High-temperature corrosion of aluminium nitride ceramics by coal ashes

被引:7
|
作者
Himpel, Gert [1 ]
Herrmann, Mathias [1 ]
Hoehn, Soeren [1 ]
Klinger, Mathias [2 ]
机构
[1] Fraunhofer Inst Keram Technologien & Syst IKSTS, D-01277 Dresden, Germany
[2] Tech Univ Bergakad Freiberg, Inst Energy Proc Engn & Chem Engn, D-09596 Freiberg, Germany
关键词
Corrosion; Aluminium nitride; Gasification reactor; REFRACTORIES; GASIFICATION;
D O I
10.1016/j.jeurceramsoc.2013.08.030
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
New high-efficiency gasification reactors with higher temperatures and pressures and with changed temperature cycles require new types of refractory linings. Besides the oxide materials currently in use, nonoxide materials such as SiC and AIN ceramics show great promise as refractories in the reducing atmospheres found in gasifiers. One of the main corrosion mechanisms occurring involves the interaction between the lining and the slag. Hence, AIN materials (without additives and with MgO or CaO additives) were tested in basic and acidic coal ashes at temperatures of 900-1300 degrees C in a tube furnace with an atmosphere containing H-2, CO and H2O. After dwell times of up to 200 h the cross sections of the materials were analysed by SEM and EDS. The results showed the high stability of the materials in acidic ashes, but interaction with alkaline and calcium oxides along the grain boundaries in basic ashes. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:267 / 276
页数:10
相关论文
共 50 条
  • [1] Comparison of the high-temperature corrosion of aluminium nitride, alumina, magnesia and zirconia ceramics by coal ashes
    Himpel, Gert
    Herrmann, Mathias
    Hoehn, Soeren
    CERAMICS INTERNATIONAL, 2015, 41 (07) : 8288 - 8298
  • [2] High-temperature corrosion of silicon carbide ceramics by coal ashes
    Herrmann, M.
    Standke, G.
    Hoehn, S.
    Himpel, G.
    Gestrich, T.
    CERAMICS INTERNATIONAL, 2014, 40 (01) : 1471 - 1479
  • [3] Cavitation induced by high-temperature plastic deformation in aluminium nitride ceramics
    Choux, S
    Masson, I
    Feiereisen, JP
    George, A
    Michel, JP
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1996, 16 (05) : 515 - 519
  • [4] CORROSION OF CERAMICS AND METALS AT HIGH-TEMPERATURE
    ELLIOTT, JF
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 1976, : 36 - 36
  • [5] Corrosion Resistance of Ceramics and High-temperature Phase Change of Powders on Cubic Silicon Nitride
    Yao Huai
    Zhu Guanglin
    Du Meng
    PHYSICAL AND NUMERICAL SIMULATION OF MATERIAL PROCESSING VI, PTS 1 AND 2, 2012, 704-705 : 853 - 857
  • [6] HIGH-TEMPERATURE ELECTRICAL CONDUCTIVITY OF ALUMINIUM NITRIDE.
    Richards, V.L.
    Tien, T.Y.
    Pehlke, R.D.
    1600, (22):
  • [7] HIGH-TEMPERATURE OXIDATION AND CORROSION OF ENGINEERING CERAMICS
    NICKEL, KG
    FU, Z
    QUIRMBACH, P
    JOURNAL OF ENGINEERING FOR GAS TURBINES AND POWER-TRANSACTIONS OF THE ASME, 1993, 115 (01): : 76 - 82
  • [8] High-temperature oxidation and corrosion of engineering ceramics
    Nickel, K.G.
    Fu, Z.
    Quirmbach, P.
    Journal of Engineering for Gas Turbines and Power, 1993, 115 (01) : 76 - 82
  • [9] HIGH-TEMPERATURE CORROSION IN COAL COMBUSTION SYSTEMS
    STRINGER, J
    JOURNAL OF METALS, 1984, 36 (07): : 8 - 8
  • [10] Joining of silicon nitride ceramics for high-temperature applications
    Xie, RJ
    Mitomo, M
    Huang, LP
    Fu, XR
    JOURNAL OF MATERIALS RESEARCH, 2000, 15 (01) : 136 - 141