Effect of Surface Treatment and Aging on Bond Strength of Composite Cement to Novel CAD/CAM Nanohybrid Composite

被引:8
|
作者
Elsaka, Shaymaa E. [1 ,2 ]
Elnaghy, Amr M. [3 ]
机构
[1] Mansoura Univ, Fac Dent, Dept Dent Biomat, Mansoura 35516, Egypt
[2] Alfarabi Private Coll Dent & Nursing, Dept Restorat Sci, Jeddah, Saudi Arabia
[3] Mansoura Univ, Fac Dent, Dept Endodont, Mansoura, Egypt
来源
JOURNAL OF ADHESIVE DENTISTRY | 2020年 / 22卷 / 02期
关键词
bond strength; composite cement; nanohybrid CAD/CAM; polymer-infiltrated ceramic; resin nanoceramic; surface roughness; surface treatments; FIXED DENTAL PROSTHESES; LOAD-BEARING CAPACITY; TITANIUM TETRAFLUORIDE; RESIN CEMENTS; FATIGUE RESISTANCE; UNIVERSAL ADHESIVE; CYCLIC FATIGUE; LUTING CEMENTS; ZIRCONIA; BLOCKS;
D O I
10.3290/j.jad.a44284
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose: To evaluate the effect of surface treatments and aging on the bond strength of composite cement to a novel CAD/CAM nanohybrid composite. Materials and Methods: Microtensile bond strength (pTBS) of a dual-curing composite cement (Bifix QM; BQ) to three CAD/CAM restorative materials (Grandio [GR], Vita Enamic EVE], and Lava Ultimate [LU]) was evaluated after different surface treatments. The surfaces of specimens received the following treatments: control (no treatment), sandblasting (SB), SB + silane (Ceramic Bond; CB), hydrofluoric acid (1-IF), HF + CB, TiF4 2 wt/v%, TiF4 2 wt/v% + CB, TiF4 4 wt/v%, and TiF4 4 wt/v% + CB. Half of the specimens in each group were aged. Surface topography and surface roughness were evaluated. Statistical analysis was conducted using ANOVA and Tukey's test. The Weibull analysis was conducted on mu TBS data of aged groups. Results: The mu TBS was significantly affected by the type of CAD/CAM material, type of treatment, and aging (p < 0.001). Silane application significantly improved the mu TBS (p < 0.05). The mu TBS decreased significantly with aging (5000 thermocycles) (p < 0.05). BQ cement resulted in the highest mu TBS to GR treated with TiF4 2% wt/v + CB compared to the other groups (p < 0.05). Aged GR/BQ treated with TiF4 2% wt/v + CB had the highest predicted mu TBS (19 MPa). Conclusion: TIF4 2% wt/v followed by silane application enhanced the adhesion of GR/BQ and LU/BQ systems. On the other hand, HF surface treatment followed by silane application improved the adhesion of the VE/BQ system.
引用
收藏
页码:195 / 204
页数:10
相关论文
共 50 条
  • [21] Effect of surface treatment of CAD/CAM resin composites on the shear bond strength of self-adhesive resin cement
    Nagasawa, Yuko
    Hibino, Yasushi
    Eda, Yoshikazu
    Nakajima, Hiroshi
    [J]. DENTAL MATERIALS JOURNAL, 2021, 40 (02) : 364 - 378
  • [22] Effect of Different Decontamination Agents on The Bond Strength of CAD/CAM Blocks and Repair Composite Materials
    Kopuz, Dilan
    Sancak, Elif Ilgi
    Tekce, Neslihan
    [J]. ODOVTOS INTERNATIONAL JOURNAL OF DENTAL SCIENCES, 2024, 26 (01) : 76 - 85
  • [23] Effect of Different Adhesive Strategies and Time on Microtensile Bond Strength of a CAD/CAM Composite to Dentin
    Meda, E. M.
    Rached, R. N.
    Ignacio, S. A.
    Fornazari, I. A.
    Souza, E. M.
    [J]. OPERATIVE DENTISTRY, 2019, 44 (03) : 262 - 272
  • [24] Effect of composite surface treatment and aging on the bond strength between a core build-up composite and a luting agent
    Cotes, Caroline
    Cardoso, Mayra
    de Melo, Renata Marques
    Valandro, Luiz Felipe
    Bottino, Marco Antonio
    [J]. JOURNAL OF APPLIED ORAL SCIENCE, 2015, 23 (01) : 71 - 78
  • [25] Influence of different surface treatments on bond strength of novel CAD/CAM restorative materials to resin cement
    Komurcuoglu, Meltem Bektas
    Sagirkaya, Elcin
    Tulga, Ayca
    [J]. JOURNAL OF ADVANCED PROSTHODONTICS, 2017, 9 (06): : 439 - 446
  • [26] Assessment the Bond Strength of Ceramic Brackets to CAD/CAM Nanoceramic Composite and Interpenetrating Network Composite after Different Surface Treatments
    Ozarslan, Mustafa Mehmet
    Ustun, Ozlem
    Buyukkaplan, Ulviye Sebnem
    Barutcigil, Cagatay
    Turker, Nurullah
    Barutcigil, Kubilay
    [J]. BIOMED RESEARCH INTERNATIONAL, 2018, 2018
  • [27] Effect of porcelain surface treatment on the porcelain to composite bond strength
    Olorunfemi, BO
    [J]. JOURNAL OF DENTAL RESEARCH, 1996, 75 (05) : 1284 - 1284
  • [28] The effect of surface treatment on the bond strength of resin composite to dentin
    Benderli, Y
    Yücel, T
    [J]. OPERATIVE DENTISTRY, 1999, 24 (02) : 96 - 102
  • [29] Effectiveness of surface treatment on bond strength of ceramic brackets to two types of CAD/CAM-prepared nanohybrid composites
    Elsaka, Shaymaa
    Hassan, Ali
    Elnaghy, Amr
    [J]. JOURNAL OF OROFACIAL ORTHOPEDICS-FORTSCHRITTE DER KIEFERORTHOPADIE, 2023, 84 (SUPPL 2): : 123 - 132
  • [30] Effect of surface treatments on shear bond strength of resin composite bonded to CAD/CAM resin-ceramic hybrid materials
    Gungor, Merve Bankoglu
    Nemli, Secil Karakoca
    Bal, Bilge Turhan
    Unver, Senem
    Dogan, Aylin
    [J]. JOURNAL OF ADVANCED PROSTHODONTICS, 2016, 8 (04): : 259 - 266