Oxidation protection of C/C-SiC composites by an electrophoretically deposited mullite precursor:: Cyclic thermogravimetric analysis

被引:18
|
作者
Damjanovic, T.
Argirusis, Chr.
Jokanovic, B.
Borchardt, G.
Moritz, K.
Mueller, E.
Herbig, R.
Weiss, R.
机构
[1] Tech Univ Clausthal, Inst Met, D-38678 Clausthal Zellerfeld, Germany
[2] TU Bergakad Freiberg, Inst Keram Werkstoffe, D-09596 Freiberg, Germany
[3] Schunk Kohlenstofftech GmbH, D-35452 Heuchelheim, Germany
关键词
mullite; composites; sol-gel synthesis; electrophoretic deposition;
D O I
10.1016/j.jeurceramsoc.2006.04.026
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Sufficiently thick and homogeneous layers which transform into mullite at T >= 1000 degrees C were synthesized by means of sot-gel technology and electrophoretically deposited onto the surface of C/C-Si-SiC composites. The protectiveness of the deposited mullite layers was isothermally tested in air in the temperature range 1200 <= T <= 1550 degrees C for up to 200 h. At temperatures above 1600 degrees C, the protectiveness of the deposited layer is reduced due to the existence of a liquid phase and the formation of CO bubbles above the cracks in the SiC layer. In order to prolong the protectiveness of our mullite layers at higher temperatures an additional layer from a suspension of mullite precursor with 5 wt.% of Al2O3 powder was deposited. The protectiveness of the obtained mullite and mullite/Al2O3 multilayer systems were also tested under cyclic conditions. These experiments yielded encouraging results, which will have to be confirmed at higher temperatures. (c) 2006 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1299 / 1302
页数:4
相关论文
共 50 条
  • [41] Effect of damage on flexural modulus of C/C-SiC composites
    Srivastava, VK
    Maile, K
    Bothe, K
    Udoh, A
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 354 (1-2): : 292 - 297
  • [42] Preparation and properties of C/C-SiC nano-composites
    Krnel, Kristoffer
    Stadler, Zmago
    Kosmac, Tomaz
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2007, 27 (2-3) : 1211 - 1216
  • [43] Tribological behaviour of C/C-SiC composites-A review
    Kumar, Parshant
    Srivastava, V. K.
    JOURNAL OF ADVANCED CERAMICS, 2016, 5 (01) : 1 - 12
  • [44] Tribological Properties of C/C-SiC Composites for Brake Discs
    Jang, G. H.
    Cho, K. H.
    Park, S. B.
    Lee, W. G.
    Hong, U. S.
    Jang, H.
    METALS AND MATERIALS INTERNATIONAL, 2010, 16 (01) : 61 - 66
  • [45] Impulse excitation nondestructive mapping of C/C-SiC composites
    Srivastava, VK
    Maile, K
    HIGH TEMPERATURE CERAMIC MATRIX COMPOSITES 5, 2005, : 569 - 573
  • [46] Mechanical properties and morphological studies of C/C-SiC composites
    Singh, Shraddha
    Srivastava, V. K.
    Prakash, Rajiv
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 534 : 707 - 710
  • [47] Tribological properties of C/C-SiC composites for brake discs
    G. H. Jang
    K. H. Cho
    S. B. Park
    W. G. Lee
    U. S. Hong
    H. Jang
    Metals and Materials International, 2010, 16 : 61 - 66
  • [48] Study on preparation and wear properties of C/C-SiC composites
    Zhao, Wei
    Zhu, Bo
    Shi, Zhengtang
    Cao, Weiwei
    ADVANCES IN ENERGY SCIENCE AND EQUIPMENT ENGINEERING, 2015, : 2889 - 2892
  • [49] High velocity impact perforation on C/C-SiC composites
    Srivastavas, VK
    Maile, K
    Klenk, A
    HIGH TEMPERATURES-HIGH PRESSURES, 1999, 31 (05) : 487 - 497
  • [50] Eddy current nondestructive mapping of C/C-SiC composites
    Srivastava, VK
    Udoh, A
    Maier, HP
    Knoch, P
    Maile, K
    FORSCHUNG IM INGENIEURWESEN-ENGINEERING RESEARCH, 2004, 68 (03): : 169 - 172