Relationship between textures and deformation modes in Mg-3Al-1Zn alloy during uniaxial tension

被引:25
|
作者
Wang, Bingshu [1 ]
Deng, Liping [1 ]
Adrien, Chapuis [2 ]
Guo, Ning [2 ]
Xu, Zeren [3 ]
Li, Qiang [1 ]
机构
[1] Fuzhou Univ, Coll Mat Sci & Engn, Fuzhou 350108, Fujian, Peoples R China
[2] Chongqing Univ, Coll Mat Sci & Engn, Chongqing 400044, Peoples R China
[3] Clemson Univ, Dept Automot Engn, Greenville, SC 29607 USA
关键词
Magnesium alloy; EBSD; Twinning; Crystal plasticity; AZ31 MAGNESIUM ALLOY; PLANE-STRAIN COMPRESSION; MECHANICAL-BEHAVIOR; ROOM-TEMPERATURE; MG ALLOY; NEUTRON-DIFFRACTION; SLIP; EVOLUTION; STRESS; SHEET;
D O I
10.1016/j.matchar.2015.08.014
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effects of initial texture on the flow behavior, microstructure and texture evolution of Mg-3Al-1Zn alloy hot rolled plate with a strong basal texture during tension at room temperature have been investigated by experiments and simulations. Three kinds of specimens were cut from this plate with their tensile directions aligned 0 degrees,45 degrees, and 90 degrees to the normal direction (ND), and they were referred as 0ND, 45ND and 90ND specimens, respectively. A crystal plasticity model was developed to demonstrate the relationship between textures and deformation modes. The results show that the general features of flow curves and texture evolutions of AZ31 alloy during tension can be well explained by the relative activities of deformation modes, which exhibit a pronounced orientation dependence on both the starting and current textures. The obvious yielding behaviors in 0ND and 45ND specimens are induced by the initial activity of {10-12} twinning, and the strain hardening behavior is related to the activities of {10-12} twinning, basal slip and prismatic slip. Due to the existence of {10-11} twinning at low strain, the elongation to rupture of 90ND specimen is much lower than those the elongation of 0ND and 45ND specimens. Although prismatic slip activity depends on the initial texture, its activities always increases during tension, affecting the flow curves, microstructure and texture evolutions. The high prismatic slip activities in 0ND and 90ND specimens result in a strong {10-10} prismatic texture, while the activity of pyramidal <c + a> slip is always negligible in all specimens and insensitive to the initial texture during tension. (C) 2015 Elsevier Inc. All rights reserved.
引用
收藏
页码:42 / 50
页数:9
相关论文
共 50 条
  • [41] Flow softening behavior during dynamic recrystallization in Mg-3Al-1Zn magnesium alloy
    Bhattacharya, R.
    Wynne, B. P.
    Rainforth, W. M.
    SCRIPTA MATERIALIA, 2012, 67 (03) : 277 - 280
  • [42] Characteristics of the contraction twins formed close to the fracture surface in Mg-3Al-1Zn alloy deformed in tension
    Cizek, P.
    Barnett, M. R.
    SCRIPTA MATERIALIA, 2008, 59 (09) : 959 - 962
  • [43] Deformation behavior of gravity cast Mg-3Al-1Zn alloy during hot compression test: A study with processing maps
    Robin, Lalu G.
    Ganesan, G.
    Raghukandan, K.
    Pillai, U.T.S.
    Pai, B.C.
    Materials Forum, 2005, 29 : 161 - 165
  • [44] The effect of twin-twin interaction in Mg-3Al-1Zn alloy during compression
    Shi, Dongfeng
    Liu, Tianmo
    Hou, Dewen
    Chen, Huicong
    Pan, Fusheng
    Chen, Hongbing
    JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 685 : 428 - 435
  • [45] The effect of twin-twin interaction in Mg-3Al-1Zn alloy during compression
    Liu, Tianmo (tmliu@cqu.edu.cn), 1600, Elsevier Ltd (685):
  • [46] Influence of grain size on the compressive deformation of wrought Mg-3Al-1Zn
    Barnett, MR
    Keshavarz, Z
    Beer, AG
    Atwell, D
    ACTA MATERIALIA, 2004, 52 (17) : 5093 - 5103
  • [47] Effect of grain size on the deformation and dynamic recrystallization of Mg-3Al-1Zn
    Barnett, MR
    Atwell, D
    Beer, AG
    RECRYSTALLIZATION AND GRAIN GROWTH, PTS 1 AND 2, 2004, 467-470 : 435 - 440
  • [48] Effect of grain size on mechanical property of Mg-3Al-1Zn alloy
    Wang, Jing Tao
    Yin, De Liang
    Liu, Jin Qiang
    Tao, Jun
    Su, Yan Ling
    Zhao, Xiang
    SCRIPTA MATERIALIA, 2008, 59 (01) : 63 - 66
  • [49] Microstructural development during hot working of Mg-3Al-1Zn
    Beer, A. G.
    Barnett, M. R.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2007, 38A (08): : 1856 - 1867
  • [50] Effect of grain size on prismatic slip in Mg-3Al-1Zn alloy
    Razavi, S. M.
    Foley, D. C.
    Karaman, I.
    Hartwig, K. T.
    Duygulu, O.
    Kecskes, L. J.
    Mathaudhu, S. N.
    Hammond, V. H.
    SCRIPTA MATERIALIA, 2012, 67 (05) : 439 - 442