Fracture toughness and the master curve for modified 9Cr-1Mo steel

被引:7
|
作者
Yoon, Ji-Hyun
Yoon, Eui-Pak
机构
[1] Hanyang Univ, Dept Mat Engn, Seoul 133791, South Korea
[2] Korea Atom Energy Res Inst, Taejon 305353, South Korea
关键词
modified; 9Cr-1Mo; master curve; SA508-Gr.3; reactor pressure vessel; fracture toughness; reference temperature; VHTR;
D O I
10.1007/BF03027747
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Modified 9Cr-1Mo steel is a primary candidate material for the reactor pressure vessel of a Very High Temperature Gas-Cooled Reactor (VHTR) in the Korean Nuclear Hydrogen Development and Demonstration (NHDD) program. In this study, the T-0 reference temperature, J-R fracture resistance and Charpy impact properties were evaluated for commercial Grade 91 steel as part of the preliminary testing for a selection of the RPV material for the VHTR. The fracture toughness of the modified 9Cr-1Mo steel was compared with that of SA508-Gr.3. The objective of this study was to obtain the pre-irradiation fracture toughness properties of the modified 9Cr-1Mo steel as reference data for an investigation of radiation effects. Charpy impact properties of the modified 9Cr-1Mo steel were similartothose of SA508-Gr.3. To reference temperatures were measured as -67.7 and -72.4 degrees C from the tests with standard PCVN (pre-cracked Charpy V-notch) and half-sized PCVN specimens respectively, which were similar to the results for SA508-Gr.3. The K-Jc values of the modified 9Cr-1Mo steel with the test temperatures are successfully expressed by the Master Curve. The J-R fracture resistance of the modified 9Cr-1Mo steel at room temperature was nearly identical to that of SA508-Gr.3; in contrast, it was slightly higher at an elevated temperature.
引用
收藏
页码:477 / 482
页数:6
相关论文
共 50 条
  • [31] Mechanical properties of modified 9Cr-1Mo steel welds with notches
    Lee, WH
    Shiue, RK
    Chen, C
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 356 (1-2): : 153 - 161
  • [32] Delta ferrite in modified 9Cr-1Mo steel weld metal
    Mahlalela, Sibusiso
    Pistorius, Pieter
    WELDING IN THE WORLD, 2025,
  • [33] Characterization of Crack Arrest Phenomena in a Modified 9Cr-1Mo Steel
    Sathyanarayanan, S.
    Moitra, A.
    Sasikala, G.
    Dasgupta, A.
    Saroja, S.
    Bhaduri, A. K.
    Raj, Baldev
    Singh, Vakil
    JOURNAL OF TESTING AND EVALUATION, 2011, 39 (03) : 448 - 455
  • [34] Modification of microstructure and the alligatoring damage in a modified 9Cr-1Mo steel
    Kishore, R
    Sinha, TK
    JOURNAL OF NUCLEAR MATERIALS, 1999, 273 (03) : 334 - 337
  • [35] Flow Behaviour of Modified 9Cr-1Mo Steel at Elevated Temperatures
    Shiva, V.
    Goyal, Sunil
    Sandhya, R.
    Laha, K.
    Bhaduri, A. K.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2017, 70 (03) : 589 - 596
  • [36] DEVELOPMENT OF NEW 9CR-1MO TYPE STEEL .3. WELDABILITY OF 9CR-1MO TYPE STEEL
    SAKURAI, H
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1987, 73 (05): : S503 - S503
  • [37] Evaluation of creep-fatigue life based on fracture energy for modified 9Cr-1Mo steel
    Nagae, Yuji
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 560 : 752 - 758
  • [38] A Study on Factors Influencing Toughness of Basic Flux-Cored Weld of Modified 9Cr-1Mo Steel
    B. Arivazhagan
    M. Kamaraj
    Journal of Materials Engineering and Performance, 2011, 20 : 1188 - 1195
  • [39] A Study on Factors Influencing Toughness of Basic Flux-Cored Weld of Modified 9Cr-1Mo Steel
    Arivazhagan, B.
    Kamaraj, M.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2011, 20 (07) : 1188 - 1195
  • [40] Creep deformation and fracture behaviour of modified 9Cr-1Mo steel in flowing liquid sodium environment
    Ravi, S.
    Vanaja, J.
    Vijayanand, V. D.
    Rajasundaram, P.
    Vijayaraghavan, S.
    Shanthugavel, M.
    Babu, B.
    Laha, K.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 702 : 232 - 240