Microstructural evolution of mechanically alloyed and spark plasma sintered Ni-W alloy matrix composites

被引:5
|
作者
Genc, Aziz [1 ]
Kaya, Pinar [2 ]
Ayas, Erhan [2 ]
Ovecoglu, M. Lutfi [1 ]
Turan, Servet [2 ]
机构
[1] Istanbul Tech Univ, Dept Met & Mat Engn, TR-34469 Istanbul, Turkey
[2] AU, Dept Mat Sci & Engn, TR-26480 Eskisehir, Turkey
关键词
Ni-W alloys; Mechanical alloying; Spark plasma sintering; Transmission electron microscopy; SOLID-SOLUTION ALLOYS; HEAT-TREATMENT; POWDER-METALLURGY; NICKEL-TUNGSTEN; AMORPHIZATION; HARDNESS; FABRICATION; KINETICS; BEHAVIOR; FIELD;
D O I
10.1016/j.jallcom.2013.03.238
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Microstructural evolution of Ni(W) solid solution alloys fabricated via mechanical alloying (MA) of Ni - 30 wt.% W powders and spark plasma sintering (SPS) at 1000 degrees C for 3 min were presented in this study. Due to contaminations during MA, fabricated alloys are termed as Ni(W) solid solution alloy matrix composites. Effects of modifications on the processing conditions such as covering the graphite dies with hexagonal boron nitride spray and/or annealing of the as-MA'd powders on the microstructure of the SPS'ed Ni(W) alloy matrix composites were investigated via analytical transmission electron microscopy (TEM) studies. X-ray diffraction (XRD) and/or TEM investigations revealed that all the samples comprise Ni(W), WC and WO2 phases. A slightly reduced amount of 13.24 wt.% WC by covering the graphite dies, significantly reduced to 3.90 wt.% with the annealing of the MA'd powders. It is found that covering the graphite dies has led significant grain growth, whereas annealing of the powders had no significant effect on the grain size of SPS'ed samples. A 96.7% relative density value was increased to 97.3% with the covering of graphite dies, which further increased to 99.4% for the sample fabricated via SPS of the annealed powders with covered graphite dies. Although the amount of WC is decreased, a microhardness value of 4.28 GPa for the sample fabricated via SPS of as-MA'd powders, slightly increased to 4.35 GPa for the samples sintered by spray covered graphite dies, which further increased to 4.52 GPa with the applied annealing, revealing the enhancement of the microhardness values by increased W solubility in Ni lattices. (C) 2013 Elsevier B. V. All rights reserved.
引用
收藏
页码:159 / 167
页数:9
相关论文
共 50 条
  • [1] Microstructural and nanoindentation study of spark plasma sintered high entropy alloy reinforced aluminium matrix composites
    Salifu, Smith
    Olubambi, Peter Apata
    JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 999
  • [2] Microstructure evolution and mechanical properties of spark plasma sintered W-Ni-Mn alloy
    Pan, Yan-lin
    Ding, Lei
    Xiang, Dao-ping
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2017, 27 (07) : 1588 - 1593
  • [3] Microstructural Characterization of Mechanically Alloyed FeCoNiMnV High Entropy Alloy Consolidated by Spark Plasma Sintering
    Alijani, Fatemeh
    Reihanian, Mohsen
    Gheisari, Khalil
    Yuasa, Motohiro
    Miyamoto, Hiroyuki
    ADVANCED ENGINEERING MATERIALS, 2020, 22 (04)
  • [4] Densification and microstructural evolution of spark plasma sintered NiTi shape memory alloy
    Velmurugan, C.
    Senthilkumar, V
    Biswas, Krishanu
    Yadav, Surekha
    ADVANCED POWDER TECHNOLOGY, 2018, 29 (10) : 2456 - 2462
  • [5] Development of Mechanically Alloyed and Sintered W-1 wt.% Ni Matrix Composites Reinforced with TiB2
    Agaogullari, Duygu
    Balci, Ozge
    Demirkan, O. Utku
    Gokce, Hasan
    Genc, Aziz
    Ovecoglu, M. Lutfi
    Duman, Ismail
    SOLID COMPOUNDS OF TRANSITION ELEMENTS II, 2013, 194 : 194 - 198
  • [6] Structural Evolution in Mechanically Alloyed and Spark Plasma Sintered Iron–0.15 wt.% MWCNT Composite
    Priyanka Sharma
    Akshay Kumar
    M. K. Banerjee
    Journal of Materials Engineering and Performance, 2018, 27 : 4740 - 4748
  • [7] Structural Evolution in Mechanically Alloyed and Spark Plasma Sintered Iron-0.15wt.% MWCNT Composite
    Sharma, Priyanka
    Kumar, Akshay
    Banerjee, M. K.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2018, 27 (09) : 4740 - 4748
  • [8] Microstructural control of sintered mechanically alloyed Al-1%Ni material
    Cintas, J
    Cuevas, FG
    Montes, JM
    Herrera, EJ
    SCRIPTA MATERIALIA, 2005, 52 (05) : 341 - 345
  • [9] TUNGSTEN SOLUTION KINETICS AND AMORPHIZATION OF NICKEL IN MECHANICALLY ALLOYED NI-W ALLOYS
    ANING, AO
    WANG, Z
    COURTNEY, TH
    ACTA METALLURGICA ET MATERIALIA, 1993, 41 (01): : 165 - 174
  • [10] Microstructural Evolution of Ni-SiC Composites Manufactured by Spark Plasma Sintering
    Chmielewski, Marcin
    Zybala, Rafal
    Strojny-Nedza, Agata
    Piatkowska, Anna
    Dobrowolski, Artur
    Jagiello, Jakub
    Diduszko, Ryszard
    Bazarnik, Piotr
    Nosewicz, Szymon
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2023, 54 (06): : 2191 - 2207