摘要
Objective: To study the interfacial ultra-morphology formed by "all-in-one" self-etch adhesives. Methods: Forty-nine extracted molars were assigned to one of five all-in-one adhesives: Adper Prompt L-Pop (AP, 3M ESPE); Clearfil S-3 Bond (S3, Kuraray); G-Bond (GB, GC America); iBond (iB, Heraeus Kulzer) and Xeno IV (XE, Dentsply Caulk). Adper Single Bond Plus (SB, 3M ESPE), a two-step etch&rinse adhesive, and Clearfil SE Bond (SE, Kuraray), a two-step self-etch adhesive, were used as controls. Dentin, unground enamel and ground enamel were used as bonding substrates. Dentin specimens were processed for FESEM and TEM analyses. Enamel specimens were processed for FESEM. Results: Dentin: GB, iB, S3, SE and XE resulted in a submicron-thick hybrid layer (0.2-0.7 mu m), but only S3 and SE did not result in interfacial gaps. AP resulted in the thickest hybrid layer (1.7-2.9 mu m) among the self-etch adhesives. SB resulted in a 3.4-5.2 mu m thick hybrid layer. Unground enamel-GB, iB and SE resulted in a mostly featureless morphology resembling that of untreated enamel with areas in which the superficial enamel layer was removed without dissolving the subsurface enamel. XE resulted in areas of intra-prismatic etching and areas without any etching pattern. S3 resulted in frequent shallow intra-prismatic etching, while AP was able to unveil the enamel crystallites across the entire enamel surface. Phosphoric acid in SB resulted in the deepest intra- and inter-prismatic demineralization. Ground enamel-AP resulted in a well-defined inter-prismatic etching pattern. iB, GB, SE and S3 resulted in islands of superficially dissolved enamel within areas without evidence of enamel dissolution. XE resulted in etched enamel areas with mild intraprismatic exposure of crystallites. Phosphoric acid in SB resulted in deep enamel etching. Conclusions: Only AP, an aggressive self-etch adhesive, showed enamel morphological features that resemble those created by etch&rinse adhesives. S3 and SE were the only self-etch adhesives that did not result in dentin interfacial debonding.
引用
收藏
页码:534 / 549
页数:16
相关论文
共 50 条
  • [31] In vitro permeability of etch-and-rinse and self-etch adhesives used for immediate dentin sealing
    Sahin, Cem
    Cehreli, Zafer C.
    Yenigul, Muhittin
    Dayangac, Bulent
    DENTAL MATERIALS JOURNAL, 2012, 31 (03) : 401 - 408
  • [32] Fatigue of enamel bonds with self-etch adhesives
    Erickson, Robert L.
    Barkmeier, Wayne W.
    Kimmes, Nicole S.
    DENTAL MATERIALS, 2009, 25 (06) : 716 - 720
  • [33] Aggressiveness of self-etch adhesives on unground enamel
    Tay, FR
    Pashley, DH
    King, NM
    Carvalho, RM
    Tsai, J
    Lai, SCN
    Marquezini, L
    OPERATIVE DENTISTRY, 2004, 29 (03) : 309 - 316
  • [34] Interactions of self-etch adhesives with resin composites
    Kurokawa, Rie
    Finger, Werner J.
    Hoffmann, Marcus
    Endo, Tatsuo
    Kanehira, Masafumi
    Komatsu, Masashi
    Manabe, Atsufumi
    JOURNAL OF DENTISTRY, 2007, 35 (12) : 923 - 929
  • [35] Effects of Double Application of Contemporary Self-Etch Adhesives on Their Bonding Performance to Dentin with Clinically Relevant Smear Layers
    Chowdhury, Abu Faem Mohammad Almas
    Saikaew, Pipop
    Alam, Arefin
    Sun, Jihao
    Carvalho, Ricardo M.
    Sano, Hidehiko
    JOURNAL OF ADHESIVE DENTISTRY, 2019, 21 (01): : 59 - 66
  • [36] Resin Bonding of Self-Etch Adhesives to Bovine Dentin Bleached from Pulp Chamber
    Haruyama, Akiko
    Kameyama, Atsushi
    Kato, Junji
    Takemoto, Shinji
    Oda, Yutaka
    Kawada, Eiji
    Takahashi, Toshiyuki
    Furusawa, Andmasahiro
    BIOMED RESEARCH INTERNATIONAL, 2016, 2016
  • [37] Comparison of enamel bond fatigue durability of universal adhesives and two-step self-etch adhesives in self-etch mode
    Tsujimoto, Akimasa
    Barkmeier, Wayne W.
    Hosoya, Yumiko
    Nojiri, Kie
    Nagura, Yuko
    Takamizawa, Toshiki
    Latta, Mark A.
    Miyazaki, Masashi
    AMERICAN JOURNAL OF DENTISTRY, 2017, 30 (05): : 279 - 284
  • [38] In vitro evaluation of giomers microleakage after exposure to 33% hydrogen peroxide:: Self-etch vs total-etch adhesives
    Deliperi, S
    Bardwell, DN
    Wegley, C
    Congiu, MD
    OPERATIVE DENTISTRY, 2006, 31 (02) : 227 - 232
  • [39] Bonding Performance of Universal Adhesives Applied to Nano-Hydroxyapatite Desensitized Dentin Using Etch-and-Rinse or Self-Etch Mode
    Meng, Yuchen
    Huang, Fan
    Wang, Silin
    Li, Meiwen
    Lu, Yi
    Pei, Dandan
    Li, Ang
    MATERIALS, 2021, 14 (16)
  • [40] One-year clinical performance of self-etch adhesives in posterior restorations
    Perdigao, Jorge
    Dutra-Correa, Maristela
    Castilhos, Natalia
    Carmo, Andre R. P.
    Anauate-Netto, Camillo
    Cordeiro, Hiram J. D.
    Amore, Ricardo
    Lewgoy, Hugo R.
    AMERICAN JOURNAL OF DENTISTRY, 2007, 20 (02): : 125 - 133