The corrosion behavior of Sc2O3-Y2O3 co-doped ZrO2 influenced by Sc2O3 content in CMAS at 1300 °C

被引:4
|
作者
Liao, Yuxuan [1 ,2 ]
Dai, Yifei [1 ,2 ]
Zhai, Yifan [1 ,2 ]
He, Aoping [1 ,2 ,3 ]
He, Huan [1 ,2 ,3 ]
Liang, Tianquan [1 ,2 ,3 ]
机构
[1] Guangxi Univ, State Key Lab Featured Met Mat & Life Cycle Safety, MOE Key Lab New Proc Technol Nonferrous Met & Mat, Nanning 530004, Peoples R China
[2] Guangxi Univ, Sch Resources Environm & Mat, Nanning 530004, Peoples R China
[3] Guangxi Univ, Ctr Ecol Collaborat Innovat Aluminum Ind Guangxi, Nanning 530004, Peoples R China
基金
中国国家自然科学基金;
关键词
ScYSZ; CMAS; Corrosion behavior; Reactivity; Mechanism; THERMAL BARRIER COATINGS; YTTRIA-STABILIZED ZIRCONIA; CALCIUM-MAGNESIUM ALUMINOSILICATE; PHYSICAL PROPERTIES; PHASE-STABILITY; PART I; RESISTANCE; CERAMICS; DEGRADATION; YB;
D O I
10.1016/j.jeurceramsoc.2023.09.025
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effect of Sc2O3 content on the corrosion behaviors of xSc2O3-3.5Y2O3 co-doped ZrO2 (ScYSZ, x = 4.5, 5.5 and 6.5 mol.%) in calcium-magnesium-alumino-silicate (CMAS) at 1300 degrees C was investigated in this paper. It is shown that the ScYSZ ceramic exhibits better resistance to molten CMAS attack when doping with more Sc2O3. The CMAS penetration depth in the ScYSZ ceramic decreases with increasing Sc2O3. It is about 18 mu m of CMAS penetrated depth in the 6.5Sc3.5YSZ after corrosion for 4 h at 1300 degrees C, including an 11 mu m and 7 mu m for the reaction-reprecipitation and grain-boundary infiltration layers, respectively. High thermochemical stability and weak reactivity of the ScYSZ to the glassy CMAS melt are beneficial to enhance the high temperature corrosion resistance, attributing to the low solubility in molten CMAS and the weak affinity to Ca2+ for small ionic radius Sc3+. The mechanism of enhancing the resistance to CMAS is discussed.
引用
收藏
页码:1179 / 1187
页数:9
相关论文
共 50 条
  • [21] Effect of point defects on the thermal conductivity of Sc2O3-Y2O3 co-stabilized tetragonal ZrO2 ceramic materials
    Fan, W.
    Bai, Y.
    Wang, Z. Z.
    Che, J. W.
    Wang, Y.
    Tao, W. Z.
    Wang, R. J.
    Liang, G. Y.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2019, 39 (07) : 2389 - 2396
  • [22] An investigation of conductivity, microstructure and stability of electrolyte compositions in the system 9 mol% (Sc2O3-Y2O3)-ZrO2(Al2O3)
    Badwal, SPS
    Ciacchi, FT
    Rajendran, S
    Drennan, J
    SOLID STATE IONICS, 1998, 109 (3-4) : 167 - 186
  • [23] INTERACTION IN THE ZRO2-Y2O3-SC2O3 SYSTEM AT 1300-1900-DEGREES-C
    MAISTER, IM
    LOPATO, LM
    ZAITSEVA, ZA
    SHEVCHENKO, AV
    INORGANIC MATERIALS, 1991, 27 (11) : 1997 - 2000
  • [24] A study of Eu2O3, Sc2O3 co-doped tungsten matrix impregnated cathode
    Wang, Jinshu
    Wang, Xi
    Liu, Wei
    Gao, Tao
    Wang, Yiman
    JOURNAL OF PHYSICS AND CHEMISTRY OF SOLIDS, 2011, 72 (10) : 1128 - 1132
  • [25] INVESTIGATION OF SC2O3 BEHAVIOR IN SC2O3-DISPERSED OXIDE CATHODES
    SAITO, M
    SUZUKI, R
    FUKUYAMA, K
    WATANABE, K
    SANO, K
    NAKANISHI, H
    IEEE TRANSACTIONS ON ELECTRON DEVICES, 1990, 37 (12) : 2605 - 2611
  • [26] Mechanical Properties Durability of Sc2O3-Y2O3 Co-Stabilized ZrO2 Thermal Barrier Materials for High Temperature Application
    Fan, Wei
    Wang, Yiqi
    Liu, Yanfen
    Bai, Yu
    Wang, Yu
    Liu, Qi
    COATINGS, 2022, 12 (02)
  • [27] THERMODYNAMICS OF DISSOCIATIVE VOLATILIZATION OF Y2O3 AND SC2O3
    YUDIN, BF
    MOGILENSKII, VI
    POLONSKII, YA
    LAPSHIN, SA
    JOURNAL OF APPLIED CHEMISTRY OF THE USSR, 1976, 49 (04): : 810 - 813
  • [28] Microstructure and mechanical properties of Sc2O3- Y2O3 co-doped ZrO2 ceramic materials for thermal barrier coating
    Wang, Zhigang
    Liu, Rengqian
    Xie, Min
    Zhang, Yonghe
    Wang, Xuanli
    Song, Xiwen
    Chang, Zhendong
    Liu, Delin
    Mu, Rende
    CAILIAO GONGCHENG-JOURNAL OF MATERIALS ENGINEERING, 2024, 52 (06): : 139 - 146
  • [29] Tunneling luminescence of Y2O3 and Sc2O3 ceramics
    O. M. Bordun
    I. M. Bordun
    A. B. Lyskovich
    Journal of Applied Spectroscopy, 1999, 66 (5) : 738 - 741
  • [30] ???????Study on thermal shock resistance of Sc2O3 and Y2O3 co-stabilized ZrO2 thermal barrier coatings
    Dong, Y. S.
    Yan, C. L.
    Li, J.
    Jiang, Z. C.
    Mo, W. L.
    Zhang, Q. J.
    CERAMICS INTERNATIONAL, 2023, 49 (12) : 20034 - 20040