Influence of Cr alloying on the oxidation resistance of Sn-8Zn-3Bi solders

被引:13
|
作者
Huang, Na [1 ]
Hu, Anmin [1 ]
Li, Ming [1 ]
Mao, Dali [1 ]
机构
[1] Shanghai Jiao Tong Univ, Sch Mat Sci & Engn, Key Lab Thin Film & Microfabricat Technol, State Key Lab Met Matrix Composites,Minist Educ, Shanghai 200240, Peoples R China
基金
中国国家自然科学基金;
关键词
LEAD-FREE SOLDER; SN-ZN SOLDERS; INTERFACIAL REACTIONS; TEMPERATURE; CU; SYSTEM; RELIABILITY; BEHAVIOR; ELEMENTS; JOINTS;
D O I
10.1007/s10854-013-1175-5
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Influence of Cr alloying on the oxidation behavior of Sn-8Zn-3Bi-xCr (SZBxCr) (x = 0, 0.1, 0.3, 0.5) solders under 250 A degrees C has been investigated. It was found that the poor oxidation resistance of the solders is attributed to the oxidation of Zn-rich phase and other Zn atoms which diffused to the beta-Sn matrix grain boundaries which form ZnO. With Cr addition, two types of Sn-Zn-Cr phases, along the grain boundaries of beta-Sn matrix and across the Zn-rich phase, were detected in Cr-bearing solder alloys, which prevent the oxygen from diffusing into the bulk of the solder, and the SZB0.3Cr alloy had the best oxidation resistance.
引用
收藏
页码:2812 / 2817
页数:6
相关论文
共 50 条
  • [31] Influence of the interfacial reaction layer on reliability of CSP joints using Sn-8Zn-3Bi solder and Ni/Au plating
    Sogo, Y
    Hojo, T
    Iwanishi, H
    Hirose, A
    Kobayashi, KF
    Yamaguch, A
    Furusawa, A
    Nishida, K
    MATERIALS TRANSACTIONS, 2004, 45 (03) : 734 - 740
  • [32] In对Sn-8Zn-3Bi无铅钎料润湿性的影响
    周健
    孙扬善
    薛烽
    稀有金属材料与工程, 2006, (04) : 613 - 616
  • [33] Sn-8Zn-3Bi无铅钎料的抗氧化性
    王常亮
    周健
    孙扬善
    方伊莉
    东南大学学报(自然科学版), 2008, (04) : 693 - 697
  • [34] Effects of current density on the formation and microstructure of Sn-9Zn, Sn-8Zn-3Bi and Sn-3Ag-0.5Cu solder joints
    Othman, R.
    Binh, D. N.
    Ismail, A. B.
    Long, B. D.
    Ariga, T.
    INTERMETALLICS, 2012, 22 : 1 - 6
  • [35] Isothermal low cycle fatigue Behavior of Sn-8Zn-3Bi on single shear solder joint
    Sun, P
    Andersson, C
    Cao, LQ
    Lai, ZH
    Cheng, ZN
    Wei, XC
    Liu, J
    55TH ELECTRONIC COMPONENTS & TECHNOLOGY CONFERENCE, VOLS 1 AND 2, 2005 PROCEEDINGS, 2005, : 696 - 700
  • [36] The Inhibition of Tin Whiskers on the Surface of Sn-8Zn-3Bi-0.5Ce Solders
    Jain, C. C.
    Chen, C. L.
    Lai, H. J.
    Chuang, T. H.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2011, 20 (06) : 1043 - 1048
  • [37] The Inhibition of Tin Whiskers on the Surface of Sn-8Zn-3Bi-0.5Ce Solders
    C. C. Jain
    C. L. Chen
    H. J. Lai
    T. H. Chuang
    Journal of Materials Engineering and Performance, 2011, 20 : 1043 - 1048
  • [38] Comments on "Effects of current density on the formation and microstructure of Sn-9Zn, Sn-8Zn-3Bi and Sn-3Ag-0.5Cu solder joints"
    Paul, A.
    Laurila, T.
    INTERMETALLICS, 2012, 28 : 164 - 165
  • [39] Interfacial Reactions, Microstructure, and Strength of Sn-8Zn-3Bi and Sn-9Zn-Al Solder on Cu and Au/Ni (P) Pads
    Chi-Shiung Hsi
    Ching-Tsung Lin
    Tao-Chih Chang
    Moo-Chin Wang
    Ming-Kann Liang
    Metallurgical and Materials Transactions A, 2010, 41 : 275 - 284
  • [40] 85℃时效Sn-8Zn-3Bi/Cu焊点界面化合物生长行为
    赵柏森
    赵国际
    特种铸造及有色合金, 2015, 35 (01) : 91 - 93