Microstructural evolution of mechanically alloyed and spark plasma sintered Ni-W alloy matrix composites

被引:5
|
作者
Genc, Aziz [1 ]
Kaya, Pinar [2 ]
Ayas, Erhan [2 ]
Ovecoglu, M. Lutfi [1 ]
Turan, Servet [2 ]
机构
[1] Istanbul Tech Univ, Dept Met & Mat Engn, TR-34469 Istanbul, Turkey
[2] AU, Dept Mat Sci & Engn, TR-26480 Eskisehir, Turkey
关键词
Ni-W alloys; Mechanical alloying; Spark plasma sintering; Transmission electron microscopy; SOLID-SOLUTION ALLOYS; HEAT-TREATMENT; POWDER-METALLURGY; NICKEL-TUNGSTEN; AMORPHIZATION; HARDNESS; FABRICATION; KINETICS; BEHAVIOR; FIELD;
D O I
10.1016/j.jallcom.2013.03.238
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Microstructural evolution of Ni(W) solid solution alloys fabricated via mechanical alloying (MA) of Ni - 30 wt.% W powders and spark plasma sintering (SPS) at 1000 degrees C for 3 min were presented in this study. Due to contaminations during MA, fabricated alloys are termed as Ni(W) solid solution alloy matrix composites. Effects of modifications on the processing conditions such as covering the graphite dies with hexagonal boron nitride spray and/or annealing of the as-MA'd powders on the microstructure of the SPS'ed Ni(W) alloy matrix composites were investigated via analytical transmission electron microscopy (TEM) studies. X-ray diffraction (XRD) and/or TEM investigations revealed that all the samples comprise Ni(W), WC and WO2 phases. A slightly reduced amount of 13.24 wt.% WC by covering the graphite dies, significantly reduced to 3.90 wt.% with the annealing of the MA'd powders. It is found that covering the graphite dies has led significant grain growth, whereas annealing of the powders had no significant effect on the grain size of SPS'ed samples. A 96.7% relative density value was increased to 97.3% with the covering of graphite dies, which further increased to 99.4% for the sample fabricated via SPS of the annealed powders with covered graphite dies. Although the amount of WC is decreased, a microhardness value of 4.28 GPa for the sample fabricated via SPS of as-MA'd powders, slightly increased to 4.35 GPa for the samples sintered by spray covered graphite dies, which further increased to 4.52 GPa with the applied annealing, revealing the enhancement of the microhardness values by increased W solubility in Ni lattices. (C) 2013 Elsevier B. V. All rights reserved.
引用
收藏
页码:159 / 167
页数:9
相关论文
共 50 条
  • [31] The Glassy Structure Formation and Phase Evolution in Mechanically Alloyed and Spark Plasma-Sintered Al-TM-RE Alloys
    Maurya, Ram S.
    Laha, Tapas
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (12) : 7407 - 7418
  • [32] Fabrication and properties of mechanically alloyed and Ni activated sintered W matrix composites reinforced with Y2O3 and TiB2 particles
    Genc, A.
    Coskun, S.
    Ovecoglu, M. L.
    MATERIALS CHARACTERIZATION, 2010, 61 (07) : 740 - 748
  • [33] Carbon uptake during Spark Plasma Sintering: investigation through the analysis of the carbide "footprint" in a Ni-W alloy
    Bokhonov, B. B.
    Ukhina, A. V.
    Dudina, D. V.
    Anisimov, A. G.
    Mali, V. I.
    Batraev, I. S.
    RSC ADVANCES, 2015, 5 (98): : 80228 - 80237
  • [34] Microstructural Characteristics and Mechanical Behavior of Spark Plasma-Sintered Cu–Cr–rGO Copper Matrix Composites
    Xin-Jiang Zhang
    Zhong-Kui Dai
    Xue-Ran Liu
    Wen-Chao Yang
    Meng He
    Zi-Run Yang
    ActaMetallurgicaSinica(EnglishLetters), 2018, 31 (07) : 761 - 770
  • [35] Microstructural Characteristics and Mechanical Behavior of Spark Plasma-Sintered Cu–Cr–rGO Copper Matrix Composites
    Xin-Jiang Zhang
    Zhong-Kui Dai
    Xue-Ran Liu
    Wen-Chao Yang
    Meng He
    Zi-Run Yang
    Acta Metallurgica Sinica (English Letters), 2018, 31 : 761 - 770
  • [36] Matrix Structure Evolution and Nanoreinforcement Distribution in Mechanically Milled and Spark Plasma Sintered Al-SiC Nanocomposites
    Saheb, Nouari
    Aliyu, Ismaila Kayode
    Hassan, Syed Fida
    Al-Aqeeli, Nasser
    MATERIALS, 2014, 7 (09): : 6748 - 6767
  • [37] Evaluation of microstructural and nanomechanical performance of spark plasma sintered TiFe-SiC reinforced aluminium matrix composites
    Akinwamide, Samuel Olukayode
    Lesufi, Miltia
    Akinribide, Ojo Jeremiah
    Mpolo, Peggy
    Olubambi, Peter Apata
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2020, 9 (06): : 12137 - 12148
  • [38] Thermal stability of spark plasma sintered aluminum matrix composites reinforced with Ni3Al
    Ferreira-Palma, C.
    De Leon-Murguia, N. V.
    Lagunes-Paredes, Y.
    Santaella-Gonzalez, J. B.
    Lopez-Hirata, V. M.
    Zuniga, M. A. Beltran
    Hernandez-Santiago, F.
    Dorantes-Rosales, H. J.
    MATERIALS LETTERS, 2024, 377
  • [39] DEVELOPMENT AND CHARACTERIZATION INVESTIGATIONS OF MECHANICALLY ALLOYED W-Ni/TiC COMPOSITES
    Coskun, Selim
    Genc, Aziz
    Ovecoglu, Mustafa L.
    EPD CONGRESS 2009, PROCEEDINGS, 2009, : 183 - 190
  • [40] Microstructures and high-temperature tensile properties of mechanically alloyed and spark plasma-sintered 304SS-CNT composites
    Cho, Hyo-haeng
    Lim, Sangyeob
    Jin, Hyung-Ha
    Kwon, Junhyun
    Hong, Soon-Jik
    Shin, Chansun
    JOURNAL OF COMPOSITE MATERIALS, 2018, 52 (20) : 2755 - 2766