Study of Aramid Yarns Sizing

被引:2
|
作者
Krstovic, Katarina [1 ]
Kovacevic, Stana [1 ]
Schwarz, Ivana [1 ]
Brnada, Snjezana [1 ]
机构
[1] Univ Zagreb, Dept Textile Design & Management, Fac Textile Technol, Prilaz Baruna Filipovica 28a, Zagreb 10000, Croatia
关键词
sizing with pre-wetting; sizing without pre-wetting; sizing of aramid yarns; mechanical yarn properties; laboratory-sizing machine; STARCH; ADHESION; FIBERS;
D O I
10.3390/polym14040761
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The process and efficiency of sizing aramid yarns before the weaving process was studied. The sizing was carried out under different conditions, with and without the pre-wetting of the threads before the actual sizing process. Two groups of yarns were tested. The first group consisted of five yarn samples that were blended with 95% meta-aramid and 5% para-aramid in counts of 20 x 2, 17 x 2, 14 x 2 and 12.5 x 2 tex. The second group of yarns consisted of three yarn samples that were blended with 93% meta-aramid, 5% para-aramid and 2% carbon in counts of 20, 20 x 2 and 17 x 2 tex. The inlet moisture of the yarn before sizing was 40% (with pre-wetting) and 4% (without pre-wetting), and the outlet moisture after drying was 4%. In order to carry out such tests to reproduce them, the sizing was carried out on a laboratory-sizing machine with the possibility of adapting to industrial conditions. According to the obtained results related to the properties of yarn before and after sizing, it can be concluded that sizing of aramid yarns is justified. When sizing the yarn without pre-wetting, the mechanical properties improved, especially breaking force, strength and abrasion resistance. Irregularity and hairiness were also reduced, especially when sizing with pre-wetting. Yarn hairiness or the frequency of protruding fibres also decreased with sizing in almost all samples and sizing conditions. The second group of yarns with a carbon fibre content mostly showed better mechanical properties before sizing, which continued after sizing. In general, the aramid yarn sized with pre-wetting showed certain deformations caused by stretching in the wet state and thus reduced the size pick-up, which caused less breaking forces and strength. Sizing with pre-wetting resulted in a slightly better smoothness of the thread and its higher evenness. It can be concluded that the aramid yarn should be sized with a lower size percentage (up to 4.5%), i.e., without pre-wetting in order to minimise the deformation of the yarn during sizing and thus improve the mechanical properties in the weaving process.
引用
收藏
页数:20
相关论文
共 50 条
  • [31] Tribological properties of aramid-polypropylene composites from commingled yarns: influence of aramid fibre weight fraction
    Pradhan, A. K.
    Alagirusamy, R.
    Bijwe, J.
    JOURNAL OF THE TEXTILE INSTITUTE, 2009, 100 (08) : 702 - 708
  • [32] A NONAQUEOUS METHOD FOR SIZING WOOL YARNS - PRELIMINARY WORK
    NASON, D
    TEXTILE RESEARCH JOURNAL, 1988, 58 (02) : 116 - 122
  • [33] Gold coated para-aramid yarns through electroless deposition
    Schwarz, Anne
    Hakuzimana, Jean
    Kaczynska, Anna
    Banaszczyk, Jedrzej
    Westbroek, Philippe
    McAdams, Eric
    Moody, Gillian
    Chronis, Yiannis
    Priniotakis, Georgios
    De Mey, Gilbert
    Tseles, Dimitris
    Van Langenhove, Lieva
    SURFACE & COATINGS TECHNOLOGY, 2010, 204 (9-10): : 1412 - 1418
  • [34] Influence of high temperature and ultraviolet radiation on durability and stability of aramid yarns
    Wang Luzhou
    Cai Guangming
    Li Ling
    Yu Weidong
    PROCEEDINGS OF THE 2007 INTERNATIONAL CONFERENCE ON ADVANCED FIBERS AND POLYMER MATERIALS VOLS 1 AND 2, 2007, : 410 - 412
  • [35] Tribological properties of woven para-aramid fabrics and their constituent yarns
    Rebouillat, S
    JOURNAL OF MATERIALS SCIENCE, 1998, 33 (13) : 3293 - 3301
  • [36] Effect of yarns in multiple directions on impact resistance of aramid/epoxy composites
    Miao, Yajing
    Liu, Shi
    Zhu, Kai
    Yang, Dan
    Xin, Binjie
    Li, Jinchun
    JOURNAL OF THE TEXTILE INSTITUTE, 2023, 114 (08) : 1246 - 1256
  • [37] The role of twist on tensile and frictional characteristics of aramid filament yarns (AFYs)
    Ding, Zuowei
    Zhao, Huihui
    Hu, Wanjin
    Wang, Rui
    MATERIALS RESEARCH EXPRESS, 2021, 8 (02)
  • [38] Tribological properties of woven para-aramid fabrics and their constituent yarns
    S. Rebouillat
    Journal of Materials Science, 1998, 33 : 3293 - 3301
  • [39] MOLECULAR AND MACROSCOPIC ORIENTATIONAL ORDER IN ARAMID SOLUTIONS - A MODEL TO EXPLAIN THE INFLUENCE OF SOME SPINNING PARAMETERS ON THE MODULUS OF ARAMID YARNS
    PICKEN, SJ
    VANDERZWAAG, S
    NORTHOLT, MG
    POLYMER, 1992, 33 (14) : 2998 - 3006
  • [40] Influence of yarn structure, sizing ingredients and type of sizing on properties and performance of sized yarns: Part II - A comparative study of sized yarn performance for ring- and rotor-spun cotton yarns
    Sengupta, AK
    Pratihar, P
    Kimothi, PD
    Vernekar, S
    Sayeed, MMA
    INDIAN JOURNAL OF FIBRE & TEXTILE RESEARCH, 2002, 27 (02) : 142 - 148