High-temperature corrosion of aluminium nitride ceramics by coal ashes

被引:7
|
作者
Himpel, Gert [1 ]
Herrmann, Mathias [1 ]
Hoehn, Soeren [1 ]
Klinger, Mathias [2 ]
机构
[1] Fraunhofer Inst Keram Technologien & Syst IKSTS, D-01277 Dresden, Germany
[2] Tech Univ Bergakad Freiberg, Inst Energy Proc Engn & Chem Engn, D-09596 Freiberg, Germany
关键词
Corrosion; Aluminium nitride; Gasification reactor; REFRACTORIES; GASIFICATION;
D O I
10.1016/j.jeurceramsoc.2013.08.030
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
New high-efficiency gasification reactors with higher temperatures and pressures and with changed temperature cycles require new types of refractory linings. Besides the oxide materials currently in use, nonoxide materials such as SiC and AIN ceramics show great promise as refractories in the reducing atmospheres found in gasifiers. One of the main corrosion mechanisms occurring involves the interaction between the lining and the slag. Hence, AIN materials (without additives and with MgO or CaO additives) were tested in basic and acidic coal ashes at temperatures of 900-1300 degrees C in a tube furnace with an atmosphere containing H-2, CO and H2O. After dwell times of up to 200 h the cross sections of the materials were analysed by SEM and EDS. The results showed the high stability of the materials in acidic ashes, but interaction with alkaline and calcium oxides along the grain boundaries in basic ashes. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:267 / 276
页数:10
相关论文
共 50 条
  • [31] HIGH-TEMPERATURE CERAMICS
    TYMCZAK, RW
    MCMURTY, CH
    SANDMEYE.KH
    INDUSTRIAL RESEARCH, 1971, 13 (13): : 53 - &
  • [32] HIGH-TEMPERATURE CORROSION AND PROTECTIVE LAYERS AGAINST HIGH-TEMPERATURE CORROSION
    SAHM, PR
    METALL, 1976, 30 (04): : 326 - 331
  • [33] HIGH-TEMPERATURE CORROSION OF REACTION-SINTERED SILICON-NITRIDE
    NASSIF, N
    HANNA, SB
    THERMOCHIMICA ACTA, 1984, 79 (SEP) : 305 - 314
  • [34] High-temperature oxidation behavior of high-purity α-, β-, and mixed silicon nitride ceramics
    Backhaus-Ricoult, M
    Guerin, V
    Huntz, AM
    Urbanovich, VS
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2002, 85 (02) : 385 - 392
  • [35] High-temperature metal corrosion during the combustion of coal with high salt content
    Shendrik, T. G.
    Dunayevska, N. I.
    Fateiev, A. I.
    MATERIALS SCIENCE, 2025, : 124 - 133
  • [36] High temperature behaviours of aluminium nitride
    Dagdag, S.
    Lebey, T.
    Dinculescu, S.
    Saiz, J.
    Dutarde, E.
    2007 EUROPEAN CONFERENCE ON POWER ELECTRONICS AND APPLICATIONS, VOLS 1-10, 2007, : 537 - +
  • [37] HIGH-TEMPERATURE THERMAL AND ENVIRONMENTAL STABILITIES OF BORON-NITRIDE, ALUMINUM NITRIDE AND SILICON-NITRIDE CERAMICS
    SINGH, M
    WIEDEMEIER, H
    MATERIALS AT HIGH TEMPERATURES, 1991, 9 (03) : 139 - 144
  • [38] High-temperature corrosion
    Mater Perform, 2008, 4 (80):
  • [39] High-temperature corrosion
    不详
    MATERIALS PERFORMANCE, 2008, 47 (04) : 80 - 80
  • [40] High-temperature corrosion
    Stringer, J
    MATERIALS PERFORMANCE, 2003, 42 (11) : 8 - 8