Characterization of wear debris from metal-on-metal hip implants during normal wear versus edge-loading conditions

被引:22
|
作者
Kovochich, Michael [1 ]
Fung, Ernest S. [1 ]
Donovan, Ellen [2 ,4 ]
Unice, Kenneth M. [3 ]
Paustenbach, Dennis J. [2 ]
Finley, Brent L. [2 ]
机构
[1] Cardno ChemRisk, Aliso Viejo, CA 92656 USA
[2] Cardno ChemRisk, San Francisco, CA 94105 USA
[3] Cardno ChemRisk, Pittsburgh, PA 15222 USA
[4] Ramboll Environ, San Francisco, CA USA
关键词
metal-on-metal; hip implant; wear debris; particle characterization; edge loading; inclination angle; microseparation; COBALT-CHROMIUM ALLOY; IN-VIVO DETERMINATION; PHYSICOCHEMICAL PROPERTIES; QUANTITATIVE-ANALYSIS; JOINT PROSTHESES; BEARING SURFACES; COCRMO-ALLOY; ION LEVELS; CUP ANGLE; PARTICLES;
D O I
10.1002/jbm.b.33902
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Advantages of second-generation metal-on-metal (MoM) hip implants include low volumetric wear rates and the release of nanosized wear particles that are chemically inert and readily cleared from local tissue. In some patients, edge loading conditions occur, which result in higher volumetric wear. The objective of this study was to characterize the size, morphology, and chemistry of wear particles released from MoM hip implants during normal (40 degrees angle) and edge-loading (65 degrees angle with microseparation) conditions. The mean primary particle size by volume under normal wear was 35 nm (range: 9-152 nm) compared with 95 nm (range: 6-573 nm) under edge-loading conditions. Hydrodynamic diameter analysis by volume showed that particles from normal wear were in the nano- (<100 nm) to submicron (<1000 nm) size range, whereas edge-loading conditions generated particles that ranged from <100 nm up to 3000-6000 nm in size. Particles isolated from normal wear were primarily chromium (98.5%) and round to oval in shape. Edge-loading conditions generated more elongated particles (4.5%) (aspect ratio2.5) and more CoCr alloy particles (9.3%) compared with normal wear conditions (1.3% CoCr particles). By total mass, edge-loading particles contained approximately 640-fold more cobalt than normal wear particles. Our findings suggest that high wear conditions are a potential risk factor for adverse local tissue effects in MoM patients who experience edge loading. This study is the first to characterize both the physical and chemical characteristics of MoM wear particles collected under normal and edge-loading conditions. (c) 2017 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 106B: 986-996, 2018.
引用
收藏
页码:986 / 996
页数:11
相关论文
共 50 条
  • [21] Metal-on-metal hip replacements: Wear performance and cellular response to wear particles
    Campbell, P
    McKellop, H
    Alim, R
    Mirra, J
    Nutt, S
    Dorr, L
    Amstutz, HC
    [J]. COBALT-BASE ALLOYS FOR BIOMEDICAL APPLICATIONS, 1999, 1365 : 193 - 209
  • [22] Clinical wear performance of metal-on-metal hip arthroplasties
    Rieker, CB
    Köttig, P
    Schön, R
    Windler, M
    Wyss, UP
    [J]. ALTERNATIVE BEARING SURFACES IN TOTAL JOINT REPLACEMENT, 1998, 1346 : 144 - 156
  • [23] Clinical wear performance of metal-on-metal hip arthroplasties
    Rieker, Claude B.
    Köttig, Petra
    Schön, Rolf
    Windler, Markus
    Wyss, Urs P.
    [J]. ASTM Special Technical Publication, 1999, (1346): : 144 - 156
  • [24] Wear of surface engineered metal-on-metal hip prostheses
    J. Fisher
    X. Q. Hu
    T. D. Stewart
    S. Williams
    J. L. Tipper
    E. Ingham
    M. H. Stone
    C. Davies
    P. Hatto
    J. Bolton
    M. Riley
    C. Hardaker
    G. H. Isaac
    G. Berry
    [J]. Journal of Materials Science: Materials in Medicine, 2004, 15 : 225 - 235
  • [25] Individual motion patterns during gait and sit-to-stand contribute to edge-loading risk in metal-on-metal hip resurfacing
    Mellon, Stephen J.
    Grammatopoulos, George
    Andersen, Michael S.
    Pegg, Elise C.
    Pandit, Hemant G.
    Murray, David W.
    Gill, Harinderjit S.
    [J]. PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART H-JOURNAL OF ENGINEERING IN MEDICINE, 2013, 227 (07) : 799 - 810
  • [26] Characterization of metal-wear nanoparticles in pseudotumor following metal-on-metal hip resurfacing
    Xia, Zhidao
    Kwon, Young-Min
    Mehmood, Shahid
    Downing, Clive
    Jurkschat, Kerstin
    Murray, David W.
    [J]. NANOMEDICINE-NANOTECHNOLOGY BIOLOGY AND MEDICINE, 2011, 7 (06) : 674 - 681
  • [27] Surface Characterization of Retrieved Metal-on-Metal Total Hip Implants from Patients with Adverse Reaction to Metal Debris
    Burbano, Maria
    Russell, Robert
    Huo, Michael
    Welch, Robert
    Roy, Diana
    Rodrigues, Danieli C.
    [J]. MATERIALS, 2014, 7 (03): : 1866 - 1879
  • [28] Wear of surface engineered metal-on-metal hip prostheses
    Fisher, J
    Hu, XQ
    Stewart, TD
    Williams, S
    Tipper, JL
    Ingham, E
    Stone, MH
    Davies, C
    Hatto, P
    Bolton, J
    Riley, M
    Hardaker, C
    Isaac, GH
    Berry, G
    [J]. JOURNAL OF MATERIALS SCIENCE-MATERIALS IN MEDICINE, 2004, 15 (03) : 225 - 235
  • [29] The effect of microstructure on the wear of cobalt-based alloys used in metal-on-metal hip implants
    Varano, R
    Bobyn, JD
    Medley, JB
    Yue, S
    [J]. PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART H-JOURNAL OF ENGINEERING IN MEDICINE, 2006, 220 (H2) : 145 - 159
  • [30] The wear of metal-on-metal total hip prostheses measured in a hip simulator
    Scholes, SC
    Green, SM
    Unsworth, A
    [J]. PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART H-JOURNAL OF ENGINEERING IN MEDICINE, 2001, 215 (H6) : 523 - 530