Modeling the Interface between Lithium Metal and Its Native Oxide

被引:27
|
作者
Lowe, Jeffrey S. [1 ,2 ]
Siegel, Donald J. [3 ,4 ]
机构
[1] Purdue Univ, Davidson Sch Chem Engn, W Lafayette, IN 47907 USA
[2] Purdue Univ, Dept Chem, W Lafayette, IN 47907 USA
[3] Univ Michigan, Mech Engn Dept, Mat Sci & Engn, Energy Inst,Appl Phys Program, Ann Arbor, MI 48109 USA
[4] Univ Michigan, Joint Ctr Energy Storage Res, Ann Arbor, MI 48109 USA
关键词
batteries; energy storage; Li-metal anode; oxidation; amorphous interface; diffusivity; INITIO MOLECULAR-DYNAMICS; TOTAL-ENERGY CALCULATIONS; IN-SITU FORMATION; SELF-DIFFUSION; ION CONDUCTION; XPS ANALYSIS; SURFACE; LAYER; ANODE; 1ST-PRINCIPLES;
D O I
10.1021/acsami.0c12468
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Owing to their high theoretical capacities, batteries that employ lithium (Li) metal as the negative electrode are attractive technologies for next-generation energy storage. However, the successful implementation of lithium metal batteries is limited by several factors, many of which can be traced to an incomplete understanding of surface phenomena involving the Li anode. Here, first-principles calculations are used to characterize the native oxide layer on Li, including several properties associated with the Li/lithium oxide (Li2O) interface. Multiple interface models are examined; the models account for differing interface (chemical) terminations and degrees of atomic ordering (i.e., crystalline vs amorphous). The interfacial energy, formation energy, and strain energies are predicted for these models. The amorphous interface yields the lowest interfacial formation energy, suggesting that it is the most probable model under equilibrium conditions. The work of adhesion is evaluated for the crystalline interfaces, and it is found that the O-terminated interface exhibits a work of adhesion more than 30 times larger than that of the Li-terminated model, implying that Li will strongly wet an oxygen-rich Li2O surface. The electronic structure of the interfaces is characterized using Voronoi charge analysis and shifts in the Li 1s binding energies. The width of the Li/Li2O interface, as determined by deviations from bulklike charges and binding energies, extends beyond the region exhibiting interfacial structural distortions. Finally, the transport of Li ions through the amorphous oxide is quantified using ab initio molecular dynamics. Facile transport of Li+ through the native oxide is observed. Thus, increasing the percentage of amorphous Li2O in the solid electrolyte interphase may be beneficial for battery performance. In total, the phenomena quantified here will aid in the optimization of batteries that employ high-capacity Li metal anodes.
引用
收藏
页码:46015 / 46026
页数:12
相关论文
共 50 条
  • [21] Modeling the interface between crystalline silicon and silicon oxide polymorphs
    Kovacevic, Goran
    Pivac, Branko
    [J]. PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 2013, 210 (04): : 717 - 722
  • [22] Mechanochemical reaction at the interface between a metal plate and oxide powders
    A. Torosyan
    L. Takacs
    [J]. Journal of Materials Science, 2004, 39 : 5491 - 5496
  • [23] Mechanochemical reaction at the interface between a metal plate and oxide powders
    Torosyan, A
    Takacs, L
    [J]. JOURNAL OF MATERIALS SCIENCE, 2004, 39 (16-17) : 5491 - 5496
  • [24] ON THE NATURE OF THE INTERFACE BETWEEN A SOLID METAL AND ITS MELT
    HILLIARD, JE
    CAHN, JW
    [J]. ACTA METALLURGICA, 1958, 6 (12): : 772 - 774
  • [25] STAGES OF FORMATION OF AN INTERFACE BETWEEN SILICON AND ITS THERMAL OXIDE
    MONAKHOV, VV
    ROMANOV, OV
    KIRILLOV, SN
    URITSKII, VY
    SMIRNOV, VA
    [J]. SOVIET PHYSICS SEMICONDUCTORS-USSR, 1986, 20 (03): : 300 - 302
  • [26] EFFECTS OF ELECTROLYTE PH ON ELECTRICAL-PROPERTIES OF THE INTERFACE BETWEEN N-INSB AND ITS ANODIC NATIVE-OXIDE
    KILICOGLU, T
    OZTURK, ZZ
    EBEOGLU, MA
    TURUT, A
    OZDEMIR, M
    ALTINDAL, A
    [J]. INDIAN JOURNAL OF PURE & APPLIED PHYSICS, 1995, 33 (04) : 205 - 209
  • [27] Storage of Lithium Metal: The Role of the Native Passivation Layer for the Anode Interface Resistance in Solid State Batteries
    Otto, Svenja-K
    Fuchs, Till
    Moryson, Yannik
    Lerch, Christian
    Mogwitz, Boris
    Sann, Joachim
    Janek, Juergen
    Henss, Anja
    [J]. ACS APPLIED ENERGY MATERIALS, 2021, 4 (11) : 12798 - 12807
  • [28] Phase-field modeling of planar interface electrodeposition in lithium-metal batteries
    Arguello, Marcos Exequiel
    Gumulya, Monica
    Derksen, Jos
    Utikar, Ranjeet
    Calo, Victor Manuel
    [J]. JOURNAL OF ENERGY STORAGE, 2022, 50
  • [29] Effects of polishing treatments on the interface between garnet solid electrolyte and lithium metal
    Ma, Xiaoning
    Xu, Youlong
    [J]. ELECTROCHIMICA ACTA, 2023, 441
  • [30] Interface behavior between garnet-type lithium-conducting solid electrolyte and lithium, metal
    Sudo, R.
    Nakata, Y.
    Ishiguro, K.
    Matsui, M.
    Hirano, A.
    Takeda, Y.
    Yamamoto, O.
    Imanishi, N.
    [J]. SOLID STATE IONICS, 2014, 262 : 151 - 154