共 50 条
- [33] Wear-resistant PACVD coatings of the system Ti-B-N SURFACE & COATINGS TECHNOLOGY, 1999, 116 : 911 - 915
- [34] Phase transitions in PACVD-(Ti,Al)N coatings after annealing SURFACE & COATINGS TECHNOLOGY, 2000, 124 (2-3): : 190 - 195
- [36] Examination of mechanical properties and failure mechanisms of TiN and Ti-TiN multilayer coatings SURFACE & COATINGS TECHNOLOGY, 1995, 76 (1-3): : 297 - 302
- [38] Microstructure and microhardness of Ti(C, N) and TiN/Ti(C, N) multilayer films Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2010, 31 (02): : 113 - 118
- [39] Increasing the Wear Resistance of High-alloy Tool Steels for Cold Work with Multilayer Coatings TiN/TiCN and TiN/Ti-B-N Applied by the PACVD Process BHM Berg- und Huttenmannische Monatshefte, 2023, 168 (03): : 120 - 129
- [40] STUDY OF THE RELATIVE WEAR AND ABRASION RESISTANCE OF TI(C,N) AND TIN COATINGS SURFACE & COATINGS TECHNOLOGY, 1992, 55 (1-3): : 466 - 469