Effects of water vapor on corrosion behaviors of C/SiC in oxidizing atmosphere containing Na2SO4 vapor

被引:13
|
作者
Luan, Xin'gang [1 ]
Zhang, Jun [1 ]
Cheng, Laifei [1 ]
机构
[1] NW Polytech Univ, Sci & Technol Thermlstruct Composite Mat Lab, Xian 710072, Shaanxi, Peoples R China
关键词
Ceramic-matrix composites (CMCs); Corrosion; Damage mechanics; Electron microscopy; SIO2 SCALE VOLATILITY; SILICON-BASED CERAMICS; COMBUSTION CONDITIONS; SALT VAPOR; ENVIRONMENTS; OXIDATION; COMPOSITE; RECESSION; KINETICS; CARBIDE;
D O I
10.1016/j.compositesb.2012.05.047
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Corrosion of a C/SiC composite has been investigated in the atmosphere containing oxygen, water vapor and sodium sulfate vapor at the temperatures range from 1000 to 1500 degrees C. The effect of water vapor on the corrosion mechanism of C/SiC were discussed based on the weight change, the residual strength change, the microstructure and calculated results from FactSage. The corrosion of C/SiC is attributed to (i) the permeation of gas through the SiO2 film below 1300 degrees C, (ii) the diffusion of oxidant through pores caused by bubbles broken in the SiO2 film above 1300 degrees C. The water vapor does not change the corrosion mechanism of C/SiC composite but the temperature range in which the corrosion mechanism works by accelerating the oxidation of SIC and the corrosion of SiO2. (C) 2012 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2968 / 2972
页数:5
相关论文
共 50 条
  • [21] Corrosion behaviours of copper alloy in solutions containing Na2SO4 and NaCl with different concentrations
    El-Meligi, A.A.
    Journal of Materials Science and Technology, 2002, 18 (06): : 549 - 551
  • [22] Corrosion behaviours of copper alloy in solutions containing Na2SO4 and NaCl with different concentrations
    El-Meligi, AA
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2002, 18 (06) : 549 - 551
  • [23] Hot corrosion of Ti3SiC2-based ceramics coated with Na2SO4 at 900 and 1000 °C in air
    Liu, GM
    Li, MS
    Zhou, YC
    CORROSION SCIENCE, 2003, 45 (06) : 1217 - 1226
  • [24] Aggregation of Na2SO4 Nanocrystals in Supercritical Water
    Voisin, Thomas
    Erriguible, Arnaud
    Aubert, Guillaume
    Aymonier, Cyril
    INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2018, 57 (06) : 2376 - 2384
  • [25] Investigation of the precipitation of Na2SO4 in supercritical water
    Voisin, T.
    Erriguible, A.
    Philippot, G.
    Ballenghien, D.
    Mateos, D.
    Cansell, F.
    Iversen, B. B.
    Aymonier, C.
    CHEMICAL ENGINEERING SCIENCE, 2017, 174 : 268 - 276
  • [26] Stressed oxidation behaviour of 3D C/SiC in water/oxygen/Na2SO4 coupled environment
    Luan, Xingang
    Yi, Runlin
    Zhang, Mingshuo
    Cheng, Laifei
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2024, 44 (13) : 7531 - 7539
  • [27] Initial oxidation of 3C-SiC (111) in oxidizing atmosphere containing water vapor: H2O adsorption from first-principles calculations
    Zhang, Pengfei
    Zhang, Yulei
    MATERIALS TODAY COMMUNICATIONS, 2021, 26
  • [28] Effects of Superheated Surface on the Deposition Behavior of Na2SO4 in Supercritical Water
    Zhu, Qiao
    Li, Zhe
    Song, Yafei
    Tong, Yujun
    Yang, Tao
    Cheng, Zhenmin
    PROCESSES, 2023, 11 (06)
  • [29] Investigation of the Interaction of Y2O3-Al2O3-SiO2 Coatings with Water Vapor and Na2SO4 at Temperatures to 1450°C
    Lebedeva, Yu E.
    Chainikova, A. S.
    Shchegoleva, N. E.
    Solntsev, S. S.
    GLASS AND CERAMICS, 2021, 78 (7-8) : 301 - 307
  • [30] MECHANISM OF NA2SO4 INDUCED CORROSION AT 600-DEGREES-C-900-DEGREES-C
    LUTHRA, KL
    SHORES, DA
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1980, 127 (10) : 2202 - 2210