The corrosion behavior of Sc2O3-Y2O3 co-doped ZrO2 influenced by Sc2O3 content in CMAS at 1300 °C

被引:4
|
作者
Liao, Yuxuan [1 ,2 ]
Dai, Yifei [1 ,2 ]
Zhai, Yifan [1 ,2 ]
He, Aoping [1 ,2 ,3 ]
He, Huan [1 ,2 ,3 ]
Liang, Tianquan [1 ,2 ,3 ]
机构
[1] Guangxi Univ, State Key Lab Featured Met Mat & Life Cycle Safety, MOE Key Lab New Proc Technol Nonferrous Met & Mat, Nanning 530004, Peoples R China
[2] Guangxi Univ, Sch Resources Environm & Mat, Nanning 530004, Peoples R China
[3] Guangxi Univ, Ctr Ecol Collaborat Innovat Aluminum Ind Guangxi, Nanning 530004, Peoples R China
基金
中国国家自然科学基金;
关键词
ScYSZ; CMAS; Corrosion behavior; Reactivity; Mechanism; THERMAL BARRIER COATINGS; YTTRIA-STABILIZED ZIRCONIA; CALCIUM-MAGNESIUM ALUMINOSILICATE; PHYSICAL PROPERTIES; PHASE-STABILITY; PART I; RESISTANCE; CERAMICS; DEGRADATION; YB;
D O I
10.1016/j.jeurceramsoc.2023.09.025
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effect of Sc2O3 content on the corrosion behaviors of xSc2O3-3.5Y2O3 co-doped ZrO2 (ScYSZ, x = 4.5, 5.5 and 6.5 mol.%) in calcium-magnesium-alumino-silicate (CMAS) at 1300 degrees C was investigated in this paper. It is shown that the ScYSZ ceramic exhibits better resistance to molten CMAS attack when doping with more Sc2O3. The CMAS penetration depth in the ScYSZ ceramic decreases with increasing Sc2O3. It is about 18 mu m of CMAS penetrated depth in the 6.5Sc3.5YSZ after corrosion for 4 h at 1300 degrees C, including an 11 mu m and 7 mu m for the reaction-reprecipitation and grain-boundary infiltration layers, respectively. High thermochemical stability and weak reactivity of the ScYSZ to the glassy CMAS melt are beneficial to enhance the high temperature corrosion resistance, attributing to the low solubility in molten CMAS and the weak affinity to Ca2+ for small ionic radius Sc3+. The mechanism of enhancing the resistance to CMAS is discussed.
引用
收藏
页码:1179 / 1187
页数:9
相关论文
共 50 条
  • [41] PHASE-DIAGRAM OF THE ZRO2(HFO2)-SC2O3 SYSTEM
    MAGUNOV, RL
    SHKLYAR, GL
    KATRIDI, VF
    INORGANIC MATERIALS, 1989, 25 (07) : 1035 - 1037
  • [42] PARAMAGNETIC RESONANCE OF TRIVALENT CHROMIUM IN SC2O3 AND Y2O3
    TIPPINS, HH
    PHYSICAL REVIEW, 1967, 158 (02): : 301 - &
  • [43] AN ODMR STUDY OF EXCITON TRAPPING IN Y2O3 AND SC2O3
    HAYES, W
    KANE, MJ
    SALMINEN, O
    KUZNETSOV, AI
    JOURNAL OF PHYSICS C-SOLID STATE PHYSICS, 1984, 17 (14): : L383 - L387
  • [44] Specific Features of the Local Structure and Transport Properties of ZrO2-Sc2O3-Y2O3 and ZrO2-Sc2O3-Yb2O3 Crystals
    Borik, M. A.
    Volkova, T. V.
    Kuritzyna, I. E.
    Larina, N. A.
    Lomonova, E. E.
    Myzina, V. A.
    Ryabochkina, P. A.
    Tabachkova, N. Yu.
    OPTICS AND SPECTROSCOPY, 2018, 125 (06) : 898 - 902
  • [45] Local trapping sites in Y2O3 and Sc2O3 ceramics
    O. M. Bordun
    I. M. Bordun
    Journal of Applied Spectroscopy, 1997, 64 (03) : 361 - 365
  • [46] Solution mechanisms for Li2O in Sc2O3, Y2O3 and La2O3
    Chroneos, A
    Busker, G
    ACTA CHIMICA SLOVENICA, 2005, 52 (04) : 417 - 421
  • [47] Preparation and Characterization of Sc2O3-Doped ZrO2 Nanofiber
    Lei, Yao
    Wei, Liu
    Gang, Ou
    Wei, Pan
    RARE METAL MATERIALS AND ENGINEERING, 2013, 42 : 745 - 747
  • [48] Phase Composition, Electrical Conductivity, and Stability of ZrO2–Sc2O3–Cr2O3 Solid Electrolytes
    Yu. N. Karavaev
    A. D. Neuimin
    E. G. Vovkotrub
    Inorganic Materials, 2004, 40 : 1073 - 1078
  • [49] Czochralski growth and laser parameters of RE3+-doped Y2O3 and Sc2O3
    Fornasiero, L
    Mix, E
    Peters, V
    Petermann, K
    Huber, G
    CERAMICS INTERNATIONAL, 2000, 26 (06) : 589 - 592
  • [50] Electrical conductivity in the system ZrO2-Y2O3-Sc2O3
    Kanagawa Univ, Yokohama, Japan
    Solid State Ionics, 3-4 (185-189):