The effect of manufacturing defects on the fatigue life of selective laser melted Ti-6Al-4V structures

被引:245
|
作者
Hu, Y. N. [1 ]
Wu, S. C. [1 ,2 ]
Withers, P. J. [2 ]
Zhang, J. [3 ]
Bao, H. Y. X. [1 ]
Fu, Y. N. [4 ]
Kang, G. Z. [1 ]
机构
[1] Southwest Jiaotong Univ, State Key Lab Tract Power, Chengdu 610031, Peoples R China
[2] Univ Manchester, Henry Royce Inst, Dept Mat, Manchester M13 9PL, Lancs, England
[3] AVIC Mfg Technol Inst, Beijing 100024, Peoples R China
[4] Chinese Acad Sci, Shanghai Adv Res Inst, Shanghai Synchrotron Radiat Facil SSRF, Shanghai 201204, Peoples R China
基金
英国工程与自然科学研究理事会; 欧洲研究理事会; 中国国家自然科学基金;
关键词
Defect tolerance method; Additive manufacturing; Fatigue crack initiation and growth; High cycle fatigue (HCF); Digital printing; MECHANICAL-PROPERTIES; POROSITY DEFECTS; PERFORMANCE; STRENGTH; ELECTRON; BEHAVIOR; ROUGHNESS; STRESS; DAMAGE;
D O I
10.1016/j.matdes.2020.108708
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The manufacturing defects introduced by selective laser melting typically lead to lower fatigue strength and a larger variation in fatigue life compared to conventionally manufactured structures. X-ray micro computed tomography (mu CT) is used to characterize the porosity and lack of fusion defects in terms of population, morphol-ogy, dimension and location. The defect size and location are combined with the NASA/FLACGRO (NASGRO) fatigue crack growth model to predict the likely fatigue life, in which an effective initial crack length is de fined using the cyclic plastic zone and the defect radius. An eXtended defect zone (XDZ) describing the propensity for local plasticity during fatigue around a defect has been shown through numerical analysis to be a good indicator of the ranking of the threat to fatigue caused by differently located manufacturing defects. This indicates that the effect of a defect, initial radius, r(0) , is likely to be pronounced when its center is within 2r(0) of the surface and maximal when it lies just beneath the surface. (C) 2020 The Author(s). Published by Elsevier Ltd.
引用
收藏
页数:10
相关论文
共 50 条
  • [31] Effect of Build Orientation on the Corrosion Behavior and Mechanical Properties of Selective Laser Melted Ti-6Al-4V
    Sui, Qingxuan
    Li, Peizhen
    Wang, Kunlun
    Yin, Xiaotian
    Liu, Lingyu
    Zhang, Yuying
    Zhang, Qingxia
    Wang, Shenghai
    Wang, Li
    METALS, 2019, 9 (09)
  • [32] Effect of mean stress on fretting fatigue of Ti-6Al-4V on Ti-6Al-4V
    Lovrich, NR
    Neu, RW
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2006, 29 (01) : 41 - 55
  • [33] Effect of concentrated solar energy on microstructure evolution of selective  laser melted Ti-6Al-4V alloy
    Lucia-Antoneta Chicos
    Sebastian Marian Zaharia
    Grzegorz Cempura
    Adam Kruk
    Sebastian Lech
    Oleksandr Kryshtal
    Maciej Ziętara
    Grzegorz Michta
    Jose Rodríguez
    Mihaela Cosnita
    Mihai Alin Pop
    Camil Lancea
    The International Journal of Advanced Manufacturing Technology, 2022, 118 : 3183 - 3207
  • [34] Corrosion behavior of selective laser melted Ti-6Al-4V alloy in NaCl solution
    Dai, Nianwei
    Zhang, Lai-Chang
    Zhang, Junxi
    Chen, Qimeng
    Wu, Maoliang
    CORROSION SCIENCE, 2016, 102 : 484 - 489
  • [35] Prediction of microstructure in selective laser melted Ti-6Al-4V alloy by cellular automaton
    Yang, Jingjing
    Yu, Hanchen
    Yang, Huihui
    Li, Fanzhi
    Wang, Zemin
    Zeng, Xiaoyan
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 748 : 281 - 290
  • [36] Effect of concentrated solar energy on microstructure evolution of selective laser melted Ti-6Al-4V alloy
    Chicos, Lucia-Antoneta
    Zaharia, Sebastian Marian
    Cempura, Grzegorz
    Kruk, Adam
    Lech, Sebastian
    Kryshtal, Oleksandr
    Zietara, Maciej
    Michta, Grzegorz
    Rodriguez, Jose
    Cosnita, Mihaela
    Pop, Mihai Alin
    Lancea, Camil
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2022, 118 (9-10): : 3183 - 3207
  • [37] Role of martensite decomposition in tensile properties of selective laser melted Ti-6Al-4V
    Cao, Sheng
    Chu, Ruikun
    Zhou, Xigen
    Yang, Kun
    Jia, Qingbo
    Lim, Chao Voon Samuel
    Huang, Aijun
    Wu, Xinhua
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 744 : 357 - 363
  • [38] CAVITATION EROSION OF LASER MELTED AND LASER NITRIDED TI-6AL-4V
    ROBINSON, JM
    ANDERSON, S
    KNUTSEN, RD
    REED, RC
    MATERIALS SCIENCE AND TECHNOLOGY, 1995, 11 (06) : 611 - 618
  • [39] Specific heat treatment of selective laser melted Ti-6Al-4V for biomedical applications
    Huang, Qianli
    Liu, Xujie
    Yang, Xing
    Zhang, Ranran
    Shen, Zhijian
    Feng, Qingling
    FRONTIERS OF MATERIALS SCIENCE, 2015, 9 (04) : 373 - 381
  • [40] AN INVESTIGATION OF HIGH TEMPERATURE TENSILE PROPERTIES OF SELECTIVE LASER MELTED TI-6AL-4V
    Baitimerov, R. M.
    Lykov, P. A.
    Radionova, L. V.
    Akhmedianov, A. M.
    Samoilov, S. P.
    PROCEEDINGS OF THE 3RD INTERNATIONAL CONFERENCE ON PROGRESS IN ADDITIVE MANUFACTURING, 2018, : 439 - 444