Effect of Mg treatment on inclusion behaviors in 430 ferritic stainless steel during solidification

被引:3
|
作者
Gan, Wen-liang [1 ,2 ,3 ]
Huang, Zai-jing [4 ]
Liu, Cheng-song [1 ,2 ,3 ]
Wang, Yong [1 ,2 ,3 ]
Zhang, Hua [1 ,2 ,3 ]
Ni, Hong-wei [1 ,2 ,3 ]
机构
[1] Wuhan Univ Sci & Technol, State Key Lab Refractories & Met, Wuhan 430081, Hubei, Peoples R China
[2] Wuhan Univ Sci & Technol, Key Lab Ferrous Met & Resources Utilizat Minist Ed, Wuhan 430081, Hubei, Peoples R China
[3] Wuhan Univ Sci & Technol, Hubei Prov Key Lab New Proc Ironmaking & Steelmaki, Wuhan 430081, Hubei, Peoples R China
[4] Guangxi BG New Mat Co Ltd, Beihai 536000, Guangxi, Peoples R China
基金
中国国家自然科学基金;
关键词
430 ferritic stainless steel; Mg treatment; Inclusions; Precipitation; Growth; And transformation behavior; Cooling and solidification; TITANIUM-OXIDE CLUSTERS; HEAT-AFFECTED ZONE; GRAIN-REFINEMENT; DEOXIDATION EQUILIBRIA; SOLUTE REDISTRIBUTION; PIPELINE STEELS; EVOLUTION; THERMODYNAMICS; MICROSTRUCTURE; DIFFUSION;
D O I
10.1016/j.jmrt.2023.12.207
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
To understand the effect of Mg treatment on the precipitation, growth, and transformation of inclusions in 430 ferritic stainless steel during solidification, slag refining and Mg treatment experiments with different cooling methods were conducted at 1873 K (1600 degrees C). Experimental results showed that the oxide inclusions in 430 stainless steel without Mg treatment were mainly Al2O3-SiO2-MnO (slag phase), Al2O3-Cr2O3-MnO (spinel phase), high-Al2O3 (corundum phase) and CaO-SiO2-Al2O3-MnO (slag phase), while all of the oxides except CaO-SiO2-Al2O3-MnO inclusions transformed to MgO-Al2O3-Cr2O3-MnO (spinel phase) after Mg treatment. With water quenching, the average inclusion diameters were about 1.4 mu m in both of the Mg-free and Mg-bearing steels, while they increased to approximate 3.1 and 1.9 mu m after furnace cooling, separately. With the decrease of cooling rate from 26.2 to 1.24 K s(-1), in the Mg-free steel, the average Al2O3 and Cr2O3 contents in the inclusion increased from 19.6 to 42.6 mass% and from 12.22 to 19.44 mass%, respectively, and the average SiO2 content decreased from 43.5 to 17.1 mass%. However, the average composition of inclusions in Mg-bearing steel was relatively stable and independent of cooling rate. A kinetic model was established with the solute micro-segregation model to predict oxide inclusion growth during cooling and solidification. Without and with Mg treatment, under a cooling rate of 1 K s(-1), the calculated final sizes of the most stable oxide inclusions were 3.27 and 1.88 mu m, respectively. The predicted average compositions and diameters of oxide inclusions were generally consistent with the experimental results.
引用
收藏
页码:3349 / 3364
页数:16
相关论文
共 50 条
  • [21] Planar colony of needle precipitates formed during solidification of a ferritic stainless steel
    Pryds, NH
    Huang, X
    SCRIPTA MATERIALIA, 1997, 36 (11) : 1219 - 1226
  • [22] Effect of microstructural parameters and casting conditions on the solidification microstructure of 430 stainless steel
    Lan, Peng
    Sun, Hai-Bo
    Li, Yang
    Zhang, Jia-Quan
    Beijing Keji Daxue Xuebao/Journal of University of Science and Technology Beijing, 2014, 36 (04): : 446 - 452
  • [23] Simulation of Line Annealing of Type 430 Ferritic Stainless Steel
    Kisko, A. P.
    Suikkanen, P. P.
    Garcia, C. I.
    Cho, K.
    Hua, M.
    Karjalainen, L. P.
    DeArdo, A. J.
    RECRYSTALLIZATION AND GRAIN GROWTH IV, 2012, 715-716 : 437 - +
  • [24] Electrochemical surface nitriding of SUS 430 ferritic stainless steel
    Tsujimura, H
    Goto, T
    Ito, Y
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 355 (1-2): : 315 - 319
  • [25] Effect of rare earth Ce treatment on the microstructure and properties of 430 ferritic stainless steel bearing Sn and Cu
    Li, Yang
    Chen, Changyong
    Du, Pengfei
    Yang, Hao
    Ma, Shuai
    Sun, Meng
    Zhang, Mina
    Jiang, Zhouhua
    IRONMAKING & STEELMAKING, 2024,
  • [26] Continuous dynamic recrystallization of AISI 430 ferritic stainless steel
    Kim, SI
    Yoo, YC
    METALS AND MATERIALS INTERNATIONAL, 2002, 8 (01): : 7 - 13
  • [27] Study on processing and properties of 430 ferritic stainless steel coil
    Liu, Hongtao
    Wu, Chunjing
    Ren, Xueping
    Li, Shuxia
    Harbin Gongye Daxue Xuebao/Journal of Harbin Institute of Technology, 2015, 47 (03): : 107 - 110
  • [28] Continuous dynamic recrystallization of AISI 430 ferritic stainless steel
    Sung-Il Kim
    Yeon-Chul Yoo
    Metals and Materials International, 2002, 8 : 7 - 13
  • [29] HEAT RESISTANT FERRITIC STAINLESS STEEL 430 Zr.
    Moroishi, Taishi
    Fujikawa, Hisao
    Makiura, Hirofumi
    Koizumi, Isamu
    Shoji, Yuji
    Sumitomo Search, 1979, (21): : 26 - 33
  • [30] Effect of hydrogen on the mechanical properties and fracture modes of annealed 430 ferritic stainless steel
    Wang, Tao
    Fang, Xueyang
    Lv, Wenjie
    Zhang, Huiyun
    Luo, Yi
    Zheng, Liuwei
    Liang, Wei
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 832