Effect of Mg treatment on inclusion behaviors in 430 ferritic stainless steel during solidification

被引:3
|
作者
Gan, Wen-liang [1 ,2 ,3 ]
Huang, Zai-jing [4 ]
Liu, Cheng-song [1 ,2 ,3 ]
Wang, Yong [1 ,2 ,3 ]
Zhang, Hua [1 ,2 ,3 ]
Ni, Hong-wei [1 ,2 ,3 ]
机构
[1] Wuhan Univ Sci & Technol, State Key Lab Refractories & Met, Wuhan 430081, Hubei, Peoples R China
[2] Wuhan Univ Sci & Technol, Key Lab Ferrous Met & Resources Utilizat Minist Ed, Wuhan 430081, Hubei, Peoples R China
[3] Wuhan Univ Sci & Technol, Hubei Prov Key Lab New Proc Ironmaking & Steelmaki, Wuhan 430081, Hubei, Peoples R China
[4] Guangxi BG New Mat Co Ltd, Beihai 536000, Guangxi, Peoples R China
基金
中国国家自然科学基金;
关键词
430 ferritic stainless steel; Mg treatment; Inclusions; Precipitation; Growth; And transformation behavior; Cooling and solidification; TITANIUM-OXIDE CLUSTERS; HEAT-AFFECTED ZONE; GRAIN-REFINEMENT; DEOXIDATION EQUILIBRIA; SOLUTE REDISTRIBUTION; PIPELINE STEELS; EVOLUTION; THERMODYNAMICS; MICROSTRUCTURE; DIFFUSION;
D O I
10.1016/j.jmrt.2023.12.207
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
To understand the effect of Mg treatment on the precipitation, growth, and transformation of inclusions in 430 ferritic stainless steel during solidification, slag refining and Mg treatment experiments with different cooling methods were conducted at 1873 K (1600 degrees C). Experimental results showed that the oxide inclusions in 430 stainless steel without Mg treatment were mainly Al2O3-SiO2-MnO (slag phase), Al2O3-Cr2O3-MnO (spinel phase), high-Al2O3 (corundum phase) and CaO-SiO2-Al2O3-MnO (slag phase), while all of the oxides except CaO-SiO2-Al2O3-MnO inclusions transformed to MgO-Al2O3-Cr2O3-MnO (spinel phase) after Mg treatment. With water quenching, the average inclusion diameters were about 1.4 mu m in both of the Mg-free and Mg-bearing steels, while they increased to approximate 3.1 and 1.9 mu m after furnace cooling, separately. With the decrease of cooling rate from 26.2 to 1.24 K s(-1), in the Mg-free steel, the average Al2O3 and Cr2O3 contents in the inclusion increased from 19.6 to 42.6 mass% and from 12.22 to 19.44 mass%, respectively, and the average SiO2 content decreased from 43.5 to 17.1 mass%. However, the average composition of inclusions in Mg-bearing steel was relatively stable and independent of cooling rate. A kinetic model was established with the solute micro-segregation model to predict oxide inclusion growth during cooling and solidification. Without and with Mg treatment, under a cooling rate of 1 K s(-1), the calculated final sizes of the most stable oxide inclusions were 3.27 and 1.88 mu m, respectively. The predicted average compositions and diameters of oxide inclusions were generally consistent with the experimental results.
引用
收藏
页码:3349 / 3364
页数:16
相关论文
共 50 条
  • [41] The effect of cold rolling reduction ratio on the microstructure and mechanical properties of ferritic stainless steel 430
    Xiaoyu Sun
    Xiaoguang Ma
    Jinghui Li
    Linan Ma
    Mingya Zhang
    Jingwei Zhao
    The International Journal of Advanced Manufacturing Technology, 2023, 126 : 4225 - 4237
  • [42] Microstructure observation of the tensile fractured 430ferritic stainless steel
    Zang, Shujun
    Li, Juanjuan
    Yin, Xiaoqiang
    Zhang, Jianbin
    ADVANCES IN MATERIALS AND MATERIALS PROCESSING IV, PTS 1 AND 2, 2014, 887-888 : 228 - 232
  • [43] A review on influence of nitriding on AISI430 ferritic stainless steel
    Manne, Vamshi
    Singh, S. K.
    Sateesh, N.
    Ram, Subbiah
    MATERIALS TODAY-PROCEEDINGS, 2020, 26 : 1010 - 1013
  • [44] Antibacterial mechanism of Cu-bearing 430 ferritic stainless steel
    Zhuang Zhang
    Xin-Rui Zhang
    Tao Jin
    Chun-Guang Yang
    Yu-Peng Sun
    Qi Li
    Ke Yang
    Rare Metals, 2022, 41 (02) : 559 - 569
  • [45] The effect of cold rolling reduction ratio on the microstructure and mechanical properties of ferritic stainless steel 430
    Sun, Xiaoyu
    Ma, Xiaoguang
    Li, Jinghui
    Ma, Linan
    Zhang, Mingya
    Zhao, Jingwei
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2023, 126 (9-10): : 4225 - 4237
  • [46] EFFECT OF APPLICATION OF THE SHOT PEENING PROCESS IN THE CORROSION RESISTANCE OF THE AISI 430 FERRITIC STAINLESS STEEL
    Peltz, Jefferson da Silva
    Antonini, Leonardo Marasca
    Kunst, Sandra Raquel
    Ludwig, Gustavo Alberto
    Fuhr, Luciana Tais
    Malfatti, Celia de Fraga
    20TH BRAZILIAN CONFERENCE ON MATERIALS SCIENCE AND ENGINEERING, 2014, 775-776 : 365 - +
  • [47] Observation of hydrogen trap and hydrogen embrittlement of 430 ferritic stainless steel
    Wang, Tao
    Fang, Xueyang
    Zhang, Huiyun
    Lv, Wenjie
    Ma, Jinyao
    Liang, Wei
    Zheng, Liuwei
    MATERIALS LETTERS, 2022, 313
  • [48] Antibacterial mechanism of Cu-bearing 430 ferritic stainless steel
    Zhuang Zhang
    Xin-Rui Zhang
    Tao Jin
    Chun-Guang Yang
    Yu-Peng Sun
    Qi Li
    Ke Yang
    Rare Metals, 2022, 41 : 559 - 569
  • [49] Behavior and Mechanism of Inclusion Deformation in Type 430 Stainless Steel During Isothermal Compression
    Hongwei Ni
    Wenliang Gan
    Chengsong Liu
    Rijin Cheng
    Yong Wang
    Hua Zhang
    Metallurgical and Materials Transactions B, 2023, 54 : 851 - 867
  • [50] Behavior and Mechanism of Inclusion Deformation in Type 430 Stainless Steel During Isothermal Compression
    Ni, Hongwei
    Gan, Wenliang
    Liu, Chengsong
    Cheng, Rijin
    Wang, Yong
    Zhang, Hua
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2023, 54 (02): : 851 - 867