Coarsening-Resistance of a Severely Deformed Al-0.2 Wt% Sc Alloy

被引:0
|
作者
Huang, Yan [1 ]
机构
[1] Brunel Univ London, BCAST, Kingston Lane, Uxbridge UB8 3PH, Middx, England
来源
基金
英国工程与自然科学研究理事会;
关键词
Al-Sc alloy; Precipitates; Severe plastic deformation; Coarsening; ALUMINUM-ALLOYS; DEFORMATION;
D O I
10.1007/978-3-030-36408-3_39
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Second-phase Al3Sc particles play an important role in several aspects of material performance. These include increasing strength, stabilizing microstructure and increasing recrystallization temperature and thermal stability. The present work was conducted to investigate the stability of Al3Sc particles in a severely deformed Al-0.25 wt% Sc alloy at room temperature in comparison to that of Al2Cu precipitates in an Al-Cu alloy. Microstructural examination and hardness tests showed that the Al3Sc particles were coarsening resistant with substantially higher stability than Al2Cu and the hardness of the Al-0.25Sc alloy remained almost constant while an apparent hardness drop was observed for the Al-Cu alloy.
引用
收藏
页码:272 / 276
页数:5
相关论文
共 50 条
  • [41] Microstructure, mechanical property and thermo-stability of traditionally and severely deformed Al-Mg-Sc-Zr alloy
    Jiang, Jingyu
    Chen, Hongwu
    Cao, Xiaohang
    Jiang, Feng
    Zhang, Menghan
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2022, 18 : 4130 - 4144
  • [42] PRECIPITATION AND COARSENING KINETICS AND EFFECT OF MECHANICAL PROPERTY OF Al3Sc IN Al-Sc ALLOY
    Wen, Qian
    Ye, Feng
    Huang, Meiting
    Wang, Ji
    Lin, Junpin
    ALUMINUM ALLOYS: FABRICATION, CHARACTERIZATION AND APPLICATIONS II, 2009, : 141 - 146
  • [43] An investigation on the microstructure, texture and mechanical properties of an optimized friction stir-welded ultrafine-grained Al–0.2 wt% Sc alloy deformed by accumulative roll bonding
    Mohammad Yousefieh
    Morteza Tamizifar
    Seyed Mohammad Ali Boutorabi
    Ehsan Borhani
    Journal of Materials Science, 2018, 53 : 4623 - 4634
  • [44] Recovery of deformation substructure and coarsening of particles on annealing severely plastically deformed Al-Mg-Si alloy and analysis of strengthening mechanisms
    Gutierrez-Urrutia I.
    Muñoz-Morris M.A.
    Morris D.G.
    Journal of Materials Research, 2006, 21 (02) : 329 - 342
  • [45] Microstructural evolution and creep of an Al-0.2wt.%Sc alloy after equal-channel angular pressing
    Kral, P.
    Dvorak, J.
    Sklenicka, V.
    NANOMATERIALS BY SEVERE PLASTIC DEFORMATION IV, PTS 1 AND 2, 2008, 584-586 : 846 - 851
  • [46] Mechanical properties of Al-5.7wt% Ni eutectic alloy severely deformed by equal-channel angular pressing
    Watanabe, Yoshimi
    Zhang, Zuogui
    Sato, Hisashi
    Inamura, Tomonari
    Hosoda, Hideki
    THERMEC 2006, PTS 1-5, 2007, 539-543 : 2916 - +
  • [47] Cast near-eutectic Al-12.5 wt.% Ce alloy with high coarsening and creep resistance
    Liu, Yang
    Michi, Richard A.
    Dunand, David C.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 767
  • [48] Coarsening kinetics of Al3Sc precipitates in an al-mg-sc alloy aged at 573 K
    Watanabe, Daizen
    Watanabe, Chihiro
    Monzen, Ryoichi
    MATERIALS TRANSACTIONS, 2007, 48 (06) : 1571 - 1574
  • [49] Statistical aspects of grain coarsening in a fine grained Al-Sc alloy
    Ferry, M.
    Burhan, N.
    RECRYSTALLIZATION AND GRAIN GROWTH III, PTS 1 AND 2, 2007, 558-559 : 729 - +
  • [50] Study on thermal stability of 2519(Sc) Al alloy and establishment of coarsening model
    Qin, Jin
    Yan, Zhijie
    Wei, Qirong
    Wang, Bin
    VACUUM, 2023, 218