Microstructure formation and elevated temperature mechanical properties of directionally solidified Ti44Al6Nb1Cr alloy

被引:10
|
作者
Liu, Yangli [1 ]
Xue, Xiang [1 ]
Tan, Yingmei [1 ]
Fang, Hongze [1 ]
Cui, Hongzhi [2 ]
Chen, Ruirun [1 ,2 ]
机构
[1] Harbin Inst Technol, Natl Key Lab Precis Hot Proc Met, Harbin 150001, Peoples R China
[2] Shandong Univ Sci & Technol, Sch Mat Sci & Engn, Qingdao 266590, Peoples R China
基金
中国国家自然科学基金;
关键词
TiAl alloy; CCDS; Columnar grains; Mechanical properties; HIGH-NB; TIAL ALLOY; PHASE-TRANSFORMATION; OXIDATION BEHAVIOR; TENSILE PROPERTIES; EVOLUTION; REFINEMENT; STRENGTH; DESIGN; BORON;
D O I
10.1016/j.msea.2020.140038
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
To improve room and elevated temperature mechanical properties of high-Nb TiAl alloys, Ti44Al6Nb1Cr alloy has been prepared by cold crucible directional solidification (CCDS) technique under loaded power of 40 kW and pulling rate of 8.3 mu m/s. Macro/micro-structure and phase composition have been characterized. Tensile properties have been tested at room and elevated temperature and the related mechanisms have been revealed. Results show that equiaxed grains change to columnar grains growing up along the axial direction of ingot after CCDS. Phase component is still composed of alpha(2), gamma and B2 phases. Microstructure consists of lamellar clusters and network structure. The lamellar clusters in a grain possess the same orientation. The content and size of B2 phases decrease and some casting defects with small size decrease as well due to sufficient diffusion of Nb and Cr atoms under action of electromagnetic force during CCDS. Tensile results indicate that comprehensive mechanical properties of Ti44Al6Nb1Cr alloy are improved significantly after CCDS. At room temperature, ultimate tensile strength and total strain are 523 MPa and 3.03%, respectively, which are improved by 18.1% and 64.7% compared with that of as-cast Ti44Al6Nb1Cr alloy (443 MPa and 1.84%). Moreover, fracture morphology also indicates that there are many deep ravines between cleavage steps and some similar dimples microstructure on cleavage steps. They are beneficial to improving comprehensive mechanical properties. At 973 K, ultimate tensile strength of Ti44Al6Nb1Cr alloy does not decrease at all, still reaching 530 MPa after CCDS. When service temperature rises to 1173 K, the strain is less than 4.28% showing excellent mechanical stability under tensile stress less than 436 MPa. The excellent stability for mechanical properties is due to thin lamellar phases, directional microstructure and large plastic deformation region.
引用
收藏
页数:9
相关论文
共 50 条
  • [31] Effect of growth rate on microstructure and microhardness of directionally solidified Ti-44Al-5Nb-1.5Cr-1.5Zr-1Mo-0.1B alloy
    Li, Zhi-ping
    Xia, Hong-ying
    Luo, Liang-shun
    Wang, Bin-bin
    Wang, Liang
    Su, Yan-qing
    Guo, Jing-jie
    Fu, Heng-zhi
    CHINA FOUNDRY, 2020, 17 (04) : 293 - 300
  • [32] Effect of growth rate on microstructure and microhardness of directionally solidified Ti-44Al-5Nb-1.5Cr-1.5Zr-1Mo-0.1B alloy
    Zhi-ping Li
    Hong-ying Xia
    Liang-shun Luo
    Bin-bin Wang
    Liang Wang
    Yan-qing Su
    Jing-jie Guo
    Heng-zhi Fu
    China Foundry, 2020, 17 (04) : 293 - 300
  • [33] Effect of Growth Rate on Microstructure Evolution and Hardness in Directionally Solidified Ti-50Al-6Nb Alloy
    Liu Guohuai
    Zhang Yuan
    Li Xinzhong
    Chen Ruirun
    Su Yanqing
    Guo Jingjie
    Fu Hengzhi
    RARE METAL MATERIALS AND ENGINEERING, 2015, 44 (07) : 1655 - 1660
  • [34] Microstructure Development of Directionally Solidified Nb-Ti-Si Based Ultrahigh Temperature Alloy
    Guo Haisheng Guo Xiping Yao Chengfang State Key Laboratory of Solidification Processing Northwestern Polytechnical University Xian China
    稀有金属材料与工程, 2009, 38(S3) (S3) : 24 - 27
  • [35] Microstructure Development of Directionally Solidified Nb-Ti-Si Based Ultrahigh Temperature Alloy
    Guo Haisheng
    Guo Xiping
    Yao Chengfang
    RARE METAL MATERIALS AND ENGINEERING, 2009, 38 : 24 - 27
  • [36] Eutectic microstructure evolution in a directionally solidified Nb-Al alloy
    Rios, CT
    Milenkovic, S
    Caram, R
    SOLIDIFICATION AND GRAVITY 2000, 2000, 329-3 : 179 - 184
  • [37] Microstructure Formation in Directionally Solidified Pb-Al Alloy
    Li Yanqiang
    Zhao Jiuzhou
    Jiang Hongxiang
    He Jie
    ACTA METALLURGICA SINICA, 2022, 58 (08) : 1072 - 1082
  • [38] Microstructure and mechanical properties of directionally solidified Nb-22Ti-16Si-7Cr-3Al-3Ta-2Hf-0.1Ho alloy
    Tian, Yuxin
    Cheng, Guangming
    Guo, Jianting
    Zhou, Lanzhang
    He, Lianlong
    Ye, Hengqiang
    ADVANCED ENGINEERING MATERIALS, 2007, 9 (11) : 963 - 966
  • [39] EUTECTIC MICROSTRUCTURE EVOLUTION OF DIRECTIONALLY SOLIDIFIED Nb-Ti-Si BASE ULTRAHIGH TEMPERATURE ALLOY
    Li Xiaofei
    Guo Xiping
    ACTA METALLURGICA SINICA, 2013, 49 (07) : 853 - 862
  • [40] Microstructure control and mechanical properties of Ti44Al6Nb1.0Cr2.0V alloy by cold crucible directional solidification
    Dong, Shulin
    Chen, Ruirun
    Guo, Jingjie
    Ding, Hongsheng
    Su, Yanqing
    Fu, Hengzhi
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 614 : 67 - 74