Characterization of wear debris from metal-on-metal hip implants during normal wear versus edge-loading conditions

被引:22
|
作者
Kovochich, Michael [1 ]
Fung, Ernest S. [1 ]
Donovan, Ellen [2 ,4 ]
Unice, Kenneth M. [3 ]
Paustenbach, Dennis J. [2 ]
Finley, Brent L. [2 ]
机构
[1] Cardno ChemRisk, Aliso Viejo, CA 92656 USA
[2] Cardno ChemRisk, San Francisco, CA 94105 USA
[3] Cardno ChemRisk, Pittsburgh, PA 15222 USA
[4] Ramboll Environ, San Francisco, CA USA
关键词
metal-on-metal; hip implant; wear debris; particle characterization; edge loading; inclination angle; microseparation; COBALT-CHROMIUM ALLOY; IN-VIVO DETERMINATION; PHYSICOCHEMICAL PROPERTIES; QUANTITATIVE-ANALYSIS; JOINT PROSTHESES; BEARING SURFACES; COCRMO-ALLOY; ION LEVELS; CUP ANGLE; PARTICLES;
D O I
10.1002/jbm.b.33902
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Advantages of second-generation metal-on-metal (MoM) hip implants include low volumetric wear rates and the release of nanosized wear particles that are chemically inert and readily cleared from local tissue. In some patients, edge loading conditions occur, which result in higher volumetric wear. The objective of this study was to characterize the size, morphology, and chemistry of wear particles released from MoM hip implants during normal (40 degrees angle) and edge-loading (65 degrees angle with microseparation) conditions. The mean primary particle size by volume under normal wear was 35 nm (range: 9-152 nm) compared with 95 nm (range: 6-573 nm) under edge-loading conditions. Hydrodynamic diameter analysis by volume showed that particles from normal wear were in the nano- (<100 nm) to submicron (<1000 nm) size range, whereas edge-loading conditions generated particles that ranged from <100 nm up to 3000-6000 nm in size. Particles isolated from normal wear were primarily chromium (98.5%) and round to oval in shape. Edge-loading conditions generated more elongated particles (4.5%) (aspect ratio2.5) and more CoCr alloy particles (9.3%) compared with normal wear conditions (1.3% CoCr particles). By total mass, edge-loading particles contained approximately 640-fold more cobalt than normal wear particles. Our findings suggest that high wear conditions are a potential risk factor for adverse local tissue effects in MoM patients who experience edge loading. This study is the first to characterize both the physical and chemical characteristics of MoM wear particles collected under normal and edge-loading conditions. (c) 2017 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 106B: 986-996, 2018.
引用
收藏
页码:986 / 996
页数:11
相关论文
共 50 条
  • [31] MINIMIZED WEAR AND DEBRIS GENERATION THROUGH OPTIMIZED MACHINING OF CO-CR-MO ALLOYS FOR USE IN METAL-ON-METAL HIP IMPLANTS
    Deshpande, Ashish
    Yang, Shu
    Puleo, Dave
    Pienkowski, David
    Dillon, Oscar, Jr.
    Outeiro, Jose
    Jawahir, I. S.
    [J]. PROCEEDINGS OF THE ASME INTERNATIONAL MANUFACTURING SCIENCE AND ENGINEERING CONFERENCE, 2012, 2012, : 297 - 305
  • [32] Carbon composition effects on wear behaviour and wear mechanisms of metal-on-metal hip prosthesis
    Ihaddadene, R.
    Affatato, S.
    Zavalloni, M.
    Bouzid, S.
    Viceconti, M.
    [J]. COMPUTER METHODS IN BIOMECHANICS AND BIOMEDICAL ENGINEERING, 2011, 14 : 33 - 34
  • [33] A study of the wear of explanted metal-on-metal resurfacing hip prostheses
    Joyce, Thomas J.
    Langton, David J.
    Nargol, Antoni V. F.
    [J]. TRIBOLOGY INTERNATIONAL, 2011, 44 (05) : 517 - 522
  • [34] Effects of CoCr metal wear debris generated from metal-on-metal hip implants and Co ions on human monocyte-like U937 cells
    Posada, Olga M.
    Tate, Rothwelle J.
    Grant, M. Helen
    [J]. TOXICOLOGY IN VITRO, 2015, 29 (02) : 271 - 280
  • [35] Influence of simulator kinematics on the wear of metal-on-metal hip prostheses
    Firkins, P.J.
    Tipper, J.L.
    Ingham, E.
    Stone, M.H.
    Farrar, R.
    Fisher, J.
    [J]. Proceedings of the Institution of Mechanical Engineers, Part H: Journal of Engineering in Medicine, 2001, 215 (01) : 119 - 122
  • [36] Influence of simulator kinematics on the wear of metal-on-metal hip prostheses
    Firkins, PJ
    Tipper, JL
    Ingham, E
    Stone, MH
    Farrar, R
    Fisher, J
    [J]. PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART H-JOURNAL OF ENGINEERING IN MEDICINE, 2001, 215 (H1) : 119 - 121
  • [37] Wear and functional biological activity of wear debris generated from UHMWPE-on-Zirconia ceramic, metal-on-metal, and alumina ceramic-on-ceramic hip prostheses during hip simulator testing
    Tipper, JL
    Matthews, JB
    Ingham, E
    Stewart, TD
    Fisher, J
    Stone, MH
    [J]. FRICTION, LUBRICATION, AND WEAR OF ARTIFICIAL JOINTS, 2003, : 7 - 28
  • [38] Wear Simulation of Metal-on-Metal Hip Replacements With Frictional Contact
    Mattei, Lorenza
    Di Puccio, Francesca
    [J]. JOURNAL OF TRIBOLOGY-TRANSACTIONS OF THE ASME, 2013, 135 (02):
  • [39] Predictive wear modeling of the articulating metal-on-metal hip replacements
    Gao, Leiming
    Dowson, Duncan
    Hewson, Robert W.
    [J]. JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2017, 105 (03) : 497 - 506
  • [40] Neural cell responses to wear debris from metal-on-metal total disc replacements
    H. Lee
    J. B. Phillips
    R. M. Hall
    Joanne L. Tipper
    [J]. European Spine Journal, 2020, 29 : 2701 - 2712