Microwave-enhanced selective leaching calcium from steelmaking slag to fix CO2 and produce high value-added CaCO3

被引:10
|
作者
Liu, Lincheng [1 ,2 ]
Fan, Xiaohui [1 ,2 ]
Gan, Min [1 ,2 ]
Wei, Jiaoyang [1 ,2 ]
Gao, Zitan [1 ]
Sun, Zengqing [1 ,2 ]
Ji, Zhiyun [1 ,2 ]
Wu, Yufeng [1 ]
Li, Jinhua [1 ]
机构
[1] Cent South Univ, Sch Minerals Proc & Bioengn, 932 South LushanRoad, Changsha 410083, Hunan, Peoples R China
[2] Cent South Univ, Minist Educ Carbon Emiss Reduct Met Resource Explo, Engn Res Ctr, Changsha 410083, Peoples R China
基金
中国国家自然科学基金;
关键词
Steel slag; Microwave-enhanced; Leaching kinetics; CO2; fixation; Crystal whiskerCaCO3; KINETICS; EXTRACTION; OPTIMIZATION; CARBONATION; BATTERIES; ACID;
D O I
10.1016/j.seppur.2023.125395
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The abundant resources of steel slag make it an intriguing prospect for long-term CO2 storage by mineral carbonation. Herein, the dissolution of steel slag in an acetic acid (HAc) solution and the fixation of CO2 in the leachate of steel slag to synthesize high-value CaCO3 were investigated. Results show that the microwave water bath condition is beneficial for improving the leaching rate of Ca and Mg elements in steel slag, while the low-concentration HAc solution displays high selectivity for Ca + Mg. In a water bath reaction enhanced by microwave, the leaching rate and selectivity of Ca + Mg can be increased by elevating the reaction temperature, extending the leaching time, lowering the concentration of HAc solution, and increasing the stirring rate. The kinetic parameters of the calcium element, including the apparent activation energy, were determined to be 14.51 kJ & sdot;mol- 1, suggesting control by surface chemical reactions. Finally, high-purity CaCO3 crystal whiskers can be synthesized under 400 W ultrasonic conditions with a reaction temperature of 70 degrees C, reaction time of 15 min, and a solution pH at 9.1 by introducing 20 % CO2 into the leachate. This strategy facilitates the concurrent utilization of dilute CO2 flue gas and voluminous solid steel slag waste, thereby improving the economic and environmental performance of the steel industry.
引用
收藏
页数:14
相关论文
共 34 条
  • [31] Microwave-assisted hydrothermal synthesis of Sn3O4 and SnO for electrocatalytic reduction of CO2 to high-added-value compounds
    Fernanda da Costa Romeiro
    Alysson Stefan Martins
    João Angelo Lima Perini
    Beatriz Costa e Silva
    Maria Valnice Boldrin Zanoni
    Marcelo Ornaghi Orlandi
    Journal of Materials Science, 2023, 58 (8) : 3508 - 3519
  • [32] CO2 sequestration and recovery of high-purity CaCO3 from bottom ash of masson pine combustion using a multifunctional reagent-amino acid
    Ji, Long
    Zheng, Xuan
    Ren, Yiwen
    Wang, Yikun
    Wang, Yan
    Yan, Shuiping
    SEPARATION AND PURIFICATION TECHNOLOGY, 2024, 329
  • [33] Hollow Submicrospherical Ni/Co-Promoted CaO/Ca12Al14O33 for H2 Production from Sorption-Enhanced Water-Gas Shift with In Situ CO2 Conversion via CH4 Reforming of CaCO3
    Zhang, Chunxiao
    Li, Yingjie
    Deng, Yumeng
    Liu, Wenqiang
    Han, Kuihua
    Wang, Yuzhuo
    He, Zirui
    Wu, Jun Jie
    ACS CATALYSIS, 2025, 15 (05): : 4208 - 4228
  • [34] CO2 conversion by high-dose rate electron beam irradiation: one-step, metal-free and simultaneous production of H2, CO, CH4, C2H6 and organic acids from an acid-decomposed CaCO3/additive EtOH mixture
    Hosokawa, Yoichi
    Kajiya, Shuji
    Ohshima, Ayako
    Ishida, Nobuhiro
    Washio, Masakazu
    Usuki, Arimitsu
    GREEN CHEMISTRY, 2019, 21 (11) : 3091 - 3098