The Effect of Flue Gas Environment on the Corrosion Behavior of the Sulfuric Acid Dew-Point Corrosion Resistant Steel

被引:2
|
作者
Lee, Byoung Ho [1 ]
Jo, Minho [1 ]
Yoo, Yun Ha [2 ]
机构
[1] POSCO Tech Res Labs, Pohang Res Lab, Steel Prod Res Grp 2, Pohang 790785, South Korea
[2] Steel Solut Mkt Off, POSCO Steel Business Div, Mat Performance Search Grp, Pohang 790785, South Korea
关键词
Corrosion; Acid Dew Point Corrosion; Corrosion Resistant Steel; Thermal Power Plant;
D O I
10.4028/www.scientific.net/MSF.941.1705
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In order to compare the corrosion resistance of conventional low carbon steel, Cu containing low carbon steel for sulfuric acid dew-point corrosion inhibition, and stainless 409L, immersion tests were carried out in 50 wt.% sulfuric acid. The effects of HCl concentraion on the corrosion behavior in a fixed sulfuric acid concentration (16.9 vol.%) was also investigated by immersion test. In addition to immersion test, field test in a thermal plant was carried out for 10 months. As a result, it was confirmed that Cu-containing dew-point corrosion resistent steel has the highest corrosion resistance compared with other materials. To verify superior corrosion resistence of dew-point corrosion resistant steel, surface morpology after various test was observed by SEM. It was found that surface corroded product of the dew-point corrosion resistant steel was much denser and thicker compared with the other steel.
引用
下载
收藏
页码:1705 / 1709
页数:5
相关论文
共 50 条
  • [21] Study on the corrosion behavior of steel for the pump used in sulfuric acid
    Qin, Zirui
    Li, Longsheng
    Guo, Shan
    Gao, Wenhua
    Shanghai Jinshu/Shanghai Metals, 1998, 20 (04): : 30 - 35
  • [22] Inhibitors of steel corrosion in sulfuric acid
    Gerasyutina, L.I.
    Glushko, L.P.
    Petukhova, E.I.
    Soroka, I.A.
    Zashchita Metallov, 1997, 33 (05): : 533 - 534
  • [23] Inhibitors of steel corrosion in sulfuric acid
    Gerasyutina, LI
    Glushko, LP
    Petukhova, EI
    Soroka, IA
    PROTECTION OF METALS, 1997, 33 (05): : 481 - 482
  • [24] Titanium Containing High Strength Sulfuric Acid Corrosion Resistant Steel
    Guo, Hairong
    Li, Tingting
    Li, Hualong
    Toshihiko, Emi
    STEEL RESEARCH INTERNATIONAL, 2012, 83 (05) : 465 - 471
  • [25] Stress Corrosion Cracking Behavior of Stainless Steel 304 in the Sulfuric Acid Environment Due to Prestrain
    Badaruddin, Mohammad
    Suudi, Ahmad
    Hamni, Arinal
    MAKARA JOURNAL OF TECHNOLOGY, 2006, 10 (02): : 67 - 71
  • [26] Research on corrosion behavior of truck body steel in chlorine-containing sulfuric acid environment
    Li, Jinshuo
    Chen, Junhang
    Song, Jialiang
    Zhang, Xin
    Li, Zhaoliang
    Luo, Hong
    Yu, Wei
    Dong, Chaofang
    Xiao, Kui
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2022, 21 : 1878 - 1889
  • [27] Acid corrosion of steel - Effect of carbon content on the corrodibility of steel in sulfuric acid
    Damon, GH
    INDUSTRIAL AND ENGINEERING CHEMISTRY, 1941, 33 : 67 - 69
  • [28] Crevice Corrosion Behavior of Stainless Steels in a Flue Gas Desulfurization Environment
    Yong Hu
    Hao Zhang
    HuiYing Zhang
    MingHui Ouyang
    YongQi Hu
    LiHua Wang
    Cheng Chu
    JingChao Wang
    JingTang Wang
    Journal of Materials Engineering and Performance, 2023, 32 : 10567 - 10581
  • [29] FLUE-GAS ACID CORROSION
    LOBLEY, DG
    TAPPI JOURNAL, 1987, 70 (11): : 144 - 144
  • [30] Sulfuric acid dew point corrosion in waste heat boiler tube for copper smelting furnace
    Ebara, R.
    Tanaka, F.
    Kawasaki, M.
    ENGINEERING FAILURE ANALYSIS, 2013, 33 : 29 - 36