Coarsening-Resistance of a Severely Deformed Al-0.2 Wt% Sc Alloy

被引:0
|
作者
Huang, Yan [1 ]
机构
[1] Brunel Univ London, BCAST, Kingston Lane, Uxbridge UB8 3PH, Middx, England
来源
基金
英国工程与自然科学研究理事会;
关键词
Al-Sc alloy; Precipitates; Severe plastic deformation; Coarsening; ALUMINUM-ALLOYS; DEFORMATION;
D O I
10.1007/978-3-030-36408-3_39
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Second-phase Al3Sc particles play an important role in several aspects of material performance. These include increasing strength, stabilizing microstructure and increasing recrystallization temperature and thermal stability. The present work was conducted to investigate the stability of Al3Sc particles in a severely deformed Al-0.25 wt% Sc alloy at room temperature in comparison to that of Al2Cu precipitates in an Al-Cu alloy. Microstructural examination and hardness tests showed that the Al3Sc particles were coarsening resistant with substantially higher stability than Al2Cu and the hardness of the Al-0.25Sc alloy remained almost constant while an apparent hardness drop was observed for the Al-Cu alloy.
引用
收藏
页码:272 / 276
页数:5
相关论文
共 50 条
  • [21] The combined effect of aging and accumulative roll bonding on the evolution of the microstructure and mechanical characteristics of an Al-0.2 wt % Zr alloy
    Azad, B.
    Semnani, H. M.
    Borhani, E.
    PHYSICS OF METALS AND METALLOGRAPHY, 2017, 118 (01): : 87 - 95
  • [22] Numerical investigation of friction stir welding parameters on microstructure, thermal and mechanical properties of ultrafine-grained Al-0.2 wt% Sc alloy sheet摩擦搅拌焊参数对超细晶Al-0.2 wt% Sc 合金薄板微观组织和热力学性能的影响
    Valeh Talebsafa
    Mohammad Yousefieh
    Ehsan Borhani
    Ehsan Gharibshahiyan
    Journal of Central South University, 2023, 30 : 61 - 73
  • [23] Coarsening of Al3Sc particles in an Al-Mg-Sc alloy
    Watanabe, Chihiro
    Watanabe, Daizen
    Monzen, Rvoichi
    Tasaki, Kazue
    Solid-Solid Phase Transformations in Inorganic Materials 2005, Vol 1, 2005, : 803 - 808
  • [24] Influence of microstructure on electrochemical properties of severely deformed Al-5 wt% Cu alloy by ECAP
    Zhang, Zuogui
    Akiyama, Eiji
    Watanabe, Yoshimi
    Katada, Yasuyuki
    Tsuzaki, Kaneaki
    ALUMINIUM ALLOYS 2006, PTS 1 AND 2: RESEARCH THROUGH INNOVATION AND TECHNOLOGY, 2006, 519-521 : 705 - 710
  • [25] High-strain-rate superplastic behavior of equal-channel angular-pressed 5083 Al-0.2 Wt Pct Sc
    Shin, DH
    Hwang, DY
    Oh, YJ
    Park, KT
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2004, 35A (03): : 825 - 837
  • [26] High-strain-rate superplastic behavior of equal-channel angular-pressed 5083 Al-0.2 wt pct Sc
    Dong Hyuk Shin
    Duck-Young Hwang
    Yong-Jun Oh
    Kyung-Tae Park
    Metallurgical and Materials Transactions A, 2004, 35 : 825 - 837
  • [27] Microstructure and aging behavior of Al-0.2wt%Zr alloy heavily deformed by ARB process
    Sato, Takatoshi
    Terada, Daisuke
    Tsuji, Nobuhiro
    NANOMATERIALS BY SEVERE PLASTIC DEFORMATION IV, PTS 1 AND 2, 2008, 584-586 : 728 - 733
  • [28] Coarsening of cuboidal Al3Sc precipitates in an Al-Mg-Sc alloy
    Watanabe, Chihiro
    Watanabe, Daizen
    Tanii, Ryo
    Monzen, Ryoichi
    PHILOSOPHICAL MAGAZINE LETTERS, 2010, 90 (02) : 103 - 111
  • [29] Coarsening behavior of Al3Sc precipitates in an Al-Mg-Sc alloy
    Watanabe, Chihiro
    Watanabe, Daizen
    Monzen, Ryoichi
    MATERIALS TRANSACTIONS, 2006, 47 (09) : 2285 - 2291
  • [30] Time and temperature regime of continuous grain coarsening in an ECAP-processed Al(0.1 wt.% Sc) alloy
    Bommareddy, A.
    Quadir, M. Z.
    Ferry, M.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2012, 527 : 145 - 151