Fracture of nickel-titanium superelastic alloy in sodium hypochlorite solution

被引:25
|
作者
Yokoyama, K
Kaneko, K
Yabuta, E
Asaoka, K
Sakai, J
机构
[1] Univ Tokushima, Sch Dent, Dept Dent Engn, Tokushima 7708504, Japan
[2] Univ Tokushima, Sch Dent, Dept Orthodont, Tokushima 7708504, Japan
[3] Waseda Univ, Dept Mat Sci & Engn, Shinjuku Ku, Tokyo 1698555, Japan
关键词
Ni-Ti; superelastic alloy; fracture; corrosion; sodium hypochlorite;
D O I
10.1016/j.msea.2003.10.320
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Fracture of the Ni-Ti superelastic alloy for endodontic instruments such as files was investigated with a sustained tensile-loading test in sodium hypochlorite (NaOCl) solution of various concentrations. It was found that the time to fracture was reduced when the applied stress exceeded the critical stress for martensite transformation. When the applied stress was higher than the critical stress, the 0.3 mm diameter wires of the Ni-Ti superelastic alloy sometimes fractured within 60 min. From the results of observations of the fracture surface using a scanning electron microscope, it was revealed that the fracture of the Ni-Ti superelastic alloy is significantly influenced by corrosion when the applied stress was higher than the critical stress for martensite transformation. The results of the present study suggest that one of the causes of the fracture of Ni-Ti files during clinical use is corrosion under the applied stress above the critical stress for martensite transformation in NaOCI solution. (C) 2003 Elsevier B.V. All rights reserved.
引用
收藏
页码:43 / 48
页数:6
相关论文
共 50 条
  • [21] Force-deflection properties of superelastic nickel-titanium archwires
    Gurgel, JD
    Kerr, S
    Powers, JM
    LeCrone, V
    AMERICAN JOURNAL OF ORTHODONTICS AND DENTOFACIAL ORTHOPEDICS, 2001, 120 (04) : 378 - 382
  • [22] Load-deflection characteristics of superelastic nickel-titanium wires
    Bartzela, Theodosia N.
    Senn, Christiane
    Wichelhaus, Andrea
    ANGLE ORTHODONTIST, 2007, 77 (06) : 991 - 998
  • [23] Finite element modeling of superelastic nickel-titanium orthodontic wires
    Ben Naceur, Ines
    Charfi, Amin
    Bouraoui, Tarak
    Elleuch, Khaled
    JOURNAL OF BIOMECHANICS, 2014, 47 (15) : 3630 - 3638
  • [24] Fatigue behaviour of nickel-titanium superelastic wires and endodontic instruments
    Bahia, M. G. A.
    Gonzalez, B. M.
    Buono, V. T. L.
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2006, 29 (07) : 518 - 523
  • [25] BENDING PROPERTIES OF SUPERELASTIC AND NONSUPERELASTIC NICKEL-TITANIUM ORTHODONTIC WIRES
    KHIER, SE
    BRANTLEY, WA
    FOURNELLE, RA
    AMERICAN JOURNAL OF ORTHODONTICS AND DENTOFACIAL ORTHOPEDICS, 1991, 99 (04) : 310 - 318
  • [26] Force-deflection comparison of superelastic nickel-titanium archwires
    Mallory, DC
    English, JD
    Powers, JM
    Brantley, WA
    Bussa, HI
    AMERICAN JOURNAL OF ORTHODONTICS AND DENTOFACIAL ORTHOPEDICS, 2004, 126 (01) : 110 - 112
  • [27] Cyclic Fatigue Resistance of Three Different Nickel-Titanium Instruments after Immersion in Sodium Hypochlorite
    Pedulla, Eugenio
    Grande, Nicola M.
    Plotino, Gianluca
    Pappalardo, Alfio
    Rapisarda, Ernesto
    JOURNAL OF ENDODONTICS, 2011, 37 (08) : 1139 - 1142
  • [28] SPINODAL DECOMPOSITION OF A NICKEL-TITANIUM ALLOY
    SINCLAIR, R
    LEAKE, JA
    RALPH, B
    PHYSICA STATUS SOLIDI A-APPLIED RESEARCH, 1974, 26 (01): : 285 - 298
  • [29] Influence of sodium hypochlorite on mechanical properties of K3 nickel-titanium rotary instruments
    Galvao Barbosa, Fabiola Ormiga
    da Cunha Ponciano Gomes, Jose Antonio
    Pimenta de Araujo, Marcos Cesar
    JOURNAL OF ENDODONTICS, 2007, 33 (08) : 982 - 985
  • [30] Cyclic fatigue resistance of two reciprocating nickel-titanium instruments after immersion in sodium hypochlorite
    Pedulla, E.
    Grande, N. M.
    Plotino, G.
    Palermo, F.
    Gambarini, G.
    Rapisarda, E.
    INTERNATIONAL ENDODONTIC JOURNAL, 2013, 46 (02) : 155 - 159