Fracture of nickel-titanium superelastic alloy in sodium hypochlorite solution

被引:25
|
作者
Yokoyama, K
Kaneko, K
Yabuta, E
Asaoka, K
Sakai, J
机构
[1] Univ Tokushima, Sch Dent, Dept Dent Engn, Tokushima 7708504, Japan
[2] Univ Tokushima, Sch Dent, Dept Orthodont, Tokushima 7708504, Japan
[3] Waseda Univ, Dept Mat Sci & Engn, Shinjuku Ku, Tokyo 1698555, Japan
关键词
Ni-Ti; superelastic alloy; fracture; corrosion; sodium hypochlorite;
D O I
10.1016/j.msea.2003.10.320
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Fracture of the Ni-Ti superelastic alloy for endodontic instruments such as files was investigated with a sustained tensile-loading test in sodium hypochlorite (NaOCl) solution of various concentrations. It was found that the time to fracture was reduced when the applied stress exceeded the critical stress for martensite transformation. When the applied stress was higher than the critical stress, the 0.3 mm diameter wires of the Ni-Ti superelastic alloy sometimes fractured within 60 min. From the results of observations of the fracture surface using a scanning electron microscope, it was revealed that the fracture of the Ni-Ti superelastic alloy is significantly influenced by corrosion when the applied stress was higher than the critical stress for martensite transformation. The results of the present study suggest that one of the causes of the fracture of Ni-Ti files during clinical use is corrosion under the applied stress above the critical stress for martensite transformation in NaOCI solution. (C) 2003 Elsevier B.V. All rights reserved.
引用
收藏
页码:43 / 48
页数:6
相关论文
共 50 条
  • [1] Fracture analysis of hydrogen-charged nickel-titanium superelastic alloy
    Yokoyama, K
    Hamada, K
    Asaoka, K
    MATERIALS TRANSACTIONS JIM, 2001, 42 (01): : 141 - 144
  • [2] Effects of sodium hypochlorite on nickel-titanium Lightspeed® instruments
    Busslinger, A
    Sener, B
    Barbakow, F
    INTERNATIONAL ENDODONTIC JOURNAL, 1998, 31 (04) : 290 - 294
  • [3] The corrosion of nickel-titanium rotary endodontic instruments in sodium hypochlorite
    Novoa, X. R.
    Martin-Biedma, B.
    Varela-Patino, P.
    Collazo, A.
    Macias-Luaces, A.
    Cantatore, G.
    Perez, M. C.
    Magan-Munoz, F.
    INTERNATIONAL ENDODONTIC JOURNAL, 2007, 40 (01) : 36 - 44
  • [4] Anomalous relationship between hardness and wear properties of a superelastic nickel-titanium alloy
    Qian, LM
    Xiao, XD
    Sun, QP
    Yu, TX
    APPLIED PHYSICS LETTERS, 2004, 84 (07) : 1076 - 1078
  • [5] SUPERELASTIC NICKEL-TITANIUM ALLOYS - PROPERTIES AND APPLICATIONS
    STOCKEL, D
    METALL, 1993, 47 (08): : 728 - 733
  • [6] Microscopic superelastic behavior of a nickel-titanium alloy under complex loading conditions
    Ni, WY
    Cheng, YT
    Grummon, DS
    APPLIED PHYSICS LETTERS, 2003, 82 (17) : 2811 - 2813
  • [7] Mechanical properties of nickel-titanium endodontic instruments and the effect of sodium hypochlorite treatment
    Haikel, Y
    Serfaty, R
    Wilson, P
    Speisser, JM
    Allemann, C
    JOURNAL OF ENDODONTICS, 1998, 24 (11) : 731 - 735
  • [8] Effect of immersion in sodium hypochlorite on torque and fatigue resistance of nickel-titanium instruments
    Peters, Ove A.
    Roehlike, Jan O.
    Baumann, Michael A.
    JOURNAL OF ENDODONTICS, 2007, 33 (05) : 589 - 593
  • [9] Cutting efficiency of nickel-titanium endodontic instruments and the effect of sodium hypochlorite treatment
    Haikel, Y
    Serfaty, R
    Wilson, P
    Speisser, JM
    Allemann, C
    JOURNAL OF ENDODONTICS, 1998, 24 (11) : 736 - 739
  • [10] Effect of nitriding surface treatment on the corrosion resistance of dental nickel-titanium files in 5.25% sodium hypochlorite solution
    Liu, Jeng-Fen
    Lin, Mau-Chin
    Hsu, Ming-Lun
    Li, Uei-Ming
    Lin, Chun-Pin
    Tsai, Wen-Fa
    Ai, Chi-Fong
    Chen, Li-Kai
    Huang, Her-Hsiung
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 475 (1-2) : 789 - 793