Microstructural evolution of mechanically alloyed and spark plasma sintered Ni-W alloy matrix composites

被引:5
|
作者
Genc, Aziz [1 ]
Kaya, Pinar [2 ]
Ayas, Erhan [2 ]
Ovecoglu, M. Lutfi [1 ]
Turan, Servet [2 ]
机构
[1] Istanbul Tech Univ, Dept Met & Mat Engn, TR-34469 Istanbul, Turkey
[2] AU, Dept Mat Sci & Engn, TR-26480 Eskisehir, Turkey
关键词
Ni-W alloys; Mechanical alloying; Spark plasma sintering; Transmission electron microscopy; SOLID-SOLUTION ALLOYS; HEAT-TREATMENT; POWDER-METALLURGY; NICKEL-TUNGSTEN; AMORPHIZATION; HARDNESS; FABRICATION; KINETICS; BEHAVIOR; FIELD;
D O I
10.1016/j.jallcom.2013.03.238
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Microstructural evolution of Ni(W) solid solution alloys fabricated via mechanical alloying (MA) of Ni - 30 wt.% W powders and spark plasma sintering (SPS) at 1000 degrees C for 3 min were presented in this study. Due to contaminations during MA, fabricated alloys are termed as Ni(W) solid solution alloy matrix composites. Effects of modifications on the processing conditions such as covering the graphite dies with hexagonal boron nitride spray and/or annealing of the as-MA'd powders on the microstructure of the SPS'ed Ni(W) alloy matrix composites were investigated via analytical transmission electron microscopy (TEM) studies. X-ray diffraction (XRD) and/or TEM investigations revealed that all the samples comprise Ni(W), WC and WO2 phases. A slightly reduced amount of 13.24 wt.% WC by covering the graphite dies, significantly reduced to 3.90 wt.% with the annealing of the MA'd powders. It is found that covering the graphite dies has led significant grain growth, whereas annealing of the powders had no significant effect on the grain size of SPS'ed samples. A 96.7% relative density value was increased to 97.3% with the covering of graphite dies, which further increased to 99.4% for the sample fabricated via SPS of the annealed powders with covered graphite dies. Although the amount of WC is decreased, a microhardness value of 4.28 GPa for the sample fabricated via SPS of as-MA'd powders, slightly increased to 4.35 GPa for the samples sintered by spray covered graphite dies, which further increased to 4.52 GPa with the applied annealing, revealing the enhancement of the microhardness values by increased W solubility in Ni lattices. (C) 2013 Elsevier B. V. All rights reserved.
引用
收藏
页码:159 / 167
页数:9
相关论文
共 50 条
  • [21] TiAl Alloy Spark Plasma Sintered from Mechanically Activated Powders
    Wang, Zhi-Wei
    Chen, Jun
    MATERIALS AND DESIGN, PTS 1-3, 2011, 284-286 : 2336 - 2339
  • [22] Effect of Ta addition on the sinterability of spark plasma sintered W-Ni-Fe alloy
    Muthuchamy, A.
    Srikanth, Muthe
    Yadav, Dig Vijay
    Annamalai, A. Raja
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART B-JOURNAL OF ENGINEERING MANUFACTURE, 2023, 237 (10) : 1518 - 1525
  • [23] Mechanical and Tribological Behavior of Mechanically Alloyed Ni-TiC Composites Processed via Spark Plasma Sintering
    Walunj, Ganesh
    Bearden, Anthony
    Patil, Amit
    Larimian, Taban
    Christudasjustus, Jijo
    Gupta, Rajeev Kumar
    Borkar, Tushar
    MATERIALS, 2020, 13 (22) : 1 - 19
  • [24] Role of binder phase on the microstructure and mechanical properties of a mechanically alloyed and spark plasma sintered WC-FCC HEA composites
    Yadav, Surekha
    Zhang, Qiaofu
    Behera, Amit
    Haridas, Ravi Sankar
    Agrawal, Priyanshi
    Gong, Jiadong
    Mishra, Rajiv S.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 877
  • [25] A study on microstructural evolution and corrosion behavior of spark plasma sintered Fe-Cr alloy system
    Kundu, Arnab
    Shrestha, Nikunja
    Korjenic, Alen
    Raja, Krishnan S.
    Charit, Indrajit
    JOURNAL OF MATERIALS SCIENCE, 2019, 54 (22) : 14171 - 14188
  • [26] On the reduction and effect of non-metallic impurities in mechanically alloyed nanocrystalline Ni-W alloys
    Marvel, C. J.
    Smeltzer, J. A.
    Hornbuckle, B. C.
    Darling, K. A.
    Harmer, M. P.
    ACTA MATERIALIA, 2020, 200 (200) : 12 - 23
  • [27] Microstructural evolution in mechanically alloyed Al-heavy-metal oxide composites
    Blaz, L
    Kaneko, J
    Sugamata, M
    MATERIALS CHEMISTRY AND PHYSICS, 2003, 81 (2-3) : 387 - 389
  • [28] Microstructural evolution of reactive-sintered aluminum matrix composites
    Chen, Zhong-Chun
    Takeda, Takenobu
    Ikeda, Keisuke
    COMPOSITES SCIENCE AND TECHNOLOGY, 2008, 68 (10-11) : 2245 - 2253
  • [29] Metastability of mechanically alloyed and spark plasma sintered Co50Ti50 powder
    Martínez Sánchez, Roberto
    Magaña, Francisco Espinosa
    Moller, Alberto Duarte
    Cabañas Moreno, José Gerardo
    Rios Jara, David
    Nishikawa, Yoshito
    De La Torre, Sebastián Díaz
    Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 2000, 47 (05): : 480 - 483
  • [30] The Glassy Structure Formation and Phase Evolution in Mechanically Alloyed and Spark Plasma-Sintered Al-TM-RE Alloys
    Ram S. Maurya
    Tapas Laha
    Journal of Materials Engineering and Performance, 2019, 28 : 7407 - 7418