The Influence of Protective Coatings on High-Temperature Corrosion under Biomass Ash Deposits

被引:0
|
作者
Maciejczyk, Anna [1 ,2 ]
Maj, Izabella [3 ]
Ciukaj, Szymon [4 ]
Hernik, Bartlomiej [3 ]
Osuch, Arkadiusz [1 ]
机构
[1] SHI FW Energia Fakop Sp Zoo, PL-41200 Sosnowiec, Poland
[2] Silesian Tech Univ, Doctoral Sch, PL-44100 Gliwice, Poland
[3] Silesian Tech Univ, Fac Energy & Environm Engn, Dept Power Engn & Turbomachinery, PL-44100 Gliwice, Poland
[4] Sumitomo SHI FW Energia Polska Sp Zoo, PL-41200 Sosnowiec, Poland
关键词
biomass; corrosion; combustion; ash; RDF; coating; Inconel; 625; Alloy; 310; HOT CORROSION; INCONEL; 625; STEELS; CR; BEHAVIOR; ALLOYS; COMBUSTION; FE; BENEATH; IRON;
D O I
10.3390/en16217221
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
The presented research determined the performance of the protective coatings against the corrosion process under biomass and refuse-derived fuel (RDF) ash deposits. High-temperature corrosion tests were performed on steel grades intended for use in the fabrication of pressure parts working in elevated temperatures such as superheaters in power boilers. Two steel grades were investigated, P235GH and 16Mo3, and two protective coatings were applied, Inconel 625 and Alloy 310. The samples were sourced from the industrial boiler manufacturing company. The samples were exposed to two ashes originating from biofuels and one ash originating from RDF for comparison, all collected from Polish heat plants and power plants. Exposures were carried out in an oxidizing atmosphere for a maximum time of 504 h. The test temperatures of 480, 520, and 580 degrees C simulated superheater conditions of biofuel- and waste-fired power boilers. The corrosion kinetics were determined by weight change measurements conducted after 24, 168, and 504 h of the exposure. Regardless of the exposure temperature and the type of ash under which the samples were investigated, the use of 2.0 mm thick protective coatings resulted in smaller increases in the weight of the tested coupons which proves that alloy coatings give measurable results and are good remedies for chlorine-induced corrosion.
引用
收藏
页数:16
相关论文
共 50 条
  • [41] PROTECTIVE COATINGS FOR HIGH-TEMPERATURE ALLOYS - STATE OF TECHNOLOGY
    GOWARD, GW
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1976, 123 (08) : C253 - C253
  • [42] DIFFUSIONAL ASPECTS OF HIGH-TEMPERATURE OXIDATION AND PROTECTIVE COATINGS
    NESBITT, JA
    JOURNAL OF METALS, 1988, 40 (07): : A36 - A36
  • [43] STANDARD TESTS NEEDED FOR HIGH-TEMPERATURE PROTECTIVE COATINGS
    WURST, JC
    HJELM, LN
    JAMES, DR
    MATERIALS RESEARCH AND STANDARDS, 1966, 6 (04): : 188 - &
  • [44] THERMAL-STABILITY OF HIGH-TEMPERATURE PROTECTIVE COATINGS
    GUSAROV, VV
    SUVOROV, SA
    JOURNAL OF APPLIED CHEMISTRY OF THE USSR, 1990, 63 (08): : 1670 - 1672
  • [45] High-temperature protective coatings for C/SiC composites
    Xiang Yang
    Chen Zhao-hui
    Cao Feng
    JOURNAL OF ASIAN CERAMIC SOCIETIES, 2014, 2 (04): : 305 - 309
  • [46] QUALITY-CONTROL OF HIGH-TEMPERATURE PROTECTIVE COATINGS
    BETTRIDGE, DF
    UBANK, RG
    MATERIALS SCIENCE AND TECHNOLOGY, 1986, 2 (03) : 232 - 242
  • [47] Influence of high-temperature protective coatings on the mechanical properties of nickel-based superalloys
    Itoh, Y
    Saitoh, M
    Ishiwata, Y
    JOURNAL OF MATERIALS SCIENCE, 1999, 34 (16) : 3957 - 3966
  • [48] Influence of high-temperature protective coatings on the mechanical properties of nickel-based superalloys
    Y. Itoh
    M. Saitoh
    Y. Ishiwata
    Journal of Materials Science, 1999, 34 : 3957 - 3966
  • [49] THE COATINGS AND HIGH-TEMPERATURE CORROSION DATA-BANK
    STREIFF, R
    KOMORNICKI, S
    SURFACE & COATINGS TECHNOLOGY, 1992, 50 (03): : 263 - 269
  • [50] Interactions of high-temperature coatings in hot corrosion environments
    Shifler, DA
    CORROSION AND CORROSION PROTECTION, 2001, 2001 (22): : 637 - 644