATION, 2016, 119 : 186 - 194
  • [36] EFFECTS OF MO AND TI ADDITIONS ON THE DO3-]B2 TRANSITION-TEMPERATURE FOR IRON ALUMINIDES NEAR FE3AL
    FORTNUM, RT
    MIKKOLA, DE
    JOURNAL OF METALS, 1985, 37 (11): : A14 - A14
  • [37] Corrosion of carbon-alloyed iron aluminides
    Sen, M
    Balasubramaniam, R
    Kumar, AVR
    BULLETIN OF MATERIALS SCIENCE, 2000, 23 (05) : 399 - 403
  • [38] Microstructural development and creep deformation in equiaxed γ, γ + α2, and γ + α2 + B2 titanium aluminides
    Ott, Eric A.
    Pollock, Tresa M.
    Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science, 29 A (3 A): : 965 - 978
  • [39] Corrosion of carbon-alloyed iron aluminides
    M. Sen
    R. Balasubramaniam
    A. V. Ramesh Kumar
    Bulletin of Materials Science, 2000, 23 : 399 - 403
  • [40] Enhancement of high temperature strength and room temperature ductility of iron aluminides by alloying
    Bahadur, A
    MATERIALS SCIENCE AND TECHNOLOGY, 2003, 19 (12) : 1627 - 1634