High-temperature corrosion of aluminium nitride ceramics by coal ashes

被引:7
|
作者
Himpel, Gert [1 ]
Herrmann, Mathias [1 ]
Hoehn, Soeren [1 ]
Klinger, Mathias [2 ]
机构
[1] Fraunhofer Inst Keram Technologien & Syst IKSTS, D-01277 Dresden, Germany
[2] Tech Univ Bergakad Freiberg, Inst Energy Proc Engn & Chem Engn, D-09596 Freiberg, Germany
关键词
Corrosion; Aluminium nitride; Gasification reactor; REFRACTORIES; GASIFICATION;
D O I
10.1016/j.jeurceramsoc.2013.08.030
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
New high-efficiency gasification reactors with higher temperatures and pressures and with changed temperature cycles require new types of refractory linings. Besides the oxide materials currently in use, nonoxide materials such as SiC and AIN ceramics show great promise as refractories in the reducing atmospheres found in gasifiers. One of the main corrosion mechanisms occurring involves the interaction between the lining and the slag. Hence, AIN materials (without additives and with MgO or CaO additives) were tested in basic and acidic coal ashes at temperatures of 900-1300 degrees C in a tube furnace with an atmosphere containing H-2, CO and H2O. After dwell times of up to 200 h the cross sections of the materials were analysed by SEM and EDS. The results showed the high stability of the materials in acidic ashes, but interaction with alkaline and calcium oxides along the grain boundaries in basic ashes. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:267 / 276
页数:10
相关论文
共 50 条
  • [21] HIGH-TEMPERATURE CORROSION IN COAL-GASIFICATION SYSTEMS
    NATESAN, K
    CORROSION, 1985, 41 (11) : 646 - 655
  • [22] High-temperature tribotechnical characteristics of ceramics based on aluminum nitride
    Tkachenko, YG
    Yurchenko, DZ
    Satanin, SV
    Shevchenko, OA
    Murzin, LM
    POWDER METALLURGY AND METAL CERAMICS, 1998, 37 (3-4) : 165 - 169
  • [23] High-temperature tribotechnical characteristics of ceramics based on aluminum nitride
    Y. G. Tkachenko
    D. Z. Yurchenko
    S. V. Satanin
    O. A. Shevchenko
    L. M. Murzin
    Powder Metallurgy and Metal Ceramics, 1998, 37 : 165 - 169
  • [24] High-Temperature Corrosion of Ni-Base Alloys by Waste Incineration Ashes
    Solecka, M.
    Kusinski, J.
    Kopia, A.
    Rozmus-Gornikowska, M.
    Radziszewska, A.
    ACTA PHYSICA POLONICA A, 2016, 130 (04) : 1045 - 1048
  • [25] Influence of aluminium nitride on the high-temperature ductility of continuous cast slabs
    Winkelhofer, Florian
    Parteder, Erik
    Clemens, Helmut
    Leitner, Harald
    Spiradek-Hahn, Krystyna
    Kozeschnik, Ernst
    PRAKTISCHE METALLOGRAPHIE-PRACTICAL METALLOGRAPHY, 2008, 45 (04): : 159 - 172
  • [26] HIGH-TEMPERATURE CORROSION AND DEGRADATION IN STRENGTH OF SILICON-NITRIDE BASED CERAMICS BY ALKALI SULFATES AND CARBONATE MELTS
    SHIMADA, M
    SATO, T
    ENDO, T
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1987, 134 (8B) : C467 - C467
  • [27] HIGH-TEMPERATURE CORROSION OF TZM IN SIMULATED COAL GASIFIER ENVIRONMENTS
    TIEARNEY, TC
    NATESAN, K
    JOURNAL OF METALS, 1980, 32 (12): : 39 - 40
  • [28] HIGH-TEMPERATURE CORROSION OF ALLOYS IN COAL-GASIFICATION ATMOSPHERE
    OKADA, M
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 72 (13): : 1484 - 1484
  • [29] DEVELOPMENT OF A COAL ASH CORROSIVITY INDEX FOR HIGH-TEMPERATURE CORROSION
    SHIGETA, J
    HAMAO, Y
    AOKI, H
    KAJIGAYA, I
    JOURNAL OF ENGINEERING MATERIALS AND TECHNOLOGY-TRANSACTIONS OF THE ASME, 1987, 109 (04): : 299 - 305
  • [30] HIGH-TEMPERATURE CORROSION PROBLEMS IN COAL-GASIFICATION SYSTEMS
    HILL, VL
    JOURNAL OF METALS, 1984, 36 (07): : 8 - 8