Relationship between textures and deformation modes in Mg-3Al-1Zn alloy during uniaxial tension

被引:25
|
作者
Wang, Bingshu [1 ]
Deng, Liping [1 ]
Adrien, Chapuis [2 ]
Guo, Ning [2 ]
Xu, Zeren [3 ]
Li, Qiang [1 ]
机构
[1] Fuzhou Univ, Coll Mat Sci & Engn, Fuzhou 350108, Fujian, Peoples R China
[2] Chongqing Univ, Coll Mat Sci & Engn, Chongqing 400044, Peoples R China
[3] Clemson Univ, Dept Automot Engn, Greenville, SC 29607 USA
关键词
Magnesium alloy; EBSD; Twinning; Crystal plasticity; AZ31 MAGNESIUM ALLOY; PLANE-STRAIN COMPRESSION; MECHANICAL-BEHAVIOR; ROOM-TEMPERATURE; MG ALLOY; NEUTRON-DIFFRACTION; SLIP; EVOLUTION; STRESS; SHEET;
D O I
10.1016/j.matchar.2015.08.014
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effects of initial texture on the flow behavior, microstructure and texture evolution of Mg-3Al-1Zn alloy hot rolled plate with a strong basal texture during tension at room temperature have been investigated by experiments and simulations. Three kinds of specimens were cut from this plate with their tensile directions aligned 0 degrees,45 degrees, and 90 degrees to the normal direction (ND), and they were referred as 0ND, 45ND and 90ND specimens, respectively. A crystal plasticity model was developed to demonstrate the relationship between textures and deformation modes. The results show that the general features of flow curves and texture evolutions of AZ31 alloy during tension can be well explained by the relative activities of deformation modes, which exhibit a pronounced orientation dependence on both the starting and current textures. The obvious yielding behaviors in 0ND and 45ND specimens are induced by the initial activity of {10-12} twinning, and the strain hardening behavior is related to the activities of {10-12} twinning, basal slip and prismatic slip. Due to the existence of {10-11} twinning at low strain, the elongation to rupture of 90ND specimen is much lower than those the elongation of 0ND and 45ND specimens. Although prismatic slip activity depends on the initial texture, its activities always increases during tension, affecting the flow curves, microstructure and texture evolutions. The high prismatic slip activities in 0ND and 90ND specimens result in a strong {10-10} prismatic texture, while the activity of pyramidal <c + a> slip is always negligible in all specimens and insensitive to the initial texture during tension. (C) 2015 Elsevier Inc. All rights reserved.
引用
收藏
页码:42 / 50
页数:9
相关论文
共 50 条
  • [31] Anisotropy of creep behaviour in extruded Mg-3Al-1Zn alloy
    Shabani-Mahalli, M.
    Mahmudi, R.
    Karami, M.
    MATERIALS SCIENCE AND TECHNOLOGY, 2015, 31 (02) : 225 - 230
  • [32] Effect of crystallographic texture on the kinetics of hot deformation of rolled Mg-3Al-1Zn alloy plate
    Prasad, Y. V. R. K.
    Rao, K. P.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 432 (1-2): : 170 - 177
  • [33] Effects of Deformation Texture and Grain Size on Corrosion Behavior of Mg-3Al-1Zn Alloy Sheets
    Li, Da-Wei
    Wang, Hui-Yuan
    Wei, Dong-Song
    Zhao, Zheng-Xue
    Liu, Yan
    ACS OMEGA, 2020, 5 (03): : 1448 - 1456
  • [34] Pyramidal slips in high cycle fatigue deformation of a rolled Mg-3Al-1Zn magnesium alloy
    Tan, Li
    Zhang, Xiyan
    Sun, Qi
    Yu, Jiangping
    Huang, Guangjie
    Liu, Qing
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 699 : 247 - 253
  • [35] Detwinning behavior of Mg-3Al-1Zn alloy at elevated temperatures
    Yu, Huihui
    Xin, Yunchang
    Zhou, Hua
    Hong, Rui
    Zhao, Lingyu
    Liu, Qing
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 617 : 24 - 30
  • [36] Enhancement of plasticity in Mg-3Al-1Zn alloy at cryogenic temperature
    Zhang, Kai
    Jiang, Jun
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 25 : 7454 - 7459
  • [37] Anisotropic fatigue behavior of rolled Mg-3Al-1Zn alloy
    Hong, Seong-Gu
    Park, Sung Hyuk
    Huh, Yong-Hak
    Lee, Chong Soo
    JOURNAL OF MATERIALS RESEARCH, 2010, 25 (05) : 966 - 971
  • [38] Interplay between the effects of deformation mechanisms and dynamic recrystallization on the failure of Mg-3Al-1Zn
    Vaughan, M. W.
    Nasim, W.
    Dogan, E.
    Herrington, J. S.
    Proust, G.
    Benzerga, A. A.
    Karaman, I.
    ACTA MATERIALIA, 2019, 168 : 448 - 472
  • [39] Microstructure and Texture Evolution During Annealing of Caliber Rolled Mg-3Al-1Zn Alloy
    Doiphode, R. L.
    Murty, S. V. S. Narayana
    Prabhu, N.
    Kashyap, B. P.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2015, 68 : S317 - S321
  • [40] Detwinning and twinning dynamics in pre-twinned Mg-3Al-1Zn alloy under uniaxial tension: a synchrotron-based multiscale study
    Deng, Y. J.
    Fang, X.
    Bian, Y. L.
    Li, S. Y.
    Li, K.
    Cai, Y.
    Lu, L.
    Luo, S. N.
    JOURNAL OF MATERIALS SCIENCE, 2025, 60 (13) : 6008 - 6021